1.3Patterned nickel film as mask
A reusable metal stencil defines where sputtered nickel lands on the underside of the copper foil. An alkaline ammoniacal copper etchant dissolves copper through the openings between the nickel features.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A reusable metal stencil defines where sputtered nickel lands on the underside of the copper foil. An alkaline ammoniacal copper etchant dissolves copper through the openings between the nickel features.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A 12 micrometer copper foil supported on a graphite carrier serves as the growth surface for chemical vapor deposition. After application of the polymer support, an ink mask on the underside leaves circular openings 0.8 millimeters in diameter on a staggered array with a 2.0 millimeter center-to-center pitch. Wet etching clears the copper through its full thickness at each opening. A transmitted-light inspection checks for residual copper, and the polymer support spans the openings during rinsing.
A drop-on-demand printhead places acrylate ink containing a photoinitiator on the underside of the copper foil. Ultraviolet exposure crosslinks the printed features to form the etch mask.
A shallow bath of aqueous ammonium persulfate contacts the patterned underside and dissolves the exposed copper. A deionized water rinse removes residual etchant and soluble copper salts from the supported composite.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Then the exposed sample is developed in the developer for 10 s, and fixed for 30 s inside the fixer solution, at last blew-dry by nitrogen, so that pattern on the photolithography mask can be replicated on the photoresist.B · US 11,760,641 B2 · ¶ 64
Put it into the etching solution (CuSO4:HCl:H2O=10 g:50 ml:50 ml) to etch the copper foil away.A · US 8,906,245 B2 · ¶ 29
An empty cell means only that no passage was reproduced there.
It is very light, with a 1-square-meter sheet weighing only 0.77 milligrams.A · US 8,906,245 B2 · ¶ 3
It has a high carrier mobility, as well as low noise, allowing it to be used as the channel in a field-effect transistor.A · US 8,906,245 B2 · ¶ 6
In step 1) of the above described method, said metal substrate is single crystal and/or polycrystalline substrate of transition metal or transition metal alloy.B · US 11,760,641 B2 · ¶ 10
Said transition metal is selected from at least one of copper, nickel, molybdenum, and gold.B · US 11,760,641 B2 · ¶ 10
patent.fyi, US 2026/0356084 A1, claim 1, first published 2026-11-19T19:49:30-05:00, https://patent.fyi/US20260356084/, SHA-256 6b293e6c18b1dc0f6b1cab2a13268f4ba703a79ea601d2efe01b9d8a95bc9afe