patent.fyi
Applications  /  US 2026/0355724
United States Patent Application Publication

US 2026/0355724 A1

Published
Nov 12, 2026
Filed
Jan 4, 2024
Earliest date on the face
Jan 28, 2023
Classification
B01J 27/053
First published here
Nov 19, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.3Magnesium acetate feed

What ifWhat if magnesium acetate supplies the metal to the substrate mixture?
Claim language“a metal nitrate”

Dissolve magnesium acetate in deionized water and add it to the acidified micellar dispersion. Stir in the silicate so the dissolved magnesium is distributed through the mixture as the silica network gels.

1.5Single initiator charge

What ifWhat if the initiator enters the reactor in a single charge?
Claim language“adding an initiator dropwise”

Meter one charge of aqueous potassium persulfate into a stirred, nitrogen-purged styrene dispersion at 70 °C. The initial burst of radicals nucleates particles, which grow as styrene diffuses from the monomer droplets.

1.6Washed aqueous sphere dispersion

What ifWhat if the washed nanospheres remain in an aqueous concentrate through blending?
Claim language“washing and then vacuum drying”

Wash and concentrate the latex by tangential-flow ultrafiltration, then measure its polymer solids content. Meter the wet concentrate by its dry polymer mass and deduct its water from the substrate formulation.

1.7Static mixing before gelation

What ifWhat if an inline static mixer blends the substrate solution and the nanosphere dispersion?
Claim language“homogenization by stirring”

Meter both streams into a tube containing fixed helical mixing elements. The elements repeatedly divide and recombine the streams, and the blended suspension flows into an aging vessel before gelation.

1.10Centrifugal recovery after leaching

What ifWhat if centrifugation recovers the catalyst precursor from the leaching solvent?
Claim language“a first vacuum filtration”

Spin the leached slurry in solvent-compatible centrifuge vessels to sediment the inorganic precursor. Decant the solvent containing dissolved polymer, then resuspend and sediment the solids in fresh solvent to wash them.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Catalyst for synthetic lubricant base stocks

The porous silica catalyst carries basic sites in its skeleton and sulfated zirconia acid sites on its pore walls. A stirred batch reactor suspends the catalyst in a hydroxyl-terminated polyol ester and a fatty acid feed. Dry nitrogen sweeps reaction water into an overhead condenser as esterification proceeds. A heated filter separates the catalyst from the ester base stock before vacuum stripping removes residual fatty acid.

Component substitution

Wax spheres as the hard template

Solid paraffin microspheres replace the polymer colloid nanospheres as the macropore template. An aqueous wax emulsion cools below the wax melting point, and wet sieving isolates the target sphere size fraction before blending with the acidified silicate and polyether mixture. The gel ages below the wax melting point, and heptane extracts the spheres from the aged gel. The washed skeleton receives the metal precursor, followed by hydrolysis, sulfate impregnation, and calcination.

Aqueous zirconium deposition on porous silica

An aqueous zirconyl acetate solution replaces the organic zirconium precursor and organic solvent. The dried, leached silica skeleton takes up a volume of solution equal to its measured water uptake at incipient wetness. Dilute ammonia vapor hydrolyzes the deposited zirconium species inside the pores, and a water wash removes soluble acetate salts. The dried solid receives ammonium sulfate by impregnation and then undergoes calcination.

Parameter or scale variation

Two separate macropore size populations

Two batches of polystyrene spheres with nominal diameters of 200 nm and 800 nm form the hard template. The batches are blended in a 1:1 dry mass ratio and dispersed together in the liquid silica precursor before gelation. Solvent extraction after aging removes both sphere populations and leaves two populations of cavities. Scanning electron microscopy of fractured, calcined granules measures the final cavity sizes after shrinkage.

Combination with existing systems

Packed bed with external water removal

A heated recirculation loop passes an insulating oil esterification mixture through a packed bed of 1 to 2 mm catalyst granules screened from the dried and calcined gel. The bed outlet discharges into a vacuum flash vessel that removes reaction water overhead. A condenser collects the vapor, and a pump returns the liquid to the bed through a feed heater. Bed inlet and outlet pressure taps track the pressure drop during circulation.

Automated or data-driven variant

Optical endpoint for template extraction

A stirred extraction vessel holds the gel in a removable perforated basket and circulates solvent through a filtered ultraviolet flow cell. The controller uses a calibration for dissolved polystyrene at 260 nm and subtracts the absorbance of fresh solvent. At fixed intervals, the controller drains and replaces the solvent while retaining the gel in the basket. It ends extraction when two consecutive fresh-solvent charges each acquire less than 0.1 g/L of dissolved polymer during a 20-minute circulation period.

Specific version of a part

Magnesium nitrate and sodium silicate

Dissolve the PEO–PPO–PEO triblock polyether in deionized water, acidify with hydrochloric acid, and let the mixture stand for micelle formation. Stir in magnesium nitrate and sodium silicate at a polyether-to-nitrate-to-silicate molar ratio of 1:6:80.

Styrene nanospheres with persulfate

Add an aqueous potassium persulfate solution dropwise to stirred styrene and ultrapure water at 70 °C under nitrogen. Wash the resulting polystyrene nanospheres with ultrapure water and vacuum-dry them at 40 °C.

Three to two blending ratio

Add 20 g of dried polymer nanospheres to 30 g of substrate solution. Stir with a pitched-blade impeller until the spheres are dispersed, then age the mixture in a covered vessel until it gels.

Tetrahydrofuran extraction of polystyrene

Stir pieces of the aged skeleton in tetrahydrofuran at room temperature to dissolve the polystyrene spheres. Recover the porous solid by vacuum filtration and wash the filter cake with fresh tetrahydrofuran.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 6,911,192 B2
Published
Jun 28, 2005
Filed
Jun 28, 2002
Document BUS 2019/0336932 A1
Published
Nov 7, 2019
Filed
Feb 17, 2018
Class
B01J 19/0046
Claim 1
Document A
Document B
1.1(1) constructing a catalyst alkaline skeleton
(ii) adding an inorganic low molecular weight compound having hydrolyzable functional groups to said homogeneous solution so as to cause a sol-gel reaction, thereby forming a gel of a continuous three-dimensional network structure composed of a solvent-rich phase which is rich in the solvent and a skeleton phase which is rich in an inorganic oxide polymer adhered to the surface of the amphiphilic substance template wherein the inorganic oxide polymer is produced from said ino
A · US 6,911,192 B2 · ¶ 13
1.2(a), preparing a catalyst alkaline substrate
The method of the present invention for producing an inorganic porous body concurrently having mesopores and macropores thus starts with the step of preparing a homogeneous solution by dissolving an amphiphilic substance as template component into an aqueous solution containing a sol-gel reaction catalyst.
A · US 6,911,192 B2 · ¶ 31
In step 2, the precursors solutions are prepared to generate a target product by using one kind or a mixture of two or more kinds of metal species, graphene oxide, MXene, carbon nanotubes, metal nanoparticles, oligomeric organosilicate (1,4-bis (triethoxysilyl) benzene, 1,2-Bis(triethoxysilyl)ethane, Bis[(3-trimethoxysilyl)propyl]amine (amine), Ethyltriethoxysilane) with amphoteric solvent.
B · US 2019/0336932 A1 · ¶ 24
1.3adding an amphiphilic block copolymer into deionized water, subjecting a resulting solution to acidification by adding an acid, mixing, and subjecting a resulting mixture to standing to allow self-assembly to form a lyotropic liquid crystal micelle, and then adding a metal nitrate and a silicate into the lyotropic liquid crystal micelle and stirring to obtain a catalyst alkaline substrate solution A;
Ethylene oxide-propylene oxide-ethylene oxide block copolymer (EO20-PO70-EO20, average molecular weight: 5800, Aldrich), an amphiphilic substance, 2.10 g was dissolved in 1 mol/L nitric acid aqueous solution 10.0 g. To the resultant homogeneous solution was added tetramethoxysilane 5.15 g while stirring to carry out hydrolysis.
A · US 6,911,192 B2 · ¶ 41
1.4(b), preparing a monodisperse polymer colloid nanosphere used as a macroporous template
In step 1, the pore-forming template agent solutions are prepared by using one kind or a mixture of two or more kinds of polymer nanospheres, carbon blacks, carbon nanotubes, carbon nanofibers, carbon nanospheres, and poly(methyl methacrylate (PMMA) microspheres, polystyrene nanosphere, latex spheres, and inorganic nanoparticles, silica nanoparticles, carbon nanoparticles, carbon dots, carbon nanocells, polymer with amphoteric solvent.
B · US 2019/0336932 A1 · ¶ 24
1.5adding an initiator dropwise into a polymer monomer and ultrapure water under inert gas protection and stirring, and conducting a reaction to obtain white polymer colloid nanospheres, and subjecting the white polymer colloid nanospheres to washing and then vacuum drying to obtain nanospheres B; alternatively,
1.6adding an initiator dropwise into a polymer monomer, a coupling monomer, an emulsifier, and ultrapure water under inert gas protection and stirring, and conducting a reaction to obtain white polymer colloid nanospheres, and then subjecting the white polymer colloid nanospheres to washing and then vacuum drying to obtain nanospheres B; and
1.7(c), blending and gelling the catalyst alkaline substrate and the macroporous template, mixing the catalyst alkaline substrate solution A and the nanospheres B, and subjecting a resulting system to homogenization by stirring, and then aging to obtain a catalyst alkaline skeleton C; and
After stirring for several minutes, the resultant clear solution was transferred into a closed vessel, which was thermostatted at 40° C. In some 120 minutes, the solution became turbid and solidified.
A · US 6,911,192 B2 · ¶ 41
Each dot has independent compositions of at least one of the precursor solutions and at least one of the pore-forming template agent solutions. In step 5, evaporating the amphoteric solvent, the composite meso/macrostructures can be formed into as-synthesized film array.
B · US 2019/0336932 A1 · ¶ 24
1.8(2) leaching the macroporous template in the catalyst alkaline skeleton C and loading a solid superacid active site
And finally in step 6, heating the as-synthesized film array to remove the organic pore-forming template, and/or treating the film array by NaOH or HF aqueous solution to remove silica template, to generate a 3D macroporous and mesoporous structured material array.
B · US 2019/0336932 A1 · ¶ 24
1.9(a), leaching the macroporous template in the catalyst skeleton
1.10adding the catalyst alkaline skeleton C into a solvent of a polymer hard template, subjecting an obtained mixture to stirring, leaching, and a first vacuum filtration in sequence, and then washing an obtained filter cake to obtain a catalyst precursor D in which the microporous template is removed; and
1.11(b), loading an acidic active site in a catalyst
Doping active elements into a macroporous/mesoporous structure substrate can greatly improve the effectiveness of catalysts and nanosensors.
B · US 2019/0336932 A1 · ¶ 3
1.12adding the catalyst precursor D into an organic solvent, adding an organic metal compound under inert gas protection and stirring, conducting a reaction, and subjecting a resulting reaction product to a second vacuum filtration to obtain a first filter cake, and then drying the first filter cake to obtain a dry filter cake; subjecting the dry filter cake to hydrolysis to obtain a hydrolysis filter cake, and then subjecting the hydrolysis filter cake to vacuum drying to obtain a powder E; and impregnating the powder E with an alcohol solution of ammonium sulfate under stirring at room temperature, subjecting an obtained system to a third vacuum filtration to obtain a second filter cake, and then subjecting the second filter cake to vacuum drying and calcination in sequence to remove a polyether in the second filter cake to obtain the solid acid-base catalyst for producing the insulating oil of the transformer; wherein the amphiphilic block copolymer in (a) of step (1) is a polyether having a structure of poly(ethylene oxide) (PEO)-poly(propylene oxide) (PPO)-PEO; a molar ratio of the amphiphilic block copolymer, the metal nitrate, and the silicate in (a) of step (1) is in a range of 1:5-8:60-110; a mass ratio of the catalyst alkaline substrate solution A to the nanospheres B in (c) of step (1) is in a range of 3:2 to 4:2; in (b) of step (2), the organic metal compound is one or two selected from the group consisting of an organic titanium compound and an organic zirconium compound, and a mass ratio of the catalyst precursor D to the organic metal compound is in a range of 1:1 to 4:1; and in (b) of step (2), the reaction is conducted at a temperature of 50 °C to 80 °C for 24 hours to 48 hours, the impregnating is conducted for 2 hours to 6 hours, the calcination is conducted at a temperature of 400 °C to 700 °C for 4 hours to 6 hours, and the alcohol solution of the ammonium sulfate has a concentration of 0.1 mol/L to 0.4 mol/L.

An empty cell means only that no passage was reproduced there.

Statements in these documents
The method of the present invention is suitably applied to the production of porous bodies for use as packing materials for chromatography, porous bodies for blood separation, porous bodies for moisture absorption, deodorizing porous bodies for low molecular substance adsorption, porous bodies for enzyme or catalyst supports and the like.
A · US 6,911,192 B2 · ¶ 1
A complicated and time-consuming process is required to produce a porous assembly by which a target substance can be smoothly introduced into nanometer-sized pores (mesopores) for contact therewith, or a bulk material having a macropores structure satisfying such condition.
A · US 6,911,192 B2 · ¶ 8
However, the big limitation for HTE is lack of fast synthesis techniques to generate large-volume, high-precision controlled 3DMM material array (compositions, pore size, and pore structure).
B · US 2019/0336932 A1 · ¶ 3
The 3DMM material array can be used for the rapid synthesis, screening and manufacture of catalysts and nanosensors.
B · US 2019/0336932 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0355724 A1, claim 1, first published 2026-11-19T14:56:45-05:00, https://patent.fyi/US20260355724/, SHA-256 7834795fa93c0b890a89a64d49b0cd16d3fe295dd793c40dd564ed817515b80a
First published
Permanent addresshttps://patent.fyi/US20260355724/
Content fingerprint (SHA-256)7834795fa93c0b890a89a64d49b0cd16d3fe295dd793c40dd564ed817515b80a
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi