1.1Direct print on fabric
A screen deposits an opaque two-part silicone ink onto the fabric in the shape of the marking. The ink wets exposed yarns and crosslinks into a flexible coating that carries the color.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A screen deposits an opaque two-part silicone ink onto the fabric in the shape of the marking. The ink wets exposed yarns and crosslinks into a flexible coating that carries the color.
The label stack bonds to the center of a woven polyester backing, leaving a narrow flange around the perimeter. A lockstitch passes through the flange and garment fabric and carries the attachment load.
A reducing discharge paste decolorizes dischargeable dye in a cotton fabric patch that extends slightly beyond the label footprint. Rinsing removes soluble reaction products before the patch is dried and the label is applied.
A reactive polyurethane primer bonds a preformed thermoplastic polyurethane film to the ethylene vinyl alcohol barrier. During lamination, the polyurethane film softens and wets the underside of the label face.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A printed polyester face film overlies an upper copolyamide layer, an ethylene vinyl alcohol barrier, and a lower copolyamide layer in that order. A flat platen hot presses the lower copolyamide against dyed polyester upholstery fabric before the fabric is cut and sewn. The lower layer bonds to the yarns, and the barrier limits dye migration from the upholstery into the printed face.
A fully hydrolyzed polyvinyl alcohol film replaces the ethylene vinyl alcohol barrier. Corona treatment raises the surface energy on both sides of the dry film before heated rolls laminate it between two copolyamide films. The upper copolyamide bonds to a printed polyester face, and the lower copolyamide bonds to the fabric during hot pressing. The continuous polyvinyl alcohol film limits dye migration in dry service.
From the fabric side outward, the label uses a 20 micrometer copolyamide layer, a 10 micrometer ethylene vinyl alcohol barrier, a 15 micrometer copolyamide layer, and a 25 micrometer polyester face film. The four layers have a combined nominal thickness of 70 micrometers before printing. Hot pressing softens the lower copolyamide to bond it to the fabric, while the reduced section thickness lowers bending stiffness.
The upper and lower copolyamide layers and the ethylene vinyl alcohol barrier extend 1.5 millimeters beyond the printed polyester face on all sides. A registered cutter cuts the face to its smaller outline before lamination, and a second cutting station cuts the larger three-layer stack. Hot pressing bonds the lower copolyamide across the full footprint, and the extended barrier increases the lateral distance that dye must travel around its edge to reach the face.
A heat-resistant release carrier supports the printed face of a laminate with an upper copolyamide layer, an ethylene vinyl alcohol barrier, and a lower copolyamide layer. A web guide brings the exposed lower copolyamide into contact with a continuous fabric web at the inlet of a heated drum press. A pressure belt holds the two webs against the drum as the lower layer bonds to the fabric. Downstream cooling rolls set the bond before a peel roller removes the carrier.
The controller uses a calibrated platen thermocouple and a load cell to monitor the hot pressing of a label with a copolyamide, ethylene vinyl alcohol, and copolyamide stack beneath a printed face. A fabric recipe stores the platen temperature band, press force band, and dwell time established on bonded test coupons. The controller accumulates dwell time only while both readings remain within their bands. It opens the press once the recipe dwell is met and flags the part if the cycle reaches its time limit first.
A patterned metal roll presses recessed characters into the softened upper film during manufacture. A polished roll surface leaves glossy recesses against a matte background so the characters remain visible by reflected light.
A 45-micrometer copolyamide hot-melt film with a softening range of 105 to 115 °C forms the fabric-facing layer. During pressing, the softened polymer flows around surface fibers and solidifies as the assembly cools.
A 15-micrometer ethylene vinyl alcohol film containing 32 mole percent ethylene covers the full label footprint. The film is laminated against the lower copolyamide layer and limits dye diffusion through the thickness of the assembly.
A 25-micrometer copolyamide upper layer meets the molten barrier polymer in a flat coextrusion die. A chill roll cools the two layers together and fixes their thickness.
A 60-micrometer matte thermoplastic polyurethane film carries cured polyurethane ink on its exposed face. The underside is corona treated and heat laminated to the upper copolyamide layer.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
The face stock may have a monolayer or multilayer structure.B · US 2018/0179411 A1 · ¶ 41
To enhance adhesion of the label to a tire sidewall having surface irregularities, such as serrations, raised or depressed lettering, vent ports and tread, extra adhesive 14 is pushed through the intermediate layer 17 to better contact the recessed areas 28 of a tire surface. The intermediate layer 17 can be made of a mesh, woven or knit fabric.A · US 7,338,914 B2 · ¶ 32
During labelling the release liner 4 is removed and the label 11 is attached onto the surface to be labelled through the adhesive layer 3.B · US 2018/0179411 A1 · ¶ 52
Barrier films and primer layers are sometimes used between the back of the label film and adhesive layer to prevent discoloration and loss of adhesion caused by migration of low molecular weight mobile components such as waxes, extender oils, lubricants, anti-reversion coagents, sulphide resins, and plasticized sulfur from within the tire into the label face stock and adhesive as the tire ages.A · US 7,338,914 B2 · ¶ 6
In some embodiments, the label 2 may include an intermediate layer 17 of label face stock material that can be capped or laminated with a cap layer 18 (FIGS. 3A-3C) which may comprise another film, coating or woven material 18 for additional stiffness, printability or prevention of adhesive flow through the label face stock 10.A · US 7,338,914 B2 · ¶ 25
Further the label typically includes graphical patterns MRK1 on the surface of the face stock 2. In an example, a topmost surface of the face stock 2 comprises printing.B · US 2018/0179411 A1 · ¶ 52
An empty cell means only that no passage was reproduced there.
The problem with these solid films is they can be stiff and non-conformable.A · US 7,338,914 B2 · ¶ 4
Thus, it is desirable to have a label construction that restricts or prevents this diffusion process.A · US 7,338,914 B2 · ¶ 6
This is often necessary for filmic face stock materials which without further surface treatment may have significantly poorer printability compared to paper face stock materials.B · US 2018/0179411 A1 · ¶ 2
For example, top coating may be used for enhancing ink anchorage, moisture resistance, optical and/or antiblocking properties, slip (coefficient of friction), antistatic properties or resistance to mechanical damages.B · US 2018/0179411 A1 · ¶ 2
patent.fyi, US 2026/0356079 A1, claim 1, first published 2026-11-19T19:49:30-05:00, https://patent.fyi/US20260356079/, SHA-256 f516e2de9c32224d5157276c3d028822ab5b4aaceb624c400329c9254523bb12