patent.fyi
Applications  /  US 2026/0356553
United States Patent Application Publication

US 2026/0356553 A1

Published
Nov 12, 2026
Filed
Feb 7, 2023
Earliest date on the face
Feb 7, 2023
Classification
B65D 53/02
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Annealed copper sealing ring

What ifWhat if the sealing element were an annealed copper ring?
Claim language“a polymer composition”

A threaded retaining collar presses the copper ring against a raised circular land on the vessel rim. The copper deforms under the load and fills shallow machining marks along the contact band.

1.1Expanded graphite sealing ring

What ifWhat if the sealing element consisted of binder-free expanded graphite?
Claim language“a polymer composition”

A press forms expanded graphite flakes into an annular gasket. A bolted cover compresses the gasket between flat faces, reducing its pore volume and pressing it into surface irregularities.

1.2Crosslinked silicone sealing ring

What ifWhat if the sealing composition used crosslinked silicone rubber as its sole polymer?
Claim language“a first butene copolymer”

A mold forms and cures the silicone rubber into a round-section ring. The closure compresses the ring in an annular groove, and elastic recovery maintains contact with the vessel rim.

1.2Lower melting butene copolymer

What ifWhat if the butene copolymer had a melting temperature of 115 °C?
Claim language“a melting temperature Tm above 130 °C”

The melting peak occurs at 115 °C on the second heating curve of a differential scanning calorimetry measurement at 10 °C per minute. A screw cap compresses the molded liner against the rim of a room-temperature vessel to form an annular seal.

1.2First heating melting measurement

What ifWhat if the melting temperature were determined from the first heating curve?
Claim language“the second heating curve”

A differential scanning calorimeter heats a specimen cut from the molded liner at 10 °C per minute. The melting temperature is the temperature at the maximum of the copolymer melting endotherm during that initial scan, which captures the effect of the liner's molding and cooling history.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Screw cap for pigment sample jars

A threaded cap closes a wide-mouth jar used to store dry ceramic pigment samples. A molded annular liner sits in a recess under the cap and contains a butene copolymer with a melting temperature above 130 °C on the second differential scanning calorimetry heating curve at 10 °C per minute. Tightening the cap compresses the liner against the flat jar rim to contain fine powder during handling.

Component substitution

Crosslinked silicone gasket in a screw cap

A molded, crosslinked silicone rubber ring replaces the butene copolymer composition in a screw-cap sealing element. An annular groove under the cap retains the ring, and a flat land on the vessel rim contacts its exposed face. A shoulder on the vessel limits cap travel and sets the installed compression of the ring.

Parameter or scale variation

Controlled gasket compression for a drum lid

A removable drum lid for a 300 mm diameter opening carries a 4.0 mm thick annular gasket in a flat-bottomed recess. The gasket contains a butene copolymer with a melting temperature above 130 °C on the second differential scanning calorimetry heating curve at 10 °C per minute. A clamp band draws the lid against a hard stop that leaves a 3.2 mm gap between the recess floor and the drum rim, giving 20 percent nominal axial gasket compression.

Two concentric sealing ribs on one liner

A screw cap carries a molded annular liner with two concentric ribs on its underside, each 0.4 mm high and spaced 2.0 mm apart center to center. The liner contains a butene copolymer with a melting temperature above 130 °C on the second differential scanning calorimetry heating curve at 10 °C per minute. Both ribs bear on a flat vessel rim that is 4.0 mm wide, and a cap stop limits their nominal compression to 0.1 mm.

Combination with existing systems

Gasketed cap with a dispensing pump

A threaded closure carries a manual piston pump through a central opening, and an elastomeric washer seals the pump flange to the closure. A separate annular liner seals the bottle rim and contains a butene copolymer with a melting temperature above 130 °C on the second differential scanning calorimetry heating curve at 10 °C per minute. A dip tube connects to the pump inlet, and inlet and outlet check valves direct liquid from the bottle to the nozzle as the piston cycles.

Automated or data-driven variant

Automated calorimetry for incoming resin lots

An autosampler loads a pan containing a sample from each incoming butene copolymer lot into a differential scanning calorimeter. The instrument heats the sample through melting, cools it under a programmed ramp, and reheats it at 10 °C per minute. Software records the melting peak temperature from the second heating curve and releases the lot to the closure-liner molding line when the recorded temperature exceeds 130 °C.

Specific version of a part

Silica filled silicone gasket

A silicone rubber composition contains dispersed fumed silica to reinforce the cured material. A compression mold shapes and cures the composition into a flat annular gasket for a clamped lid.

Foamed polyethylene disk liner

A die cuts a circular liner from closed-cell low-density polyethylene foam sheet. The foam compresses against the rim as the cap tightens and accommodates local variations in rim height.

Butene ethylene copolymer liner

The liner composition contains a butene-1 and ethylene copolymer with a melting peak at 132 °C on the second heating curve of differential scanning calorimetry at 10 °C per minute. A mold forms the composition into an annular liner that the cap presses against the vessel rim.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2017/0282647 A1
Published
Oct 5, 2017
Filed
Dec 17, 2015
Class
B60C 1/0008
Document BUS 2021/0339919 A1
Published
Nov 4, 2021
Filed
May 17, 2019
Class
B65D 51/145
Claim 1
Document A
Document B
1.1(a) the sealing element comprises a polymer composition; and
This is achieved by using a ribbon-shaped strip of a thermoplastic elastomer composition having a specific shape to form the inner liner or by providing the inner liner with specific dimensions.
A · US 2017/0282647 A1 · ¶ 4
The sealing element (3, 23, 43, 63) comprises a polymer composition.
B · US 2021/0339919 A1 · abstract
1.2(b) the polymer composition comprises a first butene copolymer, wherein the butene copolymer has a melting temperature Tm above 130 °C, wherein the melting temperature Tm is determined by the second heating curve of a DSC measurement at a heating rate of 10 °C min 1.
The polymer composition comprises a butene copolymer with a melting temperature Tm, between 30° C. and 130° C. The melting temperature Tm, can be measured during a DSC measurement by means of the second heating curve at a heating rate of 10° C/min.
B · US 2021/0339919 A1 · ¶ 6

An empty cell means only that no passage was reproduced there.

Statements in these documents
However, additives that may be suitable to improve crack resistance may have detrimental effects on, e.g., air permeability, processing properties and/or cure properties of the formulations to which they are added.
A · US 2017/0282647 A1 · ¶ 5
The inventors have now found that rosin esters with a low acid number, i.e. of at most 15 mgKOH/g, can be used in inner liner formulations comprising butyl rubber, resulting in a formulation with good crack resistance properties without significantly detrimentally affecting the air permeability, processing and curing properties of the formulation.
A · US 2017/0282647 A1 · ¶ 6
One object of the invention is to provide a polymer composition that may be used as sealing element in a closure, that is manufacturable at acceptable costs and shows very low migration values.
B · US 2021/0339919 A1 · ¶ 4
The sealing element may be configured disc-shaped or ring-shaped.
B · US 2021/0339919 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0356553 A1, claim 1, first published 2026-11-20T03:38:56-05:00, https://patent.fyi/US20260356553/, SHA-256 be2e5071a6555a88e691bdc13a40810c65023977ff4650df829d57eb67fb7985
First published
Permanent addresshttps://patent.fyi/US20260356553/
Content fingerprint (SHA-256)be2e5071a6555a88e691bdc13a40810c65023977ff4650df829d57eb67fb7985