Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Anhydrous soft paste
What ifWhat if the formulation dispersed its pigments in an anhydrous silicone paste?
Claim language“a discontinuous water phase”
A silicone elastomer gel and microcrystalline wax give the oil phase enough structure to hold dispersed pigment. The paste spreads under finger pressure, and a volatile hydrocarbon evaporates after application to concentrate the film former.
1.2Acrylate film formation
What ifWhat if an oil-soluble acrylate copolymer supplied film formation without an MQ resin?
Claim language“a film former including an MQ resin”
An acrylate copolymer with long alkyl side chains dissolves in the external phase with a volatile hydrocarbon carrier. As the carrier evaporates, the polymer concentrates into a continuous film that binds pigment to the application surface.
1.2Lower emollient loading
What ifWhat if the total emollient content was 5 wt. % of the formulation?
Claim language“an emollient in an amount of 10.0-35.0 wt. %”
Low-viscosity dimethicone at 5 wt. % provides residual glide, and a volatile hydrocarbon carrier supplies most of the spreadability during application. The carrier evaporates after spreading and leaves a film with a low proportion of mobile oil.
1.3Shift length color wear
What ifWhat if the film retained usable color for eight hours and released during evening cleansing?
Claim language“wear of at least 24 hours”
A flexible acrylic polymer binds pigment and accommodates skin movement during normal wear. A cleansing oil wets and softens the deposited film so that wiping lifts the pigment.
1.4Low tack after drying
What ifWhat if the applied film registered a tack reading below 150 at half an hour using the same measurement method?
Claim language“a tack of at least 150”
A volatile carrier leaves a polymer-rich film with a low fraction of mobile oil. Fine spherical silica reduces the contact area between the dried film and the tack probe.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Temporary color marker for animal coats
A grooming marker deposits a colored water-in-silicone emulsion on animal hair for visual identification during grooming. The continuous silicone phase contains MQ resin, an emollient, a silicone emulsifier, a thickener, and dispersed iron oxide pigment. A comb applicator lays the emulsion along a narrow band of hair, where carrier evaporation leaves a pigmented resin film around the fibers.
Component substitution
Silicone acrylate as the film former
An acrylates and polytrimethylsiloxymethacrylate copolymer replaces the MQ resin as the film former. The copolymer is dissolved in isododecane and blended with a silicone carrier, an emollient, a silicone emulsifier, and an oil-phase thickener before the aqueous phase is dispersed. After application, volatile carrier evaporates and concentrates the copolymer into a film that binds the pigment to the surface.
Parameter or scale variation
Water droplet size at pilot scale
A 10 kg pilot batch contains 20 wt.% dispersed aqueous phase and 25 wt.% emollient, with MQ resin, emulsifier, thickener, and pigment in the continuous silicone phase. A rotor-stator mixer disperses the aqueous phase at a 12 m/s tip speed while the batch stays at 20–25 °C. Mixing continues until microscopy shows a median water droplet diameter of 3–8 µm, after which low-speed agitation maintains bulk uniformity during filling.
Controlled film thickness and contact loading
A drawdown applicator deposits 25, 50, and 100 µm wet films of a pigmented water-in-silicone emulsion onto separate polymer-coated coupons. The continuous silicone phase contains MQ resin, an emollient, an emulsifier, and a thickener, and the coupons condition at 23 °C and 50% relative humidity. A texture analyzer presses a 5 mm flat probe against each film at 0.5 N for 1 second after 30 minutes and records peak pull-off force, while duplicate films undergo a 24-hour rub test to measure retained color.
Combination with existing systems
Metered application through a sponge tip
An airless piston cartridge feeds a pigmented water-in-silicone emulsion through a one-way outlet into a porous sponge tip. The continuous silicone phase contains MQ resin, an emollient, an emulsifier, and a thickener, and a positive-displacement pump delivers 60 µL per full stroke. The user spreads the metered dose with the sponge, and a gasketed cap limits carrier evaporation from the tip between applications.
Automated or data-driven variant
Image guided control of emulsification
A recirculating production vessel disperses an aqueous feed into a continuous silicone phase containing MQ resin, an emollient, an emulsifier, and a thickener. A side-stream imaging cell measures water droplet diameters, and software calculates the median and 90th-percentile values from each image set. The controller adjusts rotor speed and aqueous feed rate, then ends recirculation when both size values remain within their preset bands for three consecutive readings.
Specific version of a part
Glycerol in aqueous droplets
A 20 wt. % internal phase contains water, glycerol, and dissolved sodium chloride. A rotor-stator mixer disperses this phase into the silicone phase while a silicone polyether emulsifier stabilizes the droplet interfaces.
MQ resin in volatile carrier
Trimethylsiloxysilicate dissolves in isododecane and enters the continuous phase as a resin solution. The formulation contains 15 wt. % phenyl trimethicone as the emollient, a silicone polyether emulsifier, and a hectorite dispersion as the thickener.
Color retention through 24 hours
Surface-treated iron oxide particles remain embedded in a dried MQ resin film plasticized with low-volatility silicone oil. A wear test compares calibrated images of the same application area after dry-down and at 24 hours to assess retained color and coverage.
Probe tack after 30 minutes
A blend of MQ resin and high-viscosity dimethicone leaves a compliant film as the volatile carrier evaporates. A probe tack test uses a fixed contact load, dwell time, and withdrawal speed to measure peak detachment force at 30 minutes, with a target reading of at least 150 on the test scale.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
This two phase emulsion (e.g., oil is the continuous phase whereas water is the discontinuous phase) can include (a) a water phase comprising 5, 10, 20, 30, 40, 50, 60, 70, 80, 90, 95% or more or less or any range therein by weight of water based on the total weight of the emulsion, wherein the water phase does not include a salt;
B · US 9,918,912 B2 · ¶ 24
1.2a continuous oil phase comprising: a film former including an MQ resin; an emollient in an amount of 10.0-35.0 wt. % of the formulation; an emulsifier; and a thickener,
(b) an oil phase comprising 5, 10, 20, 30, 40, 50, 60, 70, 80, 90, 95% or more or less or any range therein by weight of oil based on the total weight of the emulsion;
B · US 9,918,912 B2 · ¶ 24
1.3wherein the formulation subsequent to application to a surface demonstrates wear of at least 24 hours, and
1.4wherein the formulation subsequent to application to the surface demonstrates a tack of at least 150 at half an hour subsequent to application to the surface.
This resin sheet, for sealing an electronic device, has a probe tack of 5 to 500 g at 25° C. The tack is measured, using a probe having a diameter of 25 mm.
A · US 2016/0269000 A1 · abstract
An empty cell means only that no passage was reproduced there.
Statements in these documents
However, according to the method described in each of Patent Documents 1 and 2, the resin sheet easily contacts the internal surface of the bag so that the resin sheet is easily shifted out of position.
A · US 2016/0269000 A1 · ¶ 6
Since the resin sheet satisfies this tack property, the sheet is not easily shifted out of position.
A · US 2016/0269000 A1 · ¶ 8
The emulsions can be used in cosmetic, food, and pharmaceutical applications.
B · US 9,918,912 B2 · ¶ 2
The emulsion has been shown to exhibit increased stability, an increased capacity to hold water, and can be made using standard mixing procedures and without the use of an external heating source.
B · US 9,918,912 B2 · ¶ 7
Cite aspatent.fyi, US 2026/0355099 A1, claim 1, first published 2026-11-19T07:53:10-05:00, https://patent.fyi/US20260355099/, SHA-256 10d7f38ddd9c616803adfb77bbd70c9a80c2357c94dbaed5912bea0ee8beb737