Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
No entries.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Conductive glass beads for shielding
A shallow vibrating tray in a vacuum chamber holds glass microspheres for use as conductive filler in shielding gaskets. An argon ion source cleans the bead surfaces while the tray turns the beads. A sputtering source deposits nickel onto the moving beads until the coating covers their surfaces. A mixer disperses the coated beads into an elastomer before molding.
Component substitution
Rotating drum for particle turnover
A horizontal rotating drum with internal lifting ribs replaces the vibrating substrate holder inside the vacuum chamber. An opening in one end of the drum faces an argon ion source and a sputtering source, each aimed at the falling particle curtain. The ribs lift the particles and release them into the curtain on each revolution. The ion source cleans the exposed surfaces before the sputtering source deposits the shell during continued rotation.
Electron beam evaporation of shells
An electron beam evaporator with a water-cooled hearth replaces the sputtering source beneath an inclined, vibrating particle tray. The tray has a retaining lip and positions the moving particle bed in the line of sight of the vapor source. An argon ion source treats the particles before the evaporation shutter opens. The electron beam heats copper in the hearth, and tray motion repeatedly exposes fresh particle surfaces to the copper vapor.
Parameter or scale variation
Thin shells on ceramic beads
A vacuum-compatible tray holds 100 to 200 micrometer alumina beads in a bed 0.5 to 1 millimeter deep. A shaker sweeps from 40 to 120 hertz, and operation continues at the frequency that produces sustained bead turnover. An argon ion beam cleans the moving beads before a sputtering source deposits a 100 to 300 nanometer titanium shell. Cross sections of sampled beads provide a thickness measurement for setting the deposition time for subsequent batches.
Combination with existing systems
Coating cells with vacuum transfer
A vacuum transfer chamber connects a load lock, an ion treatment chamber, and a sputter coating chamber through gate valves. A transfer arm moves a shallow particle tray between chambers and docks it on a shaker in each process chamber. The first shaker turns the particles during ion cleaning, and the second turns them during shell deposition. The load lock vents for tray exchange while the two process chambers remain under vacuum.
Automated or data-driven variant
Camera control of particle turnover
A camera outside the chamber views the vibrating particle tray through a window and records particle motion under pulsed illumination. Software tracks surface texture across successive images and measures the fraction of the bed that moves during each observation interval. A controller adjusts shaker amplitude to maintain the moving fraction measured during a reference run with sustained turnover. The controller closes the deposition shutter when the moving fraction stays below the control limit for a preset interval and reopens it when turnover recovers.
Cite aspatent.fyi, US 2026/0355720 A1, claim 1, first published 2026-11-19T14:30:38-05:00, https://patent.fyi/US20260355720/, SHA-256 4aab751e1d97a7691528ffe68ab943a7de1eceb61260d0c538e493ff6c78ad31