patent.fyi
Applications  /  US 2026/0355843
United States Patent Application Publication

US 2026/0355843 A1

Published
Nov 12, 2026
Filed
May 6, 2025
Earliest date on the face
May 6, 2025
Classification
B23K 9/093
First published here
Nov 19, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Alternating electrode polarity

What ifWhat if the welding current alternates between electrode-positive and electrode-negative intervals?
Claim language“a direct current (DC) waveform”

An inverter reverses electrode polarity within each cycle. An electrode-positive current pulse detaches a molten droplet, and the duration of the electrode-negative interval sets the fraction of the cycle spent at that polarity.

1.1Tungsten electrode with separate filler

What ifWhat if a nonconsumable tungsten electrode sustains the arc while a separate wire supplies filler metal?
Claim language“a consumable electrode that advances toward a workpiece”

A power source supplies current between the tungsten electrode and the workpiece. A motorized feeder advances an electrically isolated filler wire into the leading edge of the weld pool, where heat from the arc and pool melts it.

1.2Optical feedback from pool width

What ifWhat if feedback comes from optically measured weld pool width?
Claim language“integrating the weld power”

A filtered camera captures the pool during the background-current interval. The controller measures the pool width from the image and changes the next peak-current duration when the measured width differs from the setpoint.

1.2Waveform schedule by joint gap

What ifWhat if a measured joint gap selects a preset pulse schedule?
Claim language“comparing the total energy to a target energy”

A laser profile sensor ahead of the torch measures the gap between the joint edges. The controller uses the measured gap and torch position to look up the peak and background durations for that location.

1.2Heat input through travel speed

What ifWhat if the controller changes torch travel speed to regulate electrical energy per unit seam length while the pulse settings stay fixed?
Claim language“adjusting the DC waveform”

The controller divides average electrical power by the target energy per unit length to calculate a travel-speed setpoint. An encoder provides actual speed to the carriage drive, which changes motor speed to track the setpoint.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Arc deposition for die repair

A wire-fed torch deposits metal in layers to rebuild worn regions of a forming die. A direct-current power source strikes an arc and transfers one droplet per cycle while a motion stage follows the repair path. The controller integrates electrical power from each arc strike to the end of its cycle and compares the result with a target assigned to that path segment. It adjusts the background current of the next cycle within the range that sustains the arc.

Component substitution

Power integration with analog circuitry

An analog multiplier and a resettable capacitor integrator replace numerical integration of sampled weld power. Isolated voltage and current transducers feed the multiplier, and an arc-strike signal resets the integrator at the start of each cycle after the preceding value is captured. A sample-and-hold circuit captures the capacitor voltage at the cycle boundary, and a differential amplifier compares it with a reference voltage scaled to the target energy. The resulting error trims the next cycle's background current command.

Parameter or scale variation

Fixed rate with bounded correction

A direct-current source runs 100 droplet-transfer cycles per second, with each 10 millisecond cycle beginning at a commanded arc strike. Synchronized voltage and current channels sample at 50 kilohertz, and the controller accumulates 500 power samples per cycle to estimate energy. The controller compares each result with a 20 joule target and commands a higher or lower background current for the next cycle according to the sign of the error. It limits each correction to 2 amperes and clamps the background current to the operating range established for the wire and shielding gas.

Combination with existing systems

Energy control with seam tracking

A laser line profiler mounted ahead of a robotic welding torch measures joint gap and seam centerline. The robot controller associates each profile with a position along the weld path and applies the corresponding torch offset when the electrode reaches that position. At each arc strike, the welding controller selects a cycle energy target from a table indexed by the measured gap at the electrode position. It integrates weld power through droplet transfer and the remainder of the cycle, then uses the energy error to adjust the next cycle's background current.

Automated or data-driven variant

Temperature-based cycle energy selection

An infrared pyrometer measures the workpiece surface ahead of the torch, and a travel encoder associates each reading with a position on the joint. The controller retrieves the stored temperature when the electrode reaches that position and interpolates an energy target from a table calibrated on test welds. The direct-current source strikes an arc and transfers one droplet per cycle, and the controller integrates electrical power over that cycle. The difference between measured and target energy sets the direction and magnitude of the next cycle's background current correction.

Optical feedback for transfer timing

A high-speed camera views the wire tip through an optical bandpass filter, and a pulsed backlight produces a silhouette of the droplet. Image processing detects separation from the wire when a gap first appears in the silhouette and timestamps that event against the waveform clock. The controller uses the observed transfer timing to define the interval after detachment in which it adjusts the current of later cycles. It compares integrated cycle energy with the target and applies the resulting correction to the background current in that interval.

Specific version of a part

Electrode-positive pulses with solid wire

Drive rolls feed a 1.2 mm solid steel wire through a copper contact tip connected to the positive output of a DC power source. The source applies a peak-current pulse to transfer a droplet and then returns to a lower background current.

Current ramp for short-circuit transfer

A voltage sensor detects the drop in voltage when the advancing wire touches the weld pool. The source ramps up DC current to pinch the liquid metal bridge, then lowers the current as the bridge opens and the arc restrikes.

Sampled voltage and current integration

A controller samples weld voltage and current together every 10 microseconds and multiplies each pair to calculate instantaneous power. It sums power multiplied by the sampling interval from one cycle boundary to the next and compares the resulting energy with a setpoint in joules.

Peak duration correction across cycles

At the end of each cycle, the controller subtracts the integrated energy from the target energy. A proportional correction lengthens the next peak when the measured energy is low and shortens it when the measured energy is high, within configured duration limits.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2007/0210048 A1
Published
Sep 13, 2007
Filed
Feb 2, 2007
Class
B23K 9/09
Document BUS 8,937,267 B2
Published
Jan 20, 2015
Filed
Jul 20, 2012
Class
B23K 9/092
Claim 1
Document A
Document B
1.1supplying weld power to a consumable electrode that advances toward a workpiece, wherein the weld power includes a direct current (DC) waveform having cycles that each strikes an arc, and transfers a molten metal droplet, from the consumable electrode to the workpiece; and
In the present invention, two different pulse waveforms of a different pulse peak current level and a different pulse width per pulse are alternately continuously oscillated, to transfer one droplet per pulse.
A · US 2007/0210048 A1 · ¶ 19
In step 540, decrease the output current level below the background current level 111 as the molten metal ball 192 pinches off from the distal end of the electrode (e.g., 191 or 450) onto the workpiece (e.g., 199 or 460), re-establishing an electric arc 196 between the electrode (e.g., 191 or 450) and the workpiece (e.g., 199 or 460). In step 550, increase the output current level to a peak current level 131 of the waveform 100 in response to re-establishing an electric arc 196.
B · US 8,937,267 B2 · ¶ 71
1.2controlling an energy supplied to the consumable electrode across the cycles by, for each cycle: integrating the weld power to produce a total energy supplied to the consumable electrode; comparing the total energy to a target energy to produce a compare result; and when the compare result indicates that the total energy is not equal to the target energy, adjusting the DC waveform to drive the total energy to the target energy for an ongoing cycle or a subsequent cycle of the DC waveform.
Moreover, in regard to the respective wire feed rates, if the distance between a chip and a base metal varies, welding voltages are controlled every moment to keep the arc length at a given level while feedbacking a change in the welding voltage or a change in the welding current, and a welding current waveform necessary to maintain the voltage is referred to the database, to thereby make an optimum selection within the permissible range of each parameter and further to reali
A · US 2007/0210048 A1 · ¶ 40

An empty cell means only that no passage was reproduced there.

Statements in these documents
The present invention relates to a pulsed arc welding method using, as a shield gas, carbon dioxide gas alone or a mixed gas containing a carbon dioxide gas as a main component, more particularly, to a pulsed arc welding method in which droplet transfer is realized in synchronism with a group of pulses to thereby stabilize a welding arc and, at the same time, to significantly reduce spatter and fume generation rates.
A · US 2007/0210048 A1 · ¶ 2
This undesirably leads to the problems in that short-circuiting with a base metal and arc break are liable to occur, droplet transfer becomes irregular, and spatters and fumes are excessively generated.
A · US 2007/0210048 A1 · ¶ 6
The STT process produces a low hydrogen weld metal deposit in open root joints with easier operation, better back beads, better sidewall fusion, and less spatter and fumes than other processes.
B · US 8,937,267 B2 · ¶ 9
Even though the current STT process is significantly better than the traditional short-arc GMAW process, especially for root welding application, the ability to better control heat input into the weld to achieve even better penetration without increasing the weld puddle fluidity is desired.
B · US 8,937,267 B2 · ¶ 10
Cite aspatent.fyi, US 2026/0355843 A1, claim 1, first published 2026-11-19T15:46:13-05:00, https://patent.fyi/US20260355843/, SHA-256 5c04435218c7f2b67a4311371517696b32034162c40c1ad1334290d582b62b5e
First published
Permanent addresshttps://patent.fyi/US20260355843/
Content fingerprint (SHA-256)5c04435218c7f2b67a4311371517696b32034162c40c1ad1334290d582b62b5e
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi