patent.fyi
Applications  /  US 2026/0355817
United States Patent Application Publication

US 2026/0355817 A1

Published
Nov 12, 2026
Filed
Aug 29, 2024
Earliest date on the face
Aug 29, 2023
Classification
B22F 1/12
First published here
Nov 19, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Bonding with continuous copper foil

What ifWhat if a continuous copper foil forms the die attach joint by solid-state diffusion?
Claim language“metal (nano) particles”

A thin annealed copper foil sits between a copper-metallized die and a copper pad. Surface cleaning removes copper oxide, and heat and pressure deform the foil at asperities and promote diffusion across both interfaces.

1.2Alumina platelets in silver paste

What ifWhat if alumina platelets provide the rigid filler in a silver sinter paste?
Claim language“carbonaceous platelets”

A low volume fraction of alumina platelets limits shrinkage as the silver particles densify. The silver particles form a continuous metal network around the platelets and bond to the metallized die and substrate.

1.2Dry platelet placement between layers

What ifWhat if dry platelets are placed between two dried silver particle layers before assembly?
Claim language“in a common carrier”

A stencil meters graphite platelets onto the dried silver layer on the substrate, and a second dried silver layer on the die covers them. Heat and pressure consolidate the silver layers through gaps in the platelet deposit and trap the platelets in the resulting bond line.

1.2Mechanical retention around platelet edges

What ifWhat if untreated graphite platelets are retained by a continuous silver matrix?
Claim language“modified with an adhesion promoter”

A low loading of separated graphite platelets leaves space for silver particles to pack between them. During pressure-assisted sintering, silver necks join the material above and below each platelet around its perimeter, mechanically trapping it in the joint.

1.2Metal contact through silver shells

What ifWhat if a continuous silver shell on each graphite platelet provides the contact surface for silver particles?
Claim language“comprises a pendant group”

Electroless deposition forms a silver shell over the platelet faces and edges. The shell sinters directly to adjacent silver particles, forming metal necks that connect each coated platelet to the surrounding matrix.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Sintered joints for thermoelectric modules

The paste joins thermoelectric legs with silver-finished ends to silver-finished copper interconnects on ceramic plates. Silver nanoparticles and carbonaceous platelets share a carrier, and each platelet carries an anchored promoter with a pendant group that binds to silver and remains stable during reducing sintering. A fixture aligns the legs between the plates and applies compression while the carrier leaves and the silver particles sinter into electrically and thermally conductive joints.

Component substitution

Exfoliated graphite flakes as platelets

Exfoliated graphite microflakes replace few-layer graphene platelets in a silver nanoparticle paste. The graphite flakes carry an anchored adhesion promoter with a pendant group that binds to silver and remains stable during reducing sintering. The treated flakes and silver nanoparticles disperse in a common carrier, and the silver particles sinter around the flakes after the carrier leaves the bond line.

Water based carrier for silver paste

A mixture of deionized water and glycerol replaces the organic solvent carrier in a silver nanoparticle paste, and a low concentration of water-soluble dispersant supports suspension stability. The aqueous carrier holds both the silver nanoparticles and carbonaceous platelets bearing an anchored promoter with a silver-binding pendant group that remains stable during reducing sintering. A stencil deposits the paste onto the substrate, and a warm drying stage removes most of the water before die placement. A vented heating stage removes the remaining carrier before pressure-assisted reducing sintering.

Parameter or scale variation

Submicrometer platelets in thin bond lines

The paste contains silver nanoparticles and carbonaceous platelets with lateral dimensions of 0.3 to 0.8 μm and thicknesses of 10 to 20 nm. The platelets account for 0.3 wt % of the combined particle and platelet mass and carry an anchored promoter with a silver-binding pendant group that remains stable during reducing sintering. A stencil deposits a 30 μm wet layer onto a silver-finished substrate, and a displacement-controlled press holds the die at a 15 μm gap during reducing sintering.

Combination with existing systems

Die attach on copper bonded ceramic

A ceramic power-module substrate carries patterned copper on its top face and a copper heat-spreading layer on its back face. A stencil deposits a common-carrier paste containing silver nanoparticles and promoter-treated carbonaceous platelets onto silver-finished copper pads, and a placement head sets the semiconductor dies onto the deposits. A heated press sinters the paste under reducing conditions while the anchored promoter's silver-binding pendant group remains stable. Bond wires connect the die tops to adjacent copper pads after sintering.

Automated or data-driven variant

Closed loop paste volume control

A positive-displacement dispenser deposits a common-carrier paste containing silver nanoparticles and carbonaceous platelets with an anchored, reduction-stable silver-binding promoter. A laser profilometer scans each deposit before die placement, and software integrates the measured height above the substrate to calculate deposit volume. The controller adds paste to underfilled pads, flags overfilled pads for rework, and adjusts subsequent dispense strokes from measured volume errors. The placement head sets dies onto accepted deposits for reducing sintering.

Specific version of a part

Bimodal silver particle blend

The metal fraction contains silver particles with nominal diameters of 80 nanometers and 1 micrometer. The finer particles occupy interstices between larger particles and form sintering necks at particle contacts.

Submicrometer copper powder in paste

The paste contains copper particles with a median diameter of approximately 300 nanometers. A hydrogen-containing atmosphere reduces surface copper oxide during heating, exposing copper surfaces for neck growth.

Graphite and silver in terpineol

Graphite platelets with a lateral size of 2 to 5 micrometers are dispersed with silver particles in a terpineol-based carrier. A stencil deposits the suspension on a metallized substrate, and a drying step removes the carrier before sintering.

Aromatic anchor with pyridyl groups

An aromatic anchor adsorbs onto graphite basal planes through interactions between aromatic rings and the graphitic surface. Exposed pyridyl groups coordinate silver particle surfaces, and a reducing sintering cycle with a peak near 180 °C limits thermal decomposition of the aromatic tether.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2006/0196310 A1
Published
Sep 7, 2006
Filed
May 6, 2004
Class
B22F 9/24
Document BUS 11,158,867 B2
Published
Oct 26, 2021
Filed
Dec 12, 2014
Class
H01M 4/928
Claim 1
Document A
Document B
1.1metal (nano) particles (2), and
Specifically, the present invention provides a ternary metal colloid comprising metal nanoparticles which is composed of three different metal elements and has a three layer core/shell structure.
A · US 2006/0196310 A1 · ¶ 10
The platinum or platinum alloy catalyst can be in the form of unsupported nanoparticles (such as metal blacks or other unsupported particulate metal powders) or can be deposited as even higher surface area particles onto a conductive carbon substrate or other conductive material (a supported catalyst).
B · US 11,158,867 B2 · ¶ 5
1.2carbonaceous platelets (3), dispersed with the metal (nano) particles (2) in a common carrier (4), wherein the carbonaceous platelets (3) are modified with an adhesion promoter (6), wherein said adhesion promotor (6) is anchored (A) to said platelets (3) and comprises a pendant group (X) having an affinity to binding to a surface of the metal (nano) particles (2) and wherein the pendant group (X) of said adhesion promotor (6) remains stable under reducing conditions during sintering of said metal (nano) particles (2).
Synthetic graphite powder (Alfa Aesar, 46304), with an as-received average particle size of 7-11 micron, was dispersed in neat propan-1-ol. The graphite dispersion was mixed using a high shear mixer and added to the Pt black/ionomer dispersion to give a weight ratio Pt to graphite of 1:0.36.
B · US 11,158,867 B2 · ¶ 89

An empty cell means only that no passage was reproduced there.

Statements in these documents
However, the conventional study examples mainly relate to a binary metal colloid for adsorbing two metal nanoparticles (the conventional arts relating to the binary metal colloid are disclosed in, for example, the following Patent Documents).
A · US 2006/0196310 A1 · ¶ 5
Therefore, the present invention provides a ternary metal colloid and a process for producing the same, in which three metal atoms can be arranged in design in a good arrangement state.
A · US 2006/0196310 A1 · ¶ 8
The invention also relates to electrodes, catalyst-coated membranes and membrane electrode assemblies comprising the catalyst layer.
B · US 11,158,867 B2 · ¶ 1
High electrochemical potentials can occur in a number of real-life operational situations and in certain circumstances can cause damage to the catalyst layer/electrode structure, primarily due to corrosion of any carbon present in the layer, such as the support material for the catalyst.
B · US 11,158,867 B2 · ¶ 11
Cite aspatent.fyi, US 2026/0355817 A1, claim 1, first published 2026-11-19T15:46:13-05:00, https://patent.fyi/US20260355817/, SHA-256 0d233c902dc7bb0c9a6892438b576485e997d05e4aec7ced4ef78ddc3a2452b7
First published
Permanent addresshttps://patent.fyi/US20260355817/
Content fingerprint (SHA-256)0d233c902dc7bb0c9a6892438b576485e997d05e4aec7ced4ef78ddc3a2452b7
Methodv2026-11-18.2 · automated, not reviewed by a person