1.1Coarser crystalline feed
A first milling stage uses 1 mm beads to break down the coarse feed. A second stage uses 0.1 mm beads to increase the frequency of contacts with the finer particles and continue impact-driven disordering.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A first milling stage uses 1 mm beads to break down the coarse feed. A second stage uses 0.1 mm beads to increase the frequency of contacts with the finer particles and continue impact-driven disordering.
A loss-in-weight feeder meters powder to a slurry tank, and a pump feeds the slurry to the mill. Beads occupy 70% of the chamber volume on a settled-bulk basis, and an outlet screen retains them as the slurry passes through.
Anhydrous ethanol wets the calcium phosphate powder and forms a pumpable suspension for bead milling. A jacketed chamber removes heat while bead impacts fracture the suspended particles and introduce lattice disorder.
The drive reverses the chamber at each end of its stroke, and bead inertia produces motion relative to the chamber and slurry. Repeated bead collisions fracture particles and introduce lattice disorder.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A batch bead mill grinds crystalline calcium phosphate in acetone using the specified powder-to-bead and acetone-to-charge ratios. A screen retains the beads, and a vacuum dryer removes acetone from the milled slurry and condenses it for recovery. A pan granulator combines the recovered powder with a starch binder and forms granules for soil application.
Anhydrous ethanol replaces acetone in a sealed stirred bead mill. The vessel holds crystalline calcium phosphate powder and ceramic beads at a 1:3 apparent-volume ratio, and ethanol is added at a 7:1 mass ratio to the combined powder and beads. The agitator drives bead impacts through the slurry, and a screen separates the beads from the milled suspension. Laser diffraction measures particle size, and powder X-ray diffraction with an internal reference measures residual crystallinity.
The first milling stage uses 2.5 mm ceramic beads at a 1:3 apparent-volume ratio of starting powder to beads and a 7:1 mass ratio of acetone to the combined charge. A bead-retention screen transfers the slurry to a second vessel charged with 0.10 mm beads at the same apparent-volume ratio relative to the starting powder. The first stage breaks down larger particles, and the second stage continues grinding until sampled particle size and residual crystallinity reach their setpoints.
A bead-retention screen at the mill outlet feeds a sealed, agitated surge tank connected to a solvent-rated spray dryer. A metering pump feeds the acetone slurry to an atomizer, and recirculating nitrogen evaporates the solvent from the droplets. A cyclone collects the dried powder, and a condenser removes acetone from the nitrogen before the gas returns to the dryer.
The bead mill outlet passes through a bead-retention screen and feeds an enclosed continuous centrifugal classifier rated for acetone. The classifier sends the coarse fraction back to the mill and directs the fine fraction to an agitated collection vessel. A variable-speed pump and adjustable classifier rotor set the separation point, which is checked by laser diffraction on samples from both outlets.
A screened bypass supplies slurry to a laser diffraction instrument, and an automated sampler filters and dries a second aliquot for powder X-ray diffraction. The controller calculates the particle size distribution and estimates the crystalline mass fraction from diffraction data using a reference added after sampling. The controller stops the rotor when both measurements enter their configured endpoint bands and logs the results with the elapsed milling time.
A pressurized acetone jet draws dry powder into the eductor throat, where jet shear breaks loose clumps and wets the particles. The outlet feeds the suspension to a chamber preloaded with grinding beads.
Crystalline calcium phosphate powder with particle diameters of 2–4 μm is charged with 0.3 mm yttria-stabilized zirconia beads. The charge uses 100 mL of apparent powder volume and 300 mL of apparent bead volume.
The slurry uses 800 g of acetone per 100 g of combined powder and beads. A paddle agitator disperses the powder through the liquid before the grinding run begins.
A fixed-speed drive and timer execute a batch grinding run at a set rotation rate and duration. Particle sizing checks the 0.1–1.2 μm interval, microscopy checks for aggregates, and X-ray diffraction with an internal standard measures the residual crystalline fraction against the 10–50% target.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Operating conditions for the stirred media mill for producing the nanoparticles are given below: Bead size is 0.4 mm-0.6 mm Pin tip velocity is 6-10 m/s (stirrer speed) Slurry concentration is 20-50% (wt % of particle in slurry) Bead density of 4.0 g/cc, 6.0 g/cc and above 7.0 g/cc (i.e from 2.8 to 16 g/cc) Bead loading is 30-90% of mill volume Slurry loading (material loading) 70-100% of void volume of bed of beads (grinding media) Viscosity is modified during grinding SurfaA · US 2009/0084874 A1 · ¶ 54
Sitagliptin phosphate (4.0 g) was suspended in 50 ml boiling acetone (HPLC grade).B · US 2009/0247532 A1 · ¶ 79
Accordingly, the preset invention is related to a method of producing nanoparticles of size less than 100 nm using stirred media mill, said method comprising steps of: a. grinding slurry having particle concentration ranging between 20 to 50 wt % with beads occupying 60 to 90% of the mill volume at pin-tip velocity ranging between 6 to 10 m/s, b. maintaining viscosity and pH of the slurry during the grinding, and c. obtaining nanosized particle in time duration ranging betweeA · US 2009/0084874 A1 · ¶ 38
An empty cell means only that no passage was reproduced there.
At present stirred media mill suffers from contamination, high power consumption, and lack of knowledge of the optimized operating conditions (inefficient in grinding).A · US 2009/0084874 A1 · ¶ 6
Also, the existing mills are designed to operate at low rpm (to avoid contamination, i.e. wear of grinding chamber), and will take at least 20 hours of grinding to achieve the particle size that this process can do it at 45 minutes.A · US 2009/0084874 A1 · ¶ 6
Sitagliptin or sitagliptin phosphate is a dipeptidyl peptidase-IV (DPP-IV) inhibitor and is useful for the treatment and prevention of Type 2 diabetes, hyperglycemia, insulin resistance, obesity, and high blood pressure.B · US 2009/0247532 A1 · ¶ 4
Amorphous material is usually less stable, both chemically and physically, relative to crystalline forms.B · US 2009/0247532 A1 · ¶ 8
patent.fyi, US 2026/0355385 A1, claim 1, first published 2026-11-19T10:59:45-05:00, https://patent.fyi/US20260355385/, SHA-256 45efbc185dee259e1da5012a612aeadc94edfcfeb36bb9119d644549707b8bb4