1.1Glycerol as the humectant
Dissolve 3% glycerol by mass in the aqueous phase and then disperse the crosslinked glycosaminoglycan gel. Glycerol associates with water through hydrogen bonding and helps the applied layer retain moisture.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Dissolve 3% glycerol by mass in the aqueous phase and then disperse the crosslinked glycosaminoglycan gel. Glycerol associates with water through hydrogen bonding and helps the applied layer retain moisture.
Disperse molten white petrolatum into an aqueous phase using a nonionic emulsifier, then cool the emulsion and blend in the crosslinked glycosaminoglycan gel. As water evaporates from the applied layer, petrolatum deposits a hydrophobic film that slows further water loss.
Dilute an aqueous methylsilanetriol feed into a mildly acidic aqueous phase and blend it with the hydrated glycosaminoglycan gel. The mildly acidic phase favors protonated silanol groups, and those groups interact with water through hydrogen bonding.
Disperse 1% hydroxyethyl cellulose by mass into water and allow the polymer to hydrate before adding the organosilicon solution. The hydrated linear chains overlap and entangle, increasing viscosity and slowing runoff.
Disperse magnesium aluminum silicate in low-electrolyte water under high shear and let the platelets hydrate before adding the organosilicon phase. Associations between platelet edges and faces build a network that gives the dispersion a yield stress and lets it spread under shear.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A bench tribometer uses a hydrated pad of crosslinked sodium hyaluronate equilibrated in an aqueous solution of monomethylsilanetriol. A rigid cup holds the pad with its upper face flush with the rim. A polished spherical probe traverses the exposed face under a fixed normal load, and repeated passes establish the instrument's lateral force repeatability.
Ethylsilanetriol replaces monomethylsilanetriol and supplies one ethyl group and three hydroxyl groups bound to silicon. An aqueous ethylsilanetriol solution serves as the continuous phase, and prehydrated crosslinked sodium hyaluronate particles form the dispersed phase. Low-shear mixing distributes the particles, and the hydrated particles retain water in the spread layer.
A crosslinked sodium hyaluronate slab is cut into pads 1, 2, and 4 mm thick, each with the same exposed area. Each pad equilibrates in the same aqueous monomethylsilanetriol bath and is then mounted with its back and edges sealed. The exposed face contacts a stirred aqueous receiver held at 25 °C, and samples collected at 5, 15, 30, and 60 minutes track release over different diffusion distances.
A die-cut pad of crosslinked sodium hyaluronate swollen with aqueous monomethylsilanetriol sits between a flexible backing film and a porous contact sheet. A pressure-sensitive adhesive border joins the backing and contact sheet around the perimeter and secures the patch to the skin. The backing limits evaporation, and the pores provide a path for the dissolved silanol to reach the contact surface.
A refillable roller applicator holds an aqueous monomethylsilanetriol solution containing dispersed crosslinked sodium hyaluronate particles. The swollen particles are sieved so their maximum diameter is less than one-third of the minimum feed clearance around the roller. As the roller turns against the application surface, it draws gel from the reservoir and transfers a thin layer.
Two metering pumps feed a sodium monomethylsilanetriolate solution and a suspension of crosslinked sodium hyaluronate into a static mixer. A temperature-compensated conductivity probe sits in a sidestream downstream of the mixer, and software converts its readings to silanolate concentration using calibration batches with fixed background electrolyte and polymer content. The controller trims the silanolate feed while holding the combined flow constant, and a valve diverts output when the reading leaves the calibrated acceptance band.
Use methylsilanetriol, CH₃Si(OH)₃, with one methyl group and three silanol groups per silicon atom. Meter a dilute aqueous solution into the hydrated gel under gentle stirring to distribute it throughout the water phase.
Use an aqueous potassium methylsilanolate feed, with a one-carbon methyl group bonded directly to silicon. Maintain the feed under alkaline conditions to favor deprotonated silanol groups with potassium counterions.
React sodium hyaluronate with 1,4-butanediol diglycidyl ether under alkaline aqueous conditions to form ether bridges between polymer chains. Wash the gel with successive water exchanges to remove soluble residues, then equilibrate it in an aqueous medium to set its swelling.
Pass hydrated crosslinked sodium hyaluronate gel through a 250 µm screen to break it into smaller gel particles. Disperse the swollen particles in an aqueous carrier so they move past one another during spreading and contribute body at rest.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
A method of preparing an organosilanol compound is provided. The method comprises reacting (A) an initial organosilicon compound and (B) water in the presence of (C) a catalyst.B · US 2022/0112223 A1 · ¶ 4
General examples of hydrocarbyl groups include alkyl groups, aryl groups, alkenyl groups, halocarbon groups, and the like, as well as derivatives, modifications, and combinations thereof. Examples of suitable alkyl groups include methyl, ethyl, propyl (e.g. iso-propyl and/or n-propyl), butyl (e.g. isobutyl, n-butyl, tert-butyl, and/or sec-butyl), pentyl (e.g., isopentyl, neopentyl, and/or tert-pentyl), hexyl, as well as branched saturated hydrocarbon groups having from 6 to 18 carbon atoms.B · US 2022/0112223 A1 · ¶ 10
More specifically, the present invention is concerned with hydrogels made of crosslinked glycosaminoglycans, particularly crosslinked hyaluronic acid, chondroitin or chondroitin sulfate.A · US 2020/0030219 A1 · ¶ 1
An empty cell means only that no passage was reproduced there.
Hence, it is typically desired to maintain a low degree of modification by efficient crosslinking to conserve the native properties and effects of the glycosaminoglycan itself.A · US 2020/0030219 A1 · ¶ 6
It is a further object of the present invention to provide a method for crosslinking GAG molecules resulting in a hydrogel product based entirely on carbohydrate type structures.A · US 2020/0030219 A1 · ¶ 8
In particular, traditional methods of preparing certain functional organosilicon compounds are often incompatible with many silicone materials (e.g. via promoting silicone rearrangements, unselective reactions, degradation, hydrolysis of functional groups, etc.), resulting in decreased yields and purities, and limiting general applicability of such methods.B · US 2022/0112223 A1 · ¶ 3
For example, the organosilanol compound may be utilized as a starting component when preparing silicone-organic hybrid materials, e.g. via copolymerization, grafting, etc.B · US 2022/0112223 A1 · ¶ 6
patent.fyi, US 2026/0355094 A1, claim 1, first published 2026-11-19T07:53:10-05:00, https://patent.fyi/US20260355094/, SHA-256 cfa284349cf5a5d28f1219aec0e03f53bfa87be3bee891e5ac70c4e1d744b7e7