What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Transverse sampling strip

What ifWhat if the sampling region is a 10 mm by 30 mm strip across the film web?
Claim language“within a square A1”

The long axis of the strip runs across the coating direction. Three 5 μm square modulus maps centered along that axis sample the surface at evenly spaced positions.

1.1Rectangular modulus map

What ifWhat if each modulus map covers a 4 μm by 8 μm rectangle?
Claim language“square A2 with a side of 5 μm”

The atomic force microscope records a 64 by 64 array of force curves with the long axis of the map aligned with the coating direction. The rectangular footprint covers 8 μm along that direction to sample elongated surface features.

1.1Circular map with radial sampling

What ifWhat if modulus measurements are collected along concentric rings within a circular area 5 μm in diameter?
Claim language“each side of an area of square A2 with a side”

The probe collects force curves at the center and at evenly spaced points on concentric rings. The point count on each ring increases with its radius to keep the spacing between neighboring measurement locations similar across the map.

1.1Median surface modulus

What ifWhat if the median pixel modulus represents the typical stiffness of the mapped surface?
Claim language“a number average value of the elastic moduli”

The analysis sorts the 4096 pixel moduli and averages the two central readings to obtain the median. A production check compares the median with limits established from film rolls that pass package integrity and dissolution tests.

1.1Interquartile modulus spread

What ifWhat if the interquartile range measures the spread of the pixel moduli?
Claim language“a coefficient of variation of the elastic moduli”

The analysis subtracts the 25th percentile modulus from the 75th percentile modulus and reports the result in MPa. An upper limit on that difference controls the stiffness spread across the middle half of the measurements.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Water soluble packets for seed placement

A folded polyvinyl alcohol film forms a packet around a dry seed, and heat seals close its three open edges. Before folding, an atomic force microscope measures a 64 by 64 modulus grid over a 5 μm square inside a 2 cm square on one film face. The grid has a mean elastic modulus of 1 to 200 MPa and a coefficient of variation of 0.1 to 0.7. The packet is planted in soil, and irrigation water dissolves the film and exposes the seed.

Component substitution

Pullulan film with surface modulus mapping

Pullulan replaces polyvinyl alcohol as the film-forming resin. An aqueous pullulan solution containing glycerol as a plasticizer is cast onto a release liner, dried, and peeled to form a water-soluble sheet. An atomic force microscope measures the elastic modulus at 4096 sites on a 64 by 64 grid covering a 5 μm square inside a 2 cm square on one face. The arithmetic mean and the ratio of standard deviation to mean summarize the modulus distribution.

Parameter or scale variation

Wider modulus maps with finer sampling

A polyvinyl alcohol film coupon is mounted flat on a rigid support with one face exposed to an atomic force microscope. Within a 3 cm square on the exposed face, a 10 μm square is divided into 256 rows and 256 columns, giving 65,536 measurement sites at approximately 39 nm spacing. The probe records a force curve at each site, and the fitted moduli are summarized by their arithmetic mean and coefficient of variation.

Humidity stepped surface modulus mapping

A polyvinyl alcohol film coupon is mounted on a rigid support inside an atomic force microscope chamber held at 23 °C. The chamber sets relative humidity to 30%, 50%, and 70% in sequence, with a 60-minute hold before each scan. At each condition, the probe measures a 64 by 64 grid over a separate 5 μm square within the same 2 cm square on one face. All scans use the same probe and force setpoint, and the mean modulus and coefficient of variation are recorded for each humidity setting.

Combination with existing systems

Modulus mapping with thermoform packaging

A roll-fed thermoform-fill-seal machine unwinds a polyvinyl alcohol film, heats it, and draws it into pockets using vacuum. A dosing head loads dry granules into the pockets, and a sealing station bonds a second water-soluble web across their rims. An off-line atomic force microscope maps a 5 μm square at 64 by 64 sites within a 2 cm square on a flat coupon removed from each incoming roll. The machine records the coupon mean modulus and coefficient of variation with the roll identifier and the forming and sealing settings.

Automated or data-driven variant

Automated force curve fitting and screening

An atomic force microscope collects one force curve per pixel on a 64 by 64 grid over a 5 μm square within a 2 cm square on one face of a polyvinyl alcohol film. Software detects the contact point and fits a spherical indentation model using the calibrated probe radius and cantilever stiffness. The software flags curves with missing contact or excessive fit residuals and schedules a repeat at those coordinates. Once all 4096 pixels have accepted fits, it compares the arithmetic mean and coefficient of variation with the respective intervals of 1 to 200 MPa and 0.1 to 0.7.

Specific version of a part

Calibrated force curve grid

A 5 μm square inside a 2 cm square on the film surface is divided into 64 by 64 pixels. An atomic force microscope with a calibrated cantilever and a 20 nm nominal tip radius records one force curve per pixel at a fixed peak force, and a contact model converts each curve to a modulus.

Modulus statistics from pixel data

An atomic force microscope records 4096 pixel moduli on a 64 by 64 grid covering a 5 μm square within a 3 cm square on the film surface. The analysis gives every pixel equal weight, divides the population standard deviation by the arithmetic mean, and checks that the mean is 1 to 200 MPa and the resulting ratio is 0.1 to 0.7.

Cite aspatent.fyi, US 2026/0356556 A1, claim 1, first published 2026-11-20T03:38:56-05:00, https://patent.fyi/US20260356556/, SHA-256 d13301e513d859418d9907fb0dfc11e2645e1d3400dedf33f87d30d03dc14cfa
First published
Permanent addresshttps://patent.fyi/US20260356556/