patent.fyi
Applications  /  US 2026/0355816
United States Patent Application Publication

US 2026/0355816 A1

Published
Nov 12, 2026
Filed
Mar 7, 2024
Earliest date on the face
May 31, 2023
Classification
B22F 1/10
First published here
Nov 19, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.2Nickel–zinc ferrite flakes

What ifWhat if the flaky magnetic powder consists of nickel–zinc ferrite?
Claim language“one alloy powder or a mixture of two or more alloy powders”

Milled ferrite platelets disperse in the polymer binder and align approximately parallel to the sheet during calendering. The platelets provide magnetic loss for near-field suppression, and their high electrical resistivity limits eddy currents.

1.3Fine magnetic flake grade

What ifWhat if the flaky magnetic powder has a median diameter of 6 μm?
Claim language“a median diameter of 10 μm to 30 μm”

Air classification selects an iron–silicon flake grade with a median diameter of 6 μm. Calendering aligns the flakes in a thin sheet, where the magnetic phase provides an in-plane path for flux and dissipates energy through magnetic loss.

1.4Lower powder loading

What ifWhat if the composite contains 85 mass % flaky magnetic powder and the member uses a thicker sheet?
Claim language“88.9 mass % to 90 mass %”

Two plies that each contain 85 mass % iron–silicon flakes form a thicker layer with aligned flakes in both plies. The added thickness increases the amount of magnetic material per unit area relative to a single ply of the same formulation.

1.5Thermoplastic polyurethane binder

What ifWhat if thermoplastic polyurethane forms the binder phase?
Claim language“hydrogenated nitrile rubber and polyolefin”

A film-forming thermoplastic polyurethane solution wets the iron–silicon flakes in a casting slurry. Solvent evaporation forms a flexible polymer matrix that holds the flakes in place, and calendering compacts the sheet and aligns the flakes.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Magnetic lining for industrial encoder housings

A die-cut composite liner contains 89 mass % flaky iron–silicon–chromium powder with a median diameter of 20 μm, 6 mass % hydrogenated nitrile rubber, and 5 mass % polyethylene. A pressure-sensitive adhesive bonds the liner to the inside of an industrial optical encoder housing above the digital output circuit. The liner intercepts stray magnetic fields from switching currents while leaving the optical path and shaft clearance open.

Component substitution

Flakes made from iron–silicon–aluminum alloy

Flaky iron–silicon–aluminum alloy powder with a median diameter of 20 μm supplies 89 mass % of the composite. A heated mixer blends the powder with 6 mass % hydrogenated nitrile rubber and 5 mass % polyethylene. Warm calender rolls consolidate the blend into a strip and orient the broad flake faces along its surface, where magnetic losses dissipate energy from alternating fields.

Parameter or scale variation

Thin laminate with finer magnetic flakes

A composite contains 89 mass % flaky iron–silicon powder with a median diameter of 7 to 9 μm, 6 mass % hydrogenated nitrile rubber, and 5 mass % polyethylene. Warm calender rolls form the composite on a 25 μm polyimide carrier with a magnetic layer 0.12 to 0.18 mm thick. The carrier supports the layer during die cutting and installation, and the finished laminate places the magnetic material close to conductors in assemblies with limited clearance.

Combination with existing systems

Magnetic liner inside a converter shield

A patch contains 89 mass % flaky iron–chromium powder with a median diameter of 20 μm, 6 mass % hydrogenated nitrile rubber, and 5 mass % polyethylene. An insulating adhesive bonds the patch to the inside of a grounded metal shield lid above the switching loop of a step-down power converter. The patch dissipates energy from the local alternating magnetic field, and the grounded enclosure attenuates electric-field coupling to adjacent circuits.

Automated or data-driven variant

Closed-loop control of composite mass loading

Three loss-in-weight feeders supply flaky iron–silicon powder, hydrogenated nitrile rubber granules, and polyethylene pellets to a heated twin-screw compounder at targets of 89, 6, and 5 mass %, respectively. A controller computes each ingredient's mass fraction from the feeder weight changes over a rolling interval and adjusts the feeder speeds to maintain the target ratios. Heated rolls consolidate the compound, and an inline thickness gauge provides feedback to the roll-gap actuator.

Field mapping for magnetic patch placement

A motorized positioning stage moves a shielded loop probe over a powered circuit board on a 1 mm grid at the intended patch height. Software records the field spectrum at each point and groups adjacent points where the amplitude exceeds a set threshold in the frequency band of interest. A plotter cuts adhesive-backed patches from a sheet containing 89 mass % flaky iron–silicon–chromium powder, 6 mass % hydrogenated nitrile rubber, and 5 mass % polyethylene. The patches mount on an insulating cover at the mapped coordinates, and a second scan at the same probe height measures the change in field amplitude.

Specific version of a part

Laminated magnetic foil stack

Thin iron–silicon foils carry magnetic flux along the plane of the member. An oxide coating electrically isolates adjacent foils and limits eddy current loops through the stack.

Higher polyethylene binder fraction

The remaining 89 mass % consists of iron–silicon flakes. A heated mixer softens the polyethylene and disperses the rubber and flakes, and hot calendering consolidates the mixture into a sheet.

Single iron–silicon alloy powder

Gas atomization produces an iron–silicon powder with 3 mass % silicon in the alloy. Attritor milling flattens the particles into flakes, and classification controls the particle size distribution.

Twenty micrometer median diameter

Air classification removes the coarse and fine tails of a milled flake powder. Laser diffraction measures a volume median diameter of 20 μm on a dispersed powder sample.

Six percent rubber loading

Each 100 g of composite contains 6 g of hydrogenated nitrile rubber, 5 g of polyethylene, and 89 g of flaky iron–silicon powder. The rubber deforms during bending and helps the sheet conform to curved surfaces.

Three percent polyethylene loading

Each 100 g of composite contains 3 g of low-density polyethylene, 7 g of hydrogenated nitrile rubber, and 90 g of flaky iron–silicon powder. The polyethylene softens during hot calendering and solidifies as the sheet cools.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2016/0114390 A1
Published
Apr 28, 2016
Filed
May 27, 2014
Class
B22F 1/0055
Document BUS 2017/0001242 A1
Published
Jan 5, 2017
Filed
Mar 24, 2015
Class
B22F 1/0055
Claim 1
Document A
Document B
1.1a composite composition containing flaky magnetic powder and a binder,
Provided are a flaky-like silver powder having a low bulk density as well as a predetermined average particle size (D50) and the like, which is obtainable by using a predetermined wet reduction method, a conductive paste obtainable using such a flaky-like silver powder, and a method for producing such a flaky-like silver powder.
A · US 2016/0114390 A1 · abstract
Hereinafter described will be embodiments of a flaky metal pigment of the present invention, a metallic composition containing the same and a coated product, and a method of manufacturing the flaky metal pigment.
B · US 2017/0001242 A1 · ¶ 28
1.2wherein the flaky magnetic powder is one alloy powder or a mixture of two or more alloy powders selected from among an Fe—Si—Cr alloy, an Fe—Si alloy, and an Fe—Cr alloy,
1.3the flaky magnetic powder has a median diameter of 10 μm to 30 μm,
Disclosed are a flaky-like silver powder obtainable by a wet reduction method, a conductive paste obtainable using a flaky-like silver powder, and a method for producing a flaky-like silver powder, in which the average particle size (D50) as an equivalent circle diameter obtainable when the flaky-like silver powder particles are viewed planarly is adjusted to a value within the range of 1.1 to 30 μm, the thickness of the flaky-like silver powder particles is adjusted to 0.01
A · US 2016/0114390 A1 · abstract
According to the flaky metal pigment of the present invention, in the case where the flaky metal pigment is measured by a flow-type particle image analyzer, P50 showing a 50% cumulative frequency of a diameter equivalent to an area circle in a number distribution is less than 0.500 μm.
B · US 2017/0001242 A1 · abstract
1.4a content ratio of the flaky magnetic powder is from 88.9 mass % to 90 mass % in terms of a mass ratio with respect to 100 mass % of the composite composition,
1.5the binder contains hydrogenated nitrile rubber and polyolefin,
On the occasion of configuring the conductive paste of the invention, it is preferable that the electrically insulating resin includes at least one thermoplastic resin selected from the group consisting of a polyester resin, a polyolefin resin, a polyamide resin, and a polyurethane resin.
A · US 2016/0114390 A1 · ¶ 33
As the above-described resin, a combination of two or more of the following elements is suitably used, which include an epoxy resin, a polyester resin, an acrylic resin, an acrylic silicone resin, a vinyl resin, a silicon resin, a polyamide resin, a polyamideimide resin, a fluorine resin, boiled oil, chlorinated rubber, an amino resin, a phenol resin, a polyisocyanate resin, a urea resin, and the like.
B · US 2017/0001242 A1 · ¶ 58
1.6a content ratio of the hydrogenated nitrile rubber is from 2 mass % to 9 mass % in terms of the mass ratio with respect to 100 mass % of the composite composition, and
1.7a content ratio of the polyolefin is from 1 mass % to 8 mass % in terms of the mass ratio with respect to 100 mass % of the composite composition.

An empty cell means only that no passage was reproduced there.

Statements in these documents
More particularly, the invention relates to a flaky-like silver powder which has a predetermined average particle size and the like and also has a small bulk density, a conductive paste using such a flaky-like silver powder, and an efficient method for producing such a flaky-like silver powder.
A · US 2016/0114390 A1 · ¶ 2
However, a flaky metal pigment is not small enough for the diameter of the hole of the ink-jet nozzle used in an industrially-applied or non-commercially-applied general ink jetting process, which causes blockage in the ink-jet nozzle, with the result that ink cannot be discharged.
B · US 2017/0001242 A1 · ¶ 6
In order to solve the above-described problems, an attempt has been made to produce flaky metal pigments reduced in particle diameter, thereby allowing metallic printing implemented by ink jetting.
B · US 2017/0001242 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0355816 A1, claim 1, first published 2026-11-19T15:46:13-05:00, https://patent.fyi/US20260355816/, SHA-256 e93f05f0a622b5c95dabee47566bf0f164e40d9bb5d006caed665208729ed6db
First published
Permanent addresshttps://patent.fyi/US20260355816/
Content fingerprint (SHA-256)e93f05f0a622b5c95dabee47566bf0f164e40d9bb5d006caed665208729ed6db
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi