patent.fyi
Applications  /  US 2026/0355847
United States Patent Application Publication

US 2026/0355847 A1

Published
Nov 12, 2026
Filed
Apr 1, 2026
Earliest date on the face
May 9, 2025
Classification
B23K 20/023
First published here
Nov 19, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Pure metal starting blanks

What ifWhat if the blanks consist of pure copper and pure silver?
Claim language“made in metal alloys”

Copper supplies a reddish region and silver supplies a pale region. A diffusion hold below the copper–silver eutectic temperature produces composition changes near the bonded interfaces, and a shallow bevel spreads the exposed transitions across the visible face.

1.2Side by side strip assembly

What ifWhat if the blanks meet edge to edge across the width of the article?
Claim language“Stacking said blanks”

Strips of copper-rich and nickel-rich copper alloys sit side by side in order of increasing nickel content, with their broad faces coplanar. A heated die applies pressure across the strip edges to bond them, and a finishing cut exposes the ordered colour bands across the width.

1.3Capillary bonding without compression

What ifWhat if capillary brazing forms the cohesive stack without applied compression?
Claim language“Applying stress at room temperature or at a hot temperature”

Integral stand-offs set the gaps between the blanks, and a fixture supports the assembly without clamping the layers together. Molten filler wets the facing surfaces and flows into the gaps by capillary action, then solidifies into joints that hold the stack together during subsequent handling.

1.4Graded colour by area fraction

What ifWhat if the visible gradient comes from changing exposed proportions of two colours without a diffusion heat treatment?
Claim language“Diffusion thermal treatment between the blanks”

Cold roll bonding joins alternating foils of two differently coloured copper alloys, with the thickness ratio shifting progressively through the stack. An oblique cut exposes fine bands that blend visually at the intended viewing distance, and the changing band-width ratio shifts the apparent colour along the face.

1.5Inclined surface cut by milling

What ifWhat if a milling cutter removes material to form the inclined surface?
Claim language“Shaping by deformation”

An angled fixture holds the bonded stack beneath a carbide end mill, which cuts a ramp across successive layer interfaces. The fixture angle controls the exposed width of each layer, and the programmed cut depth determines how many layers the ramp intersects.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Colour gradient on architectural handles

An architectural pull handle carries a flat grip insert made from stacked copper, brass and bronze blanks. A hot press consolidates the stack and holds it at temperature for interdiffusion between adjacent blanks. A wedge die deforms the consolidated stack so the interfaces slope along the length of the insert. The insert is ground and polished from its original outer face through more than one blank thickness, and two rear clamps secure it to the handle with the gradient facing outward.

Component substitution

Fixed abrasive belt for face polishing

A water-cooled fixed abrasive belt replaces loose abrasive slurry and a polishing pad. A fixture registers the deformed stack against a rear datum and presents its outer face to the belt over a rigid platen. Successively finer silicon carbide belts remove material in shallow passes until the total removal exceeds one blank thickness and exposes the inclined interfaces. A thickness gauge referenced to the rear datum measures stock removal between passes.

Matched rolls for continuous ramp forming

A profiled upper roll and a smooth lower roll replace a reciprocating forming die. The upper roll has a raised annular land with a tapered shoulder that presses a longitudinal track into a strip of pressure-consolidated, diffusion-treated alloy layers. The lower roll supports the rear face while the shoulder displaces the internal interfaces into a slope across the strip width. A flat finishing head removes more than one blank thickness from the original outer face and intersects the sloping interfaces to expose a continuous colour transition along the strip.

Parameter or scale variation

Two blanks with a shallow ramp

A 0.25 mm brass blank sits on a 1.00 mm copper blank during pressure consolidation and diffusion heat treatment. A flat-backed die depresses the consolidated stack locally and forms a 0.20 mm descent over a 10 mm ramp relative to the original outer face. The face is polished to a plane 0.35 mm below the original outer face, so the plane intersects the inclined brass-to-copper transition. The die geometry leaves at least 0.10 mm of transition depth below the finished face on the depressed side of the intersection.

Combination with existing systems

Vacuum hot pressing with transfer tooling

A vacuum hot press consolidates the alloy blanks between flat platens and maintains the stack under pressure during the diffusion dwell. A removable carrier locates the cooled stack against edge stops and presents the same edges to a separate ramp-forming press. The ramp die deforms the bonded layers beneath the original outer face. A surface grinder registers the part from the same edges and removes stock from the outer face through more than one blank thickness before final polishing.

Automated or data-driven variant

Camera guided polishing depth control

An automated polishing station clamps the shaped stack against a rear datum and measures face height with a displacement sensor. After each pass, the station rinses and dries the face and captures an image under fixed diffuse lighting with a colour reference tile in view. Software measures the position and width of the visible colour transition and uses their change between passes to set the next removal increment. The controller stops when the transition lies within the specified position and width limits and measured removal exceeds one blank thickness.

Specific version of a part

Diamond cutting exposes the gradient

A single-point diamond tool removes successive thin chips from a shaped stack of compatible copper alloys. The total cut exceeds the thickness of the outermost blank, and a fine final pass leaves the exposed colour regions with a low-roughness finish.

Copper alloys with stepped composition

Four wrought blanks have nominal zinc contents of 5, 15, 25 and 30 percent by mass, with copper making up the balance. The blanks span reddish to yellow tones and follow increasing zinc content through the stack.

Hot pressing between flat platens

A vacuum hot press compresses four cleaned copper-alloy blanks between parallel platens. The platens apply load normal to the interfaces, and a displacement stop limits compression to a final stack thickness of 0.8 mm.

Warm coining with tapered tooling

A wedge-faced punch presses the warmed stack against a flat lower die and displaces metal into a relief pocket beside the punch. A mechanical stop sets the deepest point of the coined ramp 0.3 mm below the original outer-face plane.

Directional satin finishing

A fine nonwoven abrasive belt makes parallel passes over the exposed face with the belt direction aligned to the length of the article. Light contact pressure produces a uniform satin texture while limiting removal to a few micrometres.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2007/0111646 A1
Published
May 17, 2007
Filed
Nov 2, 2006
Class
B24B 9/00
Document BUS 2021/0301421 A1
Published
Sep 30, 2021
Filed
Jul 24, 2019
Class
C30B 29/36
Document CUS 2005/0280182 A1
Published
Dec 22, 2005
Filed
Jun 22, 2005
Claim 1
Document A
Document B
1.1Providing several blanks respectively made in metal alloys, distinguished by their chemical composition and colour,
1.2Stacking said blanks to form a stack, said stack being defined with an outer face,
1.3the method further comprising the following successive or concomitant steps: Applying stress at room temperature or at a hot temperature to said stack to form a cohesive stack having a thickness E greater than or equal to 100 μm,
1.4the method further comprising the following successive or concomitant steps: Diffusion thermal treatment between the blanks of said cohesive stack,
1.5the method further comprising the following successive or concomitant steps: Shaping by deformation, at room temperature or a hot temperature, of the cohesive stack to form an inclined surface (10a) relative to the plane of the outer face, the inclined surface (10a) extending to a depth P with respect to said outer face,
In this aspect, the SiC wafer manufacturing method further includes, before the etching process, an ingot molding process of processing a mass of a crystal-grown single crystal SiC into a columnar ingot; a slicing process of slicing the ingot to obtain a thin disk-shaped SiC wafer; a stamp forming process of forming a stamp portion by selectively removing a surface of the SiC wafer; and a chamfering process of chamfering an outer peripheral portion of the SiC wafer.
B · US 2021/0301421 A1 · ¶ 49
1.6the method further comprising the following successive or concomitant steps: Polishing the shaped stack from the outer face to a depth greater than the thickness of a blank to obtain the face with the colour gradient,,
For finishing (satin finishing and/or polishing) of sheet metal, systems with abrasive cloths are currently used, in which each finishing station comprises a pair of opposed finishing heads, each of which comprises a ring of abrasive cloth carried by a drive roller and by a roller which holds the abrasive cloth in contact with the surface to be processed.
A · US 2007/0111646 A1 · ¶ 2
In this aspect, the SiC wafer manufacturing method further includes: a chemical mechanical polishing process of performing chemical mechanical polishing on a surface of the SiC wafer following the etching process.
B · US 2021/0301421 A1 · ¶ 97
1.7the method further comprising the following successive or concomitant steps: the method further comprising the following optional step: Finishing the surface of the face to obtain the article.
Object of the present invention is to overcome the above-mentioned limits and drawbacks presented by satin finishing systems for sheet metal with sand belts and those with conventional flap wheels, allowing sheet metal to be satin finished—with a uniformly even surface finish—with a single mechanically fixed flap wheel, which has proved to be strong enough to be able to have the same width as the sheet metal to be satin finished.
A · US 2007/0111646 A1 · ¶ 13
The method includes: a satin finishing process S141 of satin-finishing at least a back surface 22 of a SiC wafer 20; an etching process 21 of etching at least the back surface 22 of the SiC wafer 20 by heating under Si vapor pressure after the satin finishing process S141; and a mirror surface processing process S31 of mirror-processing a main surface 21 of the SiC wafer 20 after the etching process S21.
B · US 2021/0301421 A1 · abstract

An empty cell means only that no passage was reproduced there.

Statements in these documents
The drawbacks and limitations inherent in conventional flap wheels have not thus far allowed flap wheel systems capable of satin finishing sheet metal with satisfactory results to be produced.
A · US 2007/0111646 A1 · ¶ 9
In fact it has been found experimentally that the length of conventional flap wheels cannot exceed about 10 cm: to satin finish sheets of metal with a greater width it would be necessary to use two or more conventional flap wheels side by side but the satin finished sheet metal would have lines coinciding with the gaps that are inevitably present between the side-by-side flap wheels.
A · US 2007/0111646 A1 · ¶ 10
Further, there are advantages that a friction coefficient on the back surface of the wafer is increased to prevent slipping during conveyance or in the equipment, the wafer is easily peeled off from an electrostatic chuck type sample table, and the like.
B · US 2021/0301421 A1 · ¶ 4
In order not to reduce the yield in the device manufacturing process, it is necessary to remove the work-affected layer.
B · US 2021/0301421 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0355847 A1, claim 1, first published 2026-11-19T16:20:06-05:00, https://patent.fyi/US20260355847/, SHA-256 14a433b609ddf4bf69c240d22d2d90f3a9a56c246131c10948fb7bd49d55dc42
First published
Permanent addresshttps://patent.fyi/US20260355847/
Content fingerprint (SHA-256)14a433b609ddf4bf69c240d22d2d90f3a9a56c246131c10948fb7bd49d55dc42
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi