Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Acrylate network with pendant fluorine
What ifWhat if the coating uses a fluorinated acrylate formulation with no silicon-containing polymer?
Claim language“a polymer with a silicon-containing hydrolyzable terminal group”
A metering roll applies a thin layer of urethane diacrylate blended with a fluorinated acrylate and a photoinitiator. Ultraviolet exposure crosslinks the acrylate groups, and fluorinated side groups lower the surface energy of the cured layer.
1.1Removable interleaf between turns
What ifWhat if a removable fluoropolymer interleaf separates adjacent turns during rubber curing?
Claim language“a layer of curable coating composition”
A second unwind feeds a preformed polytetrafluoroethylene film into the winding nip alongside the uncured rubber sheet. The film keeps neighboring turns apart during heating and feeds onto a separate take-up reel when the cured sheet unwinds.
1.2Cooling sets the surface film
What ifWhat if cooling solidifies a thermoplastic surface film before winding?
Claim language“form a cured coating layer”
A heated slot die applies molten low-density polyethylene to the rubber, and a chilled roll solidifies the film by cooling. During the subsequent low-temperature rubber cure, the roll stays below the melting onset of the polyethylene so the film continues to separate adjacent rubber surfaces.
1.3Flat panels on trays
What ifWhat if perforated trays carry flat panels of coated rubber through curing?
Claim language“onto itself to form a roll”
A guillotine cuts the coated uncured sheet into panels, and a rack supports each panel on a release-faced perforated tray. Forced hot air circulates between the trays and heats each panel while adjacent panels remain separated.
1.4Moving web through a press
What ifWhat if the rubber cures as a flat moving web before take-up?
Claim language“subjecting the roll to curing conditions”
A double-belt press carries the coated uncured sheet between heated steel belts under pressure. Line speed sets the dwell time in the heated zone, and the cured web cools before it reaches the take-up reel.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Roll curing for conveyor skirt stock
A flexible coating based on an alkoxysilane-terminated polymer is applied to one planar face of uncured nitrile rubber sheet intended for conveyor skirting. The coated web passes through a humidified tunnel that cures the coating before the sheet is wound onto itself. The wound sheet is heated to vulcanize the nitrile rubber, then cooled, unwound and slit into skirt strips.
Component substitution
Ultraviolet cure with urethane acrylate
A flexible urethane acrylate formulation with a radical photoinitiator replaces the coating based on a polymer with hydrolyzable silicon terminal groups. A reverse-roll coater meters the formulation onto one face of the uncured rubber, and an ultraviolet lamp bank in a nitrogen-purged enclosure polymerizes the film. The sheet is wound after the film becomes tack-free, heat-cured in roll form and unwound after cooling.
Parameter or scale variation
Short rolls with limited radial buildup
A slitter divides a 600 mm wide, 2 mm thick uncured sheet carrying a cured surface coating into four 150 mm wide lanes. Each lane is wound onto a 200 mm diameter steel core to a maximum outer diameter of 300 mm, which limits radial buildup to 50 mm. The rolls sit on separate rack positions during thermal curing, and a thermocouple at the slowest-heating position in an instrumented reference roll determines when the rubber cure hold begins. The rolls cool on their cores before unwinding.
Combination with existing systems
Heated cores in a recirculating oven
A forced-air batch oven circulates hot air around rolls of uncured rubber sheet carrying a cured surface coating. Each sheet is wound onto a hollow steel mandrel fitted after winding with a removable electric heater that supplies heat through the core. Core and chamber temperature sensors regulate the two heat inputs during rubber vulcanization. The rolls are cooled and transferred to an unwind stand.
Automated or data-driven variant
Inline measurement of coating cure
A near-infrared sensor scans the coated face across the web at the outlet of a humidified coating cure tunnel. A calibration model built from samples with measured gel fractions converts the spectra into an estimate of coating cure. A controller adjusts web speed to maintain the validated cure threshold and uses an encoder to mark below-threshold sections for removal ahead of the winder. Accepted sections are wound, thermally cured as rolls and unwound after cooling.
Rubber cure control from embedded temperatures
An instrumented reference roll with the same dimensions and winding conditions as the production rolls carries thermocouples between wraps near the core, at mid-radius and near the outer surface. A controller integrates the measured temperature histories using a cure-rate model calibrated from moving-die rheometer data for the rubber compound. The controller ends the heating cycle when the lowest predicted cure state among the monitored positions reaches the specified target. The production rolls are cooled and unwound.
Specific version of a part
Alkoxysilane terminated polyether coating
A reverse-roll coater meters a blend of alkoxysilane-terminated polyether and a silanol condensation catalyst onto one face of the uncured rubber sheet. The applicator gap and roll speed control the wet film thickness.
Humidity controlled coating cure
A web conveyor carries the coated rubber through a chamber supplied with warm, humid air. Water hydrolyzes the terminal alkoxysilane groups, and condensation of the resulting silanols links the polymer chains through silicon–oxygen–silicon bonds.
Torque controlled core winding
A driven mandrel winds the uncured sheet over a rigid cylindrical core with the cured coating facing outward. A load cell measures web tension, and the drive tapers the tension setpoint as the roll diameter increases.
Forced air roll curing
A rack supports the wound roll by its core in a recirculating hot-air oven. A thermocouple near the core of an instrumented roll tracks heat penetration, and the cure schedule gives the inner wraps the dwell time required by the rubber compound.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1(i) applying a curable coating composition to a planar surface of an uncured rubber sheet to form a layer of curable coating composition, wherein the curable coating composition includes a polymer with a silicon-containing hydrolyzable terminal group;
A method of adhering a substrate to an adherent in an electrical component is also provided which includes the steps of providing an adhesive composition comprising an acrylic resin containing polymerizable acrylates, a moisture-curable alkoxy or acyloxy silane terminated polymer, a photoinitiator for polymerizing the acrylates, and a photoacid generator for catalyzing a moisture cure reaction of the alkoxy or acyloxy silane terminated polymer; providing a substrate; providin
A · US 2007/0219285 A1 · ¶ 38
This uncured rubber sheet, which can also be referred to as a green sheet, can be provided to the coating step 25, wherein a layer of curable coating composition is applied to one planar surface of the uncured rubber sheet.
B · US 2016/0319090 A1 · ¶ 12
1.2(ii) subjecting the curable coating composition to curing conditions that cure the coating composition and thereby form a cured coating layer on the uncured rubber sheet;
Following application of the curable coating composition, which forms a layer of curable coating composition on the uncured sheet, the curable coating composition is subjected to curing conditions within a curing step 30. Following the step of curing the curable coating composition, which forms a cured coating layer on the uncured rubber sheet, the membrane is rolled onto itself, which may also be referred to as winding, within rolling or winding step 35.
B · US 2016/0319090 A1 · ¶ 12
1.3(iii) rolling the uncured rubber sheet having a cured coating layer onto itself to form a roll;
Preferably, the IC chip strap and antenna roll are compressed together, for example by rolling the RFID assembly tightly, because pressing maximizes wetting and electrical contact between the adhesive composition and the IC chip roll, and between the adhesive composition and the antenna roll.
A · US 2007/0219285 A1 · ¶ 42
Following the step of curing the curable coating composition, which forms a cured coating layer on the uncured rubber sheet, the membrane is rolled onto itself, which may also be referred to as winding, within rolling or winding step 35. This step produces a roll of uncured rubber sheet having disposed on one planar surface thereof a layer of cured coating.
B · US 2016/0319090 A1 · ¶ 12
1.4(iv) subjecting the roll to curing conditions that cure the uncured rubber sheet and thereby forms a roll of cured rubber sheet, and
This roll is then subjected to curing conditions within curing step 40, which serves to cure the uncured rubber sheet. As a result of curing step 40, a roll of cured rubber sheet is produced, wherein the cured rubber sheet has disposed on one planar surface thereof a cured coating layer.
B · US 2016/0319090 A1 · ¶ 12
1.5(v) unrolling the roll of cured rubber sheet after subjecting the roll to curing conditions.
The method of claim 1, further comprising the step of unrolling the roll of cured rubber sheet after said step of subjecting the roll to curing conditions.
B · US 2016/0319090 A1 · claim 3
An empty cell means only that no passage was reproduced there.
Statements in these documents
There is still a need for an adhesive composition which can be B-staged quickly and efficiently and which allows for quick assembly of electronic components, such as for the assembly of radio frequency identification tags.
A · US 2007/0219285 A1 · ¶ 3
The composition of the present invention is useful for rapid electronic assembly, such as assembly of radio frequency identification tags.
A · US 2007/0219285 A1 · ¶ 7
The rubber sheet is fabricated by using a process that results in a particulate-free cured sheet.
B · US 2016/0319090 A1 · ¶ 2
Where adhesives are employed to seam the membranes to each other (i.e., create a lap seam) and/or adhere the membrane to the roof surface, the presence of the dusting agent, which may also be referred to as particulate, can be problematic since the dusting agent can interfere with proper adhesion between the membrane and the adhesive.
B · US 2016/0319090 A1 · ¶ 6
Cite aspatent.fyi, US 2026/0356009 A1, claim 1, first published 2026-11-19T19:14:50-05:00, https://patent.fyi/US20260356009/, SHA-256 d395ec7da631db1ce75aec213301b0615ba5a59536eb2a13b4a6e1deb314e9f7