patent.fyi
Applications  /  US 2026/0355730
United States Patent Application Publication

US 2026/0355730 A1

Published
Nov 12, 2026
Filed
Nov 20, 2023
Earliest date on the face
Dec 8, 2022
Classification
B01J 37/0203
First published here
Nov 19, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.2Continuous titanium dioxide coating

What ifWhat if a continuous titanium dioxide film covered the support surface?
Claim language“particles of at least one oxide of a metal”

Alternating pulses of a titanium precursor and water grow a conformal film on mesoporous silica. Gold deposits on the exposed film, which provides a gold–oxide interface wherever a gold particle attaches.

1.2Iron oxide surface particles

What ifWhat if iron oxide particles provided the oxide surface for gold deposition?
Claim language“aluminum, titanium, lanthanides, zirconium, nickel, cobalt, zinc, tellurium, antimony, bismuth, rhenium, tungsten”

Hydrolysis of a dilute iron nitrate solution deposits an iron hydroxide precursor on silica. Calcination converts the deposit to iron oxide, and subsequent deposition of a gold precursor places gold on the iron oxide surface.

1.3Deposition of preformed gold

What ifWhat if preformed metallic gold nanoparticles supplied the gold in a washed aqueous dispersion?
Claim language“a gold salt”

A dispersion containing citrate-stabilized gold nanoparticles contacts silica bearing titanium dioxide particles at a pH below the titanium dioxide point of zero charge. The positively charged oxide surface adsorbs the negatively charged gold nanoparticles, and a water rinse removes unbound particles.

1.4Room temperature chemical reduction

What ifWhat if sodium borohydride converted the adsorbed gold precursor to metallic gold at 20 °C?
Claim language“heating the support”

The oxide-bearing support contacts a dilute gold salt solution and is rinsed to remove dissolved precursor. A freshly prepared aqueous sodium borohydride solution reduces the retained gold species to metallic nanoparticles, and a final water wash removes soluble residues.

1.4Gold on separate silica grains

What ifWhat if the gold nanoparticles occupied silica grains whose nearest metal oxide particles were more than 20 nm away?
Claim language“within 20 nm of a particle”

A catalyst cartridge holds gold-bearing mesoporous silica granules in one compartment and metal-oxide-bearing granules in another, with a porous frit between them. Methacrolein, methanol and dissolved oxygen flow through the gold-bearing compartment, where exposed gold surfaces provide sites for oxidative esterification.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Carbon monoxide removal from process air

Titanium dioxide particles coat porous silica granules, and heating converts a deposited gold precursor to gold nanoparticles next to the titanium dioxide. The granules fill a fixed-bed cartridge between retaining screens downstream of a particulate filter. Oxygen in the process air reacts with carbon monoxide at the supported gold particles to form carbon dioxide, and an outlet sensor measures residual carbon monoxide.

Component substitution

Preformed gold colloid replaces gold salt

A citrate-stabilized colloid containing 4 to 6 nm metallic gold particles replaces the gold salt at the support-contact step. An aqueous slurry of silica granules bearing alumina particles is adjusted to pH 5 to promote adsorption of the negatively charged gold colloid onto the alumina. Filtration and rinsing remove free colloid, and a 200 °C air treatment removes surface citrate.

Parameter or scale variation

Thin catalyst coating on channel walls

A silicon carbide honeycomb with 1.5 mm square channels carries a 30 to 50 μm porous silica coating on its channel walls. An aqueous dispersion deposits 20 to 40 nm zirconia particles in the coating, and a gold salt solution enters the coated channels before drainage. A 2 h hold at 250 °C forms gold nanoparticles in the coating, and electron micrographs of sections from the inlet, middle, and outlet show the particle size and distribution along the channels.

Combination with existing systems

Catalyst bed with methanol solvent recovery

Gold nanoparticles on zirconia-decorated silica granules fill a jacketed trickle-bed reactor supplied with methacrolein, methanol, and a metered oxygen-containing gas. A downstream gas–liquid separator sends the liquid effluent to a distillation column that recovers a methanol-rich overhead stream. A condenser and liquid receiver return a controlled fraction of the recovered methanol to the reactor feed, and a purge limits accumulation of recycled impurities.

Automated or data-driven variant

Automated microscopy of gold particle placement

An automated scanning transmission electron microscope acquires images and elemental maps from randomly selected fields of cross-sectioned gold catalyst granules bearing zirconia particles. Image-analysis software segments the gold particles and zirconia regions, calculates projected gold particle diameters, and measures the shortest projected edge-to-edge distance from each gold particle to zirconia. The software records the mean and standard deviation of the diameters and the number fraction within a projected distance of 20 nm, then flags batches for review against configured limits.

Feedback control of gold precursor uptake

A stirred vessel holds silica granules bearing titania particles, and a metering pump adds an aqueous gold salt solution while a pH probe regulates the addition of dilute base. A filtered sampling loop measures dissolved gold by ultraviolet–visible absorbance using standards prepared at the operating pH and chloride concentration. A controller estimates uptake from the cumulative gold dose and dissolved gold inventory, then initiates filtration and rinsing when uptake reaches the target and levels off. The recovered granules enter a programmable furnace for conversion of the deposited precursor to metallic gold.

Specific version of a part

Porous carbon catalyst support

Oxygen-containing groups on the carbon surface anchor the precursor used to deposit titanium dioxide particles. Mesopores expose the titanium dioxide and supported gold to the liquid reaction mixture.

Mesoporous silica granule support

The support consists of amorphous silica granules screened to 150–300 µm. Mesopores with diameters of 15–30 nm provide internal surface for oxide deposition and liquid access.

Titanium dioxide surface islands

Dilute titanium alkoxide impregnates silica granules at low surface coverage. Controlled hydrolysis followed by calcination forms discrete titanium dioxide particles on the silica surface.

Aqueous chloroaurate deposition

Titanium dioxide-bearing silica contacts a dilute aqueous sodium tetrachloroaurate solution adjusted to pH 7–8. Hydrolysis promotes deposition of gold species on the oxide surface, and a water rinse removes residual chloride.

Thermal conversion under dilute hydrogen

A tube furnace holds the impregnated support at 200 °C for 2 h under 5% hydrogen in nitrogen to reduce the deposited gold species. Electron microscopy with elemental mapping measures gold particle diameters and nearest oxide distances, with targets of a mean below 12 nm, a standard deviation of 4 nm and at least 75% of the gold particles within 20 nm of an oxide particle.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 8,329,613 B2
Published
Dec 11, 2012
Filed
Aug 1, 2006
Class
B01J 23/44
Document BUS 10,940,460 B2
Published
Mar 9, 2021
Filed
May 9, 2016
Class
B01J 21/16
Claim 1
Document A
Document B
1.1providing a support, wherein the support comprises a material selected from the group consisting of an oxide of silicon, a carbide of silicon, a metal oxide, and a metal carbide;
Preferably, metal oxides such as aluminum oxide, titanium dioxide or silicon oxide are used as the support.
A · US 8,329,613 B2 · ¶ 21
1.2providing particles of at least one oxide of a metal on a surface of the support, wherein the metal is selected from the group consisting of aluminum, titanium, lanthanides, zirconium, nickel, cobalt, zinc, tellurium, antimony, bismuth, rhenium, tungsten, alkali metals, and alkaline earth metals,
The method according to claim 1, wherein doping agents, selected from oxides of the alkali metals, alkaline earth metals, and rare earth metals, are added to the support and/or the precursor solution.
A · US 8,329,613 B2 · claim 8
The open, porous network of the expanded clay is stabilized by the intercalated aluminum-rare earth or lanthanide element-oxygen structures between the interlayers of the clay.
B · US 10,940,460 B2 · ¶ 12
1.3contacting the support with a gold salt,
The technical problem of the invention is solved by providing a method for producing a supported gold catalyst from a porous metal oxide support and a chloroauric acid precursor, wherein in a step a) the metal oxide support is prepared, in a step b) the support is placed in contact with an aqueous solution of the chloroauric acid precursor.
A · US 8,329,613 B2 · ¶ 11
An aqueous solution of a metal salt such as zinc chloride or magnesium chloride is prepared and the pillared clay is contacted with or added to the solution, preferably with stirring.
B · US 10,940,460 B2 · ¶ 118
1.4heating the support at a temperature ranging from 50 °C to 600 °C for a time ranging from at least 0.1 h to 48 h to convert the gold salt to gold nanoparticles having an average diameter less than 12 nm and a standard deviation of +/−4 nm, wherein at least 75% by number of the gold nanoparticles are positioned within 20 nm of a particle of the oxide of the metal.
The catalyst of the invention is characterized especially in that the average size of the gold particles on the support is essentially smaller than 10 nm, preferably smaller than or equal to 5 nm, especially preferably from 1 nm to 2 nm.
A · US 8,329,613 B2 · ¶ 28

An empty cell means only that no passage was reproduced there.

Statements in these documents
For this reason, it is necessary for new catalyst types to be developed, which will enable effective catalytic oxidation, especially of carbohydrates, for example for the production of aldonic acids using dioxygen as the oxidation agent, and which, in addition to high activity and selectivity, will have a long lifespan.
A · US 8,329,613 B2 · ¶ 6
The invention also relates to a metal oxide supported gold catalyst and its use in the oxidation of alcohols, aldehydes, polyhydroxy compounds and carbohydrates.
A · US 8,329,613 B2 · ¶ 2
However, aluminoxane and borate activators are both expensive and difficult to handle, particularly in a commercial setting, and thus there is a continuing need for improved activators.
B · US 10,940,460 B2 · ¶ 3
By combining properties of a support such as pillared clay with those of an activator, heterogeneous metallocene catalysts can be further improved.
B · US 10,940,460 B2 · ¶ 4
Cite aspatent.fyi, US 2026/0355730 A1, claim 1, first published 2026-11-19T14:56:45-05:00, https://patent.fyi/US20260355730/, SHA-256 523abd7e87e214168e7f6f7a72d63316558bb7f14608ebb65fa2f801f66b3b6e
First published
Permanent addresshttps://patent.fyi/US20260355730/
Content fingerprint (SHA-256)523abd7e87e214168e7f6f7a72d63316558bb7f14608ebb65fa2f801f66b3b6e
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi