Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Acrylic resin flux binder
What ifWhat if a low-softening thermoplastic acrylic resin serves as the flux binder?
Claim language“a rosin”
The acrylic resin forms a tacky film as the carrier evaporates, holding the indium sheet against the mating surface. The film softens during heating, allowing the acid activator to contact the surface oxides and the bonding pressure to displace the softened film toward the joint edges.
1.2Inorganic chloride flux activator
What ifWhat if an aqueous zinc chloride and ammonium chloride solution provides the flux activation?
Claim language“an organic acid”
A thin coating dries on the mating surfaces before the indium sheet is placed. During heating, the acidic chloride flux disrupts surface oxides and promotes indium wetting. A warm water rinse removes accessible chloride residues after bonding.
1.3Dry powder flux transfer
What ifWhat if a dry powder blend supplies the flux to the indium sheet?
Claim language“a solvent(S)”
A stencil meters a thin layer of powdered rosin and lauric acid onto the sheet, and a warm roller tacks the powder to the surface. During bonding, the flux melts, the acid reacts with surface oxides, and the clamping load pushes excess flux toward the open joint edges.
1.4Glutaric acid flux activation
What ifWhat if glutaric acid supplies the flux activation?
Claim language“a monocarboxylic acid (A1)”
Glutaric acid has two carboxyl groups and melts at approximately 98 °C. The molten acid contacts the mating surfaces during preheat and reacts with surface oxides before the indium melts.
1.4Liquid monocarboxylic acid activator
What ifWhat if the monocarboxylic acid activator is caprylic acid with a melting point near 16 °C?
Claim language“a melting point of 35 °C or higher and 90 °C or lower”
Caprylic acid is liquid at typical room temperature and spreads through the flux film as the carrier evaporates. During preheat, the acid reacts with surface oxides, and a thin coating limits the amount of liquid the bonding load must displace.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Indium seals for optical windows
A stamped indium ring fits between a gold-coated annulus on a sapphire window and a gold-plated annular seat on an instrument housing. A thin coat of flux containing rosin, lauric acid, and ethanol covers each face of the ring. The parts remain apart during solvent evaporation, then a fixture brings them together and holds the gap while the indium melts and solidifies.
Component substitution
Polyester resin in place of rosin
An ethanol-soluble, carboxyl-terminated polyester resin replaces rosin as the film-forming component. Lauric acid and the polyester resin dissolve in ethanol, and a stencil deposits the solution on nickel-gold plated copper before placement of the indium sheet. Ethanol evaporates during preheating, and the acid promotes wetting when the indium melts.
Parameter or scale variation
Thin foil with a staged heating cycle
A 75 µm indium foil joins two nickel-gold plated copper coupons, and 50 µm fixture stops set the final separation. A 10 µm wet film of flux containing rosin, lauric acid, and ethanol covers each mating surface, and the coupons dwell separately at 80 °C for 90 seconds in flowing nitrogen. The fixture closes the stack, holds the joint at 165 °C for 45 seconds, and maintains the separation until the indium solidifies.
Combination with existing systems
Flux bonding in a vacuum reflow chamber
An indium preform sits between nickel-gold plated copper parts in a vacuum reflow chamber with a heated platen and a movable upper fixture. A flux containing rosin, lauric acid, and ethanol coats the mating faces, and the fixture holds the faces apart during a warm nitrogen purge. The fixture closes the stack against hard stops, and the chamber reduces pressure during the molten dwell to expand trapped gas and promote its escape through the joint perimeter.
Indium bonding with a heated roller
A slot die coats one face of a moving nickel-gold plated copper strip with flux containing rosin, lauric acid, and ethanol. The strip passes through a ventilated drying zone before a second unwind feeds indium ribbon onto the coated face. Heated rollers bring the interface above the indium melting point, and an adjustable roller gap sets the laminate thickness before a cooled roller solidifies the bond.
Automated or data-driven variant
Mass feedback for flux dispensing
A positive-displacement dispenser applies a flux containing rosin, lauric acid, and ethanol to a plated copper part on a load cell. The controller tares the part, records the mass immediately after each dispensing pass, and adjusts the next pass to reach the target wet flux mass before solvent evaporation changes the reading substantially. After a timed drying step, a placement head aligns an indium preform and the mating part for reflow.
Specific version of a part
Gum rosin flux binder
Gum rosin dissolved in isopropanol deposits a continuous resin film as the carrier evaporates. The film holds the acid activator on the coated surface and softens during preheat.
Lauric and glutaric acid blend
The acid package contains lauric acid as a monocarboxylic component and glutaric acid as a dicarboxylic component. Both acids melt below the melting point of indium and contact surface oxides during preheat.
Myristic acid flux activator
Myristic acid contains one carboxyl group and melts at approximately 54 °C. It melts during preheat and reacts with surface oxides as the joint approaches the bonding temperature.
Isopropanol coating solvent
Isopropanol boils at approximately 83 °C at atmospheric pressure and dissolves gum rosin and lauric acid for thin-film coating. The film dries on the exposed mating surface before the indium sheet is placed.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
A rosin composition includes a gum rosin, an emulsifier, and a randomizing additive.
A · US 2014/0272113 A1 · abstract
In one or more embodiments, gum rosins in accordance with the present disclosure may be low molecular weight gums produced from natural sources including various species of pine tree, such as Pinus eliotti.
B · US 2017/0137690 A1 · ¶ 17
1.2an organic acid; and
For example, in one or more embodiments, gum rosins may be activated with rosin activators including halide activators such as organic halide salts, including dimethylammonium chloride and diethylammonium chloride, and organic acids including monocarboxylic acids such as tannic acid, acetic acid, propionic acid, and dicarboxylic acids such as oxalic acid, malonic acid, sebacic acid.
B · US 2017/0137690 A1 · ¶ 18
1.3a solvent(S),
In other embodiments, the gum rosin protective coating composition is adjusted such that the disclosed gum rosin flux/emulsifier/randomizing agent mixture is in a range from about 20 to about 100% by weight with the remaining components including an aqueous solvent or organic polymer solvent.
A · US 2014/0272113 A1 · ¶ 35
1.4wherein the organic acid includes a monocarboxylic acid (A1) having a melting point of 35 °C or higher and 90 °C or lower, and
1.5the solvent(S) includes a solvent (S1) having a boiling point of 100 °C or lower.
Examples of solvent-based emulsifiers include, but are not limited to, trichloroethane, acetone isopropyl alcohol (IPA), an IPA and water combination, toluene, benzene, 2-propanol (IPA), methyl ethyl ketone (MEK), toluene/acetone/methyl ethyl ketone (MEK) and IPA combination, 1,1-dichloroethane, isoamyl acetate, cellusolve acetate, acetone, xylene, 1,1,1,1-tetrachloromethane, 1,1,2,2-tetrachloroethene, 1,1,1-trichloroethane, 1,1,2-trichloroethane, 1,1-dichloroethane, 1,1-dich
A · US 2014/0272113 A1 · ¶ 18
Other mutual solvents may include low molecular weight alcohols, esters of fatty acids such as isopropyl myristate, isopropyi oleate, rapeseed methyl esters, and the like.
B · US 2017/0137690 A1 · ¶ 19
An empty cell means only that no passage was reproduced there.
Statements in these documents
Accordingly, a protective coating to preserve the solderability of a circuit card during storage is desired to improve the manufacturing of circuit card assemblies and printed wiring boards.
A · US 2014/0272113 A1 · ¶ 4
In some embodiments of the present invention, a method of protecting a circuit card for storage is provided, where the method includes applying a rosin composition including a gum rosin, an emulsifier, and a randomizing additive, drying the circuit card to obtain a coated circuit card, storing the circuit card, and optionally removing the rosin composition from the coated circuit card.
A · US 2014/0272113 A1 · ¶ 6
Thus, fluid loss or lost circulation is a recurring drilling problem, characterized by loss of wellbore fluids into downhole formations that are fractured, highly permeable, porous, cavernous, or vugular.
B · US 2017/0137690 A1 · ¶ 3
In one aspect, embodiments of the present disclosure are directed to wellbore strengthening compositions that may contain a base fluid; and a solid gum rosin additive, wherein the solid gum rosin additive has an average particle size of 1 μm to 15 mm.
B · US 2017/0137690 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0355865 A1, claim 1, first published 2026-11-19T16:20:06-05:00, https://patent.fyi/US20260355865/, SHA-256 6a0a00bf8ff7c7c98cd1e178fe5a1ed9e4757f4d87c8db4f7e177d66d29fa92b