Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Ranking by measured light
What ifWhat if the process ranks finished crystals by measured light output without setting an optical yield or output target?
Claim language“a target optical yield”
A fixed abrasive sequence finishes each crystal in the batch. A pulsed excitation source and a photodetector measure the integrated signal from each crystal under the same coupling conditions. The measured signal ranks the crystals for assembly.
1.1Timing based finish selection
What ifWhat if a detector coincidence timing requirement replaces the optical output target and no optical yield target is set?
Claim language“a target optical output value”
Test crystals with different side finishes are coupled to photodetectors and exposed to coincident excitation events. Timing electronics measure the distribution of arrival-time differences. Production uses the finish that meets the specified width of that distribution.
1.2Light collection on every face
What ifWhat if every crystal face serves as a light output surface?
Claim language“at least one non-light-output surface”
Optical gel couples a photodetector tile to each of the six polished faces of a cubic crystal. Readout electronics sum the six integrated signals to measure the collected light from each event.
1.3Contact driven finish selection
What ifWhat if assembly contact requirements alone set the finishes on the output face and the side faces?
Claim language“based on at least one of the target optical yield”
The optical coupling pad sets the output-face flatness tolerance through its allowable compression range. Adhesive bond tests on side-face coupons set the side-face roughness range. The drawing records both limits for machining and inspection.
1.4Finish transfer during growth
What ifWhat if the crystal acquires its face finishes during growth without a machining step?
Claim language“machining the crystal”
A seed initiates solidification in a split mold for a low-melting crystal material that releases from the mold after cooling. A smooth mold insert defines the light exit face, and textured wall inserts imprint the side faces as the melt solidifies.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Surface finishing for spectrometer light guides
A rectangular sapphire light guide carries near-infrared light from a sample chamber to a spectrometer. The detector-facing end serves as the light output surface, and the four long faces sit against a light-absorbing sleeve. A ray model uses the minimum detector power and maximum power leaking through the sleeve to set a roughness limit for the output end and a separate roughness range for the long faces. A polishing lap finishes the output end, and a fine grinding wheel textures the long faces.
Component substitution
Ion beam finishing of the exit face
A machining station replaces the contact polishing head for the light output face with a rastered ion beam. The target power coupled into a downstream lens sets the flatness tolerance of the output face and the roughness range of the non-output sidewalls through a calibrated optical model. An interferometer maps the prepolished output face, and the station uses the measured height map and calibrated beam removal profile to compute dwell times. The beam corrects the output face while a separate abrasive station grinds the sidewalls to their roughness range.
Parameter or scale variation
Face finishing for fine pitch arrays
A 16 by 16 detector array uses crystal bars that measure 0.8 mm by 0.8 mm by 12 mm. A calibration table maps the target signal per channel to an output-end roughness of 20 nm RMS or less and a non-output sidewall roughness of 0.4 to 0.8 µm RMS. A grooved carrier holds 16 bars with their output ends coplanar for batch polishing. The carrier indexes the bars through four positions for sidewall grinding, and a surface profilometer verifies both finishes over their specified measurement bandwidths.
Stepped sidewall finish along long crystals
A 100 mm scintillator bar has one detector-facing output end and four non-output sidewalls, each divided into four 25 mm bands. A ray model uses the target power at the detector to select an output-end roughness limit and a sidewall roughness profile from calibrated finishes of 0.2, 0.5, and 1.0 µm RMS. A numerically controlled grinder applies the selected finish to each band by changing the abrasive pass sequence at the programmed band boundaries. A separate lap polishes the output end to its assigned limit.
Combination with existing systems
Crystal finishing with integrating sphere feedback
A crystal machining cell pairs a polishing station and a sidewall grinding station with an integrating sphere that measures power from one face at a time. A fixture registers the output face against the sphere port while a baffled source illuminates the opposite end at fixed power. A calibration table assigns an output-face roughness limit and a non-output sidewall roughness range from the target collected power. The cell machines each face group to its assigned finish and uses the sphere to verify the finished crystal.
Automated or data-driven variant
Model selection of paired surface finishes
A controller reads the output-face and non-output-face assignments from the crystal fixture drawing. A regression model trained on finished samples predicts collected power from the roughness of each face group, crystal dimensions, and reflector spacing. The controller evaluates finish pairs from a table of available machining recipes and selects the shortest recipe pair whose predicted power meets the target. A profilometer measures both finishes after machining, and an optical test station records the resulting power with the measured finishes.
Specific version of a part
Background corrected photoelectron target
A process controller reads a target mean count of 3,000 detected photoelectrons per excitation pulse from a recipe file. The recipe fixes the excitation energy, detector bias, coupling layer thickness, and integration gate used for the background-corrected measurement.
Face assignment by fixture datums
A keyed fixture locates a rectangular crystal against two side stops and places one end face against an optical coupling pad. The process record identifies that end face as the light output surface and the opposite end and four long faces as non-light-output surfaces.
Paired roughness from coupon measurements
A calibration table stores measured optical output for pairs of arithmetic mean roughness values on the exit face and the side faces. The controller selects a pair whose measured output falls within the target band and records the two roughness setpoints in the machining recipe.
Face specific abrasive finishing
A rotary fixture presents the output face to a pitch lap charged with a 1 micrometre diamond slurry, then indexes the side faces against a platen carrying 15 micrometre diamond abrasive. The machine checks each face group with an optical profilometer between passes and stops finishing that group when its measured roughness enters the assigned tolerance band.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1obtaining at least one of a target optical yield or a target optical output value of a crystal;
1.2determining at least one light output surface and at least one non-light-output surface of the crystal;
1.3determining a first surface parameter of the least one light output surface and a second surface parameter of the least one non-light-output surface based on at least one of the target optical yield or the target optical output value;
1.4machining the crystal based on the first surface parameter and the second surface parameter.
No. 4,256,467 (Gorsuch) describes an abrasive article with diamond particles plated onto an electrically insulated mesh cloth which can be cut into a “daisy wheel” for use in grinding curved, convex, or concave optical lenses.
A · US 2005/0032469 A1 · ¶ 36
Lapping is a time-honored way of refining the geometry and finish of work pieces. Typically, the work piece is rubbed over a flat abrasive base surface that is larger than the work piece.
B · US 2005/0255803 A1 · ¶ 2
An empty cell means only that no passage was reproduced there.
Statements in these documents
Uniform wear of the abrasive is experienced across the full annular band of abrasive material that allows a continuously flat abrasive surface to be presented to a workpiece.
A · US 2005/0032469 A1 · ¶ 3
Most performance issues relate to two primary concerns, 1) hydroplaning caused by water lubricant and 2) vibrations created by grinding machine component dimensional inaccuracies and thickness variations of abrasive disks along their tangential surfaces.
A · US 2005/0032469 A1 · ¶ 5
The present invention relates to a precision abrasive finishing apparatus, specifically, to a lap surface capable of being retrofitted to a conventional lapping table or to a curved mold.
B · US 2005/0255803 A1 · ¶ 1
What is needed is a means for using a true flat granite base for lapping applications that does not employ abrasive papers and films and that does not abrade the granite base.
B · US 2005/0255803 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0355896 A1, claim 1, first published 2026-11-19T16:57:22-05:00, https://patent.fyi/US20260355896/, SHA-256 eff398f403464366e910db741471c1acc91af9cddb1d0e114c4fd2e3906072c1