Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Profile a seamless tube
What ifWhat if the wall thickness profile were formed on a seamless tube?
Claim language“forming a wall profile on a metal strip”
A cold pilger mill works a seamless steel tube between grooved rolls and a tapered internal mandrel. Programmed axial positioning changes the clearance between the roll pass and mandrel along the tube, producing the required wall thickness profile before reel winding.
1.2Use a discrete wall step
What ifWhat if two constant wall thicknesses met at a discrete step?
Claim language“a first taper between the first and second wall thicknesses”
A square butt weld joins two flat strips of different gauges with their outer faces flush. The joined strip is roll formed and longitudinally seam welded, leaving the thickness step on the inside of the tube.
1.3Keep both profiles connected
What ifWhat if both profile sections stayed connected throughout tube forming?
Claim language“segmenting the metal strip into a first strip section and a second strip section”
The rolling mill creates both profile sections in their required axial sequence on one continuous strip. A strip accumulator feeds the profiled strip to the forming rolls and seam welder without a transverse cut between the sections.
1.4Join lengths after tube forming
What ifWhat if the two strip sections were formed into tubes before their ends were joined?
Claim language“coupling an end of the first strip section to a first end of a third strip section”
Each strip section passes separately through forming rolls and a longitudinal seam welder. An orbital welding head makes a circumferential butt weld between the finished tube ends, and the joined tubing is wound onto a reel.
1.5Form tubing by hot piercing
What ifWhat if the coiled tubing were formed from a solid steel billet?
Claim language“forming a first section of coiled tubing from the new metal strip”
Oblique rolls push a heated billet over a piercing plug to produce a seamless hollow. A mandrel mill elongates and thins the hollow, and a sizing mill establishes the outside diameter before the tubing cools and is wound onto a reel.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Coiled wash tubing for process vessels
A reel feeds stainless steel tubing through a guide to a rotary wash head inside a process vessel. A profiled strip is cut to isolate a tapered section, and its thick end is butt joined to a constant-thickness strip for the reel end. The joined strip is roll formed, longitudinally seam welded, and wound with the thinner end accessible for attachment to the wash head.
Component substitution
Forged strip joint by flash welding
A flash butt welder replaces the transverse fusion welding head at the strip joining station. Water-cooled clamps align the edges and forming face of the tapered strip section with those of the extension strip. The machine flashes the opposed ends and then drives them together under axial force. Opposed planishing rolls flatten the hot upset before the joined strip enters the tube forming stands.
Local strip profiling with a press
A servo-hydraulic press with wide, radiused dies forms the thickness taper by incremental compression. An indexed feed advances the strip in overlapping steps while the press varies the die gap along the taper and holds it fixed over each constant-thickness section. The starting strip width accounts for lateral spread, and side-sizing rolls restore a constant width before segmentation. A transverse butt joint connects the selected section to an extension strip, and a tube mill forms and seam welds the assembly.
Parameter or scale variation
Two taper lengths in one coil
Two tapered sections are cut from profiled stock and assembled on either side of a 30 m strip section with a thickness of 2.6 mm. The first section tapers from 3.2 mm to 2.6 mm over 12 m, and the second tapers from 2.6 mm to 2.2 mm over 8 m. Transverse butt joints connect the sections at their 2.6 mm ends. The assembled strip passes through a tube mill and is wound as a single length of tubing with a 31.8 mm outside diameter.
Combination with existing systems
Tube mill with strip loop accumulator
A powered loop accumulator sits between the strip joining station and the first tube forming stand. Before a strip end reaches the joining station, the entry drive charges the accumulator with enough strip to cover the mill feed rate multiplied by the joining cycle time. The entry drive stops for end alignment and joining while the forming stands draw stored strip from the accumulator. After the joint clears the clamps, the entry drive runs above mill speed until the loop returns to its operating depth.
Automated or data-driven variant
Thickness mapped cutting and strip assembly
Opposed laser displacement sensors measure strip thickness, and an encoder assigns a longitudinal position to each measurement. A controller compares the measured profile with the specified endpoint thicknesses and taper length, then tracks the selected cut positions to a flying shear. Powered transfer tables index the cut section and an extension strip into a butt joining fixture with edge guides. The controller releases the joined strip to the forming line after a displacement sensor verifies alignment across the joint.
Specific version of a part
Hydraulic cold rolling control
A four-high cold rolling stand reduces low-carbon steel strip. A strip travel encoder indexes the hydraulic roll gap setpoint, and a downstream thickness gauge supplies feedback to correct the reduction.
Linear taper between plateaus
The first profile section has a 3.5 mm plateau and a 2.5 mm plateau linked by a 5 m linear taper. The thickness setpoint decreases by 0.2 mm per metre along the taper.
Encoder triggered flying shear
A measuring wheel tracks strip travel from the rolling stand to a flying shear. The shear carriage matches strip speed and executes a transverse cut at the boundary between the two profile sections.
Matched gauge laser butt weld
Clamps align square-cut strip ends of the same gauge over a copper backing shoe. A traversing laser head makes a full penetration weld across the strip width.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1forming a wall profile on a metal strip, the wall profile comprising: a first profile section with a first wall thickness, a second wall thickness, and
1.2a first taper between the first and second wall thicknesses; and a second profile section;
1.3segmenting the metal strip into a first strip section and a second strip section, wherein the first strip section comprises the first profile section and the second strip section comprises the second profile section;
Next, the first shearing blade 11 can be driven to cut the steel strip 6 by the commanding handle 15.
A · US 2008/0295665 A1 · ¶ 16
1.4coupling an end of the first strip section to a first end of a third strip section to form a new metal strip; and
After welding the oil separator bottom plate 104 with the first condenser dome shell 102, the second condenser dome shell 114 is welded with the first condenser dome shell 102 (with integrated oil separator) using the third seam welding 122 and the fourth seam welding 124, preferably but not limited to diagonally opposite ends to form a condenser from the first condenser dome shell and the second condenser dome shell.
B · US 11,499,763 B2 · ¶ 45
1.5forming a first section of coiled tubing from the new metal strip.
An empty cell means only that no passage was reproduced there.
Statements in these documents
That is, the hammer 7 has to be carried with the shearing device 1 any time, posing an inconvenience in practice.
A · US 2008/0295665 A1 · ¶ 4
The striking sleeve is engaged with the rear portion of the positioning rod and the struck block, able to move back and forth along the positioning rod to strike the struck block, so as to quickly squeeze a second shearing blade connected in front of the positioning rod into under a steel strip tied around a packing box, getting ready for shearing.
A · US 2008/0295665 A1 · ¶ 6
Since the oil separator needs to be welded inside the condenser shell, there is also a possibility of welding damage/leakage as oil separator sheet metal thickness is small.
B · US 11,499,763 B2 · ¶ 5
In view of the afore-mentioned problems, there is a need of an efficient and effective system and a method for manufacturing an integrated oil separator with the condenser which alleviates the problems in the existing internal oil separators.
B · US 11,499,763 B2 · ¶ 6
Cite aspatent.fyi, US 2026/0355804 A1, claim 1, first published 2026-11-19T15:46:13-05:00, https://patent.fyi/US20260355804/, SHA-256 94e70015b44cc73642a2c99a53e46cf976636eb0879ca12c85baa95b192d1039