patent.fyi
Applications  /  US 2026/0355815
United States Patent Application Publication

US 2026/0355815 A1

Published
Nov 12, 2026
Filed
Jun 19, 2023
Earliest date on the face
Aug 17, 2022
Classification
B22F 1/052
First published here
Nov 19, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Rounded silver powder

What ifWhat if rounded silver particles form the coarse fraction of the paste?
Claim language“silver flakes”

The paste contains 20 wt. % rounded silver particles with a D90 of 12 μm. Finer silver particles occupy spaces between the coarse particles and form sintering necks that tie the packed particles together.

1.2Finer silver particle fraction

What ifWhat if the fine silver fraction has a D90 of 150 nm?
Claim language“from 300 to 1,000 nm”

Disperse the fine powder in the liquid vehicle and blend it with the silver flakes. During heating, the fine particles form necks with one another and with the flakes, producing a continuous silver network.

1.3Water based vehicle

What ifWhat if deionized water serves as the sole solvent?
Claim language“at least one organic solvent”

An ammonium polyacrylate dispersant stabilizes the silver particles in the water. A staged drying cycle removes water from the deposited paste before the assembly reaches the silver sintering temperature.

1.3Low solvent stencil paste

What ifWhat if the paste uses 8 wt. % organic solvent?
Claim language“10 to 25 wt. %”

A formulation with 22 wt. % silver flakes and 70 wt. % fine silver powder uses 8 wt. % glycol ether as its liquid vehicle. The two powder fractions pack together, and a squeegee forces the resulting high-solids paste through stencil openings.

1.4Acrylic rheology binder

What ifWhat if an acrylic binder controls the paste rheology?
Claim language“at least one cellulose derivative”

Dissolve 0.5 wt. % poly(methyl methacrylate) in a compatible ester solvent before mixing in the silver powders. The polymer raises vehicle viscosity, and an air firing cycle removes it before the silver joint densifies.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Silver joints for vacuum feedthroughs

A silver sintering paste containing silver flakes, submicrometer silver particles and an organic solvent bonds terminal lugs to silver-plated pins on the air side of a ceramic vacuum feedthrough. A stencil deposits paste on each lug, and a fixture holds the lug against the flattened end of its pin. A vented heating stage removes solvent before a heated press consolidates the silver into an electrically conductive joint. The ceramic-to-metal seal maintains the vacuum boundary.

Component substitution

Polyvinyl butyral as the paste binder

The paste contains 15 wt. % silver flakes with a D90 of 10 μm, 68 wt. % silver particles with a D90 of 600 nm, 16.5 wt. % diethylene glycol monobutyl ether and 0.5 wt. % polyvinyl butyral in place of the cellulose derivative. Mixing first dissolves the polyvinyl butyral in the solvent and then disperses both silver fractions in that solution. After printing onto a silver-plated bonding surface, a vented heating cycle removes the solvent and decomposes the binder before pressure-assisted sintering forms the joint.

Parameter or scale variation

Silver paste with larger flakes

The paste contains 22 wt. % silver flakes with a D90 of 30 μm, 60 wt. % silver particles with a D90 of 700 nm and 18 wt. % diethylene glycol monobutyl ether. A 125 μm stencil with a 2 mm square aperture deposits the paste on a silver-plated copper pad. An open-face drying step removes solvent before a second silver-plated part is placed on the deposit and a heated press consolidates the joint.

Segmented deposits for large copper joints

A stencil with a four-by-four array of 3 mm square apertures deposits silver paste on a 15 mm square silver-plated copper pad. The stencil leaves 0.5 mm gaps between neighboring deposits, and the paste contains silver flakes with a D90 of 12 μm and finer silver particles with a D90 of 600 nm. The exposed deposits dry before a matching silver-plated copper plate is placed over the array. A heated press consolidates the deposits into multiple bonded areas between the two copper parts.

Combination with existing systems

Silver die attach on liquid coolers

A silver sintering paste containing silver flakes, submicrometer silver particles and an organic solvent attaches a silver-backed power semiconductor die to the silver-plated top wall of a copper microchannel cooler. The paste is stencil printed on the cooler wall and dried before die placement. During pressure-assisted sintering, a support fixture aligns the applied load with the ribs that separate the coolant channels. In service, the sintered silver joint conducts heat from the die into the channel wall, and circulating coolant carries heat away.

Automated or data-driven variant

Deposit volume control with laser profiling

A positive-displacement dispenser deposits paste containing silver flakes, submicrometer silver particles and an organic solvent on silver-plated die pads. A laser triangulation sensor scans each wet deposit, and software integrates its height above the adjacent pad surface to calculate volume. The controller adjusts the dispenser stroke for subsequent pads using the measured volume error and routes out-of-tolerance deposits for rework. Accepted deposits proceed to drying, die placement and pressure-assisted sintering.

Specific version of a part

Milled silver flakes

Use 20 wt. % mechanically flattened silver flakes with a D90 of 12 μm. The platelets orient under stencil printing shear and create overlapping contacts in the deposited layer.

Precipitated silver powder

Use 65 wt. % near-spherical silver particles produced by liquid-phase reduction and classified to a D90 of 700 nm. The particles occupy spaces between the flakes and form sintering necks during heating.

Glycol ether solvent blend

Use 10 wt. % diethylene glycol monobutyl ether and 5 wt. % propylene glycol methyl ether acetate. The more volatile acetate contributes to initial drying, while the glycol ether maintains wetting during deposition.

Ethyl cellulose thickener

Dissolve 0.5 wt. % ethyl cellulose in the organic vehicle before incorporating the silver powders. The dissolved polymer raises viscosity and helps the stencil deposit retain its shape before drying.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2009/0242854 A1
Published
Oct 1, 2009
Filed
Feb 24, 2009
Class
H01B 1/22
Document BUS 2015/0104625 A1
Published
Apr 16, 2015
Filed
Apr 25, 2013
Class
C09D 5/24
Claim 1
Document A
Document B
1.1(A) 5 to 40 wt. % of silver flakes with a particle size D90 in the range from 5 to 20 μm,
The electroconductive composition comprises (A) a crystalline flake silver powder and (B) an organic binder, wherein the blending ratio of the (A) crystalline flake silver powder is 90% by mass to 98% by mass with respect the total solid content of the composition. In a preferred embodiment, the (A) crystalline flake silver powder contains polygonal single particles and has an average particle size (D50), which is determined by a laser diffraction-scattering particle size distribution analysis, of 1 μm to 3 μm.
B · US 2015/0104625 A1 · abstract
1.2(B) 50 to 85 wt. % of silver particles with a particle size D90 in the range from 300 to 1,000 nm,
The nanoparticles may be, for example, copper, silver, nickel, iron, cobalt, aluminum, palladium, gold, tin, zinc, cadmium, etc., or any combination thereof. The nanoparticles may be about 0.1 μm (100 nm) in diameter or smaller.
A · US 2009/0242854 A1 · ¶ 18
1.3(C) 10 to 25 wt. % of at least one organic solvent,
In some implementations, the solvent includes water, an organic solvent, or any combination thereof.
A · US 2009/0242854 A1 · ¶ 5
In the electroconductive composition of the present invention, as required, a solvent may also be used for dispersing the above-described silver powder. As the solvent, an organic solvent can be used.
B · US 2015/0104625 A1 · ¶ 34
1.4(D) 0 to 2 wt. % of at least one cellulose derivative, and
Examples of the dry-type organic binder include polyester resins, acrylic resins, butyral resins, vinyl chloride-vinyl acetate copolymer resins, polyamide imide, polyamide, polyvinyl chloride, nitrocellulose, cellulose-acetate-butyrate (CAB) and cellulose-acetate-propionate (CAP), which are soluble to a solvent and capable of forming a film when dried, and these dry-type organic binders can be cured at a low temperature depending on the solvent selection.
B · US 2015/0104625 A1 · ¶ 30
1.5(E) 0 to 10 wt. % of at least one additive different from constituents (A) to (D).
In certain implementations, the conductive ink includes a stabilizing agent, an adhesion promoter, a surface tension modifier, a defoaming agent, a leveling additive, a rheology modifier, a wetting agent, an ionic strength modifier, or any combination thereof.
A · US 2009/0242854 A1 · ¶ 5
In the electroconductive composition of the present invention, as required, a variety of additives, such as an antioxidant, a stabilizer, a dispersant, an antifoaming agent, an antiblocking agent, a fine molten silica, a silane coupling agent, a thixotropic agent, a colorant and an electroconductive powder other than the above-described silver powder (e.g., carbon powder) may also be incorporated.
B · US 2015/0104625 A1 · ¶ 36

An empty cell means only that no passage was reproduced there.

Statements in these documents
These metallic ink dispersions may be used for printing conductors, thereby making the direct writing of electronic circuits possible.
A · US 2009/0242854 A1 · ¶ 3
Any residues from these dispersants remaining in the cured metallic films will result in higher resistivities being obtained in the metal conductor that is formed because these dispersants and their decomposition products are non-conducting organic compounds, or insulators.
A · US 2009/0242854 A1 · ¶ 4
More particularly, the present invention relates to an electroconductive composition that is useful for forming, for example, a conductor pattern circuit of a printed wiring board, especially a flexible printed wiring board, and a conductor pattern circuit on a front substrate or back substrate of a plasma display panel.
B · US 2015/0104625 A1 · ¶ 1
In recent years, as resin substrates and thermally weak parts are more often used due to product down-sizing, there is a demand for a low-resistance electroconductive material that is cured at a low temperature.
B · US 2015/0104625 A1 · ¶ 2
Cite aspatent.fyi, US 2026/0355815 A1, claim 1, first published 2026-11-19T15:46:13-05:00, https://patent.fyi/US20260355815/, SHA-256 b0eecdcc2d2f0d0b57d92920a04f36bd6e7f0b5afe1e9cf61f2f616eeb65c147
First published
Permanent addresshttps://patent.fyi/US20260355815/
Content fingerprint (SHA-256)b0eecdcc2d2f0d0b57d92920a04f36bd6e7f0b5afe1e9cf61f2f616eeb65c147