Applications  /  US 2026/0356662
United States Patent Application Publication

US 2026/0356662 A1

Published
Nov 12, 2026
Filed
Jun 25, 2026
Earliest date on the face
Sep 14, 2022
Classification
C01B 3/0031
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Magnetite on porous zirconia

What ifWhat if the reactive material consists of magnetite dispersed through porous zirconia granules?
Claim language“a Fe-xSn powder blend”

Hydrogen removes oxygen from the magnetite during charging, and steam restores oxygen to the reduced iron during discharge, releasing hydrogen. The zirconia skeleton separates iron-rich domains and provides interconnected channels for gas transport.

1.1Porosity formed by sacrificial fibers

What ifWhat if sacrificial fibers form the open channels before the iron–tin material enters service?
Claim language“transient liquid-phase sintering induced swelling effect”

Iron oxide, tin oxide, and short cellulose fibers form a green compact. An air firing burns out the fibers and bonds the remaining oxide particles in the solid state, leaving channels that admit hydrogen and steam to the reactive material.

1.1Hydrogen stored by hydride formation

What ifWhat if hydrogen storage and release use reversible hydride formation?
Claim language“reversible transformations throughout redox cycling between oxidized and reduced states”

A bed of lanthanum–nickel alloy granules absorbs hydrogen under pressure and forms a metal hydride. Lowering hydrogen pressure and supplying heat releases hydrogen gas from the hydride.

1.2Tin placed in patterned films

What ifWhat if discrete tin films on porous iron sheets supply the tin, with loading set by film thickness and surface coverage?
Claim language“concentration (at. %) of tin (Sn) in the powder blend”

Masked physical vapor deposition places tin islands on the exposed ligaments of a preformed porous iron sheet. The sheet provides open channels for hydrogen and steam, while reduced tin melts during the hot reduction step and redistributes locally along the ligaments.

1.2Dilute tin on porous support

What ifWhat if the iron–tin powder contains 0.05 at. % tin and a porous ceramic maintains gas access?
Claim language“in a range of about 0.5-40 at. %”

Porous magnesium aluminate granules carry a thin coating of the dilute iron–tin powder, with tin content measured relative to iron plus tin. Hydrogen reduces the iron oxide in the coating, and steam reoxidizes the iron to release hydrogen while the ceramic maintains open transport paths.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Hydrogen buffer for glass forming

An iron–tin powder bed supplies hydrogen to an oxyhydrogen burner at a glass forming station. During periods of low burner demand, a hydrogen header feeds the heated bed to reduce its iron oxide. During forming, steam passes through the reduced bed and releases hydrogen as the iron reoxidizes. A condenser removes residual steam, and a surge vessel feeds the burner through a pressure regulator and flashback arrestor.

Component substitution

Tin dioxide as the tin feed

Tin dioxide powder replaces metallic tin powder in the initial blend with iron powder. The blend contains 5 atomic percent tin on a total iron-plus-tin basis, with oxygen excluded from the calculation. An initial treatment in dry hydrogen at 650 °C reduces the tin dioxide to metallic tin, and the outlet carries away the resulting water vapor. The transient liquid tin redistributes within the bed during activation, and subsequent hydrogen and steam exposures cycle the material between reduced and oxidized states.

Parameter or scale variation

Parallel shallow beds for increased throughput

Eight heated cartridges each hold a 4 mm layer of iron–tin powder between porous alumina retainers. Inlet and outlet manifolds connect the cartridges in parallel, and an inlet restrictor at each branch balances gas flow. The cartridges operate at 600 °C with alternating 20-minute hydrogen and steam steps and a nitrogen purge between steps. Increasing the cartridge count increases the powder inventory while retaining the same gas path length through each layer.

Axial temperature staging during hydrogen release

A tubular reactor contains two 15 mm layers of iron–tin powder separated by a porous alumina disk. Independent heaters and thermocouples maintain the steam inlet layer at 575 °C and the downstream layer at 650 °C during hydrogen release. Steam flows through both layers in series, and a downstream condenser removes water from the product gas. During charging, both layers operate at 650 °C, and dry hydrogen enters from the discharge outlet so that the gas flows through the layers in reverse order.

Combination with existing systems

Thermal integration with an electrolyzer

A solid oxide steam electrolyzer supplies hydrogen to a separate heated vessel containing the iron–tin powder bed. During charging, a condenser removes residual water from the electrolyzer hydrogen stream, and a recuperator reheats the dried hydrogen before it enters the vessel. A separate heat exchanger transfers heat from the electrolyzer exhaust to the steam feed used during discharge. The discharge outlet passes through a condenser and delivers hydrogen to a gas header.

Automated or data-driven variant

Gas measurements control cycle transitions

A programmable controller receives outlet hydrogen and water vapor measurements from a heated sample line and operates the hydrogen, steam and nitrogen valves. During reduction, the controller tracks the outlet water generation rate, and during steam oxidation it tracks the outlet hydrogen generation rate. Each step ends when its generation rate stays below 5 percent of the peak measured during that step for 60 seconds. The controller closes the active feed valve and runs a nitrogen purge before it opens the next feed valve.

Specific version of a part

Elemental iron and tin powders

A blend combines 20–45 µm iron particles with 5–15 µm tin particles at 5 at. % tin. During hydrogen reduction at 550 °C, metallic tin melts and redistributes at iron particle contacts, leaving voids at former tin sites as iron–tin intermetallic phases grow.

Tin regenerated from oxide powder

A blend of magnetite and tin dioxide contains 10 at. % tin on an iron-plus-tin basis. Dry hydrogen at 650 °C reduces the oxides and produces transient liquid tin, while the subsequent steam exposure reoxidizes the reduced material and releases hydrogen.

Two atomic percent tin blend

The blend contains 2 tin atoms per 100 iron and tin atoms combined. This composition corresponds to about 4.16 mass % tin in a blend prepared from elemental iron and tin powders.

Fifteen atomic percent tin blend

The blend contains 15 tin atoms per 100 iron and tin atoms combined. Each 100 g batch of elemental powder contains about 27.28 g of tin and 72.72 g of iron.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2015/0206615 A1
Published
Jul 23, 2015
Filed
Jul 31, 2013
Class
H01B 1/08
Document BUS 2020/0303612 A1
Published
Sep 24, 2020
Filed
Mar 17, 2017
Class
H01L 35/14
Claim 1
Document A
Document B
1.1a Fe-xSn powder blend capable of exhibiting a transient liquid-phase sintering induced swelling effect and undergoing reversible transformations throughout redox cycling between oxidized and reduced states
In the second sintering step S5, the tin powder, the magnesium powder, and the like are dissolved, and hence a liquid phase is formed. Accordingly, by the liquid phase sintering, the second layer 15 directly joined to the first layer 14 is formed.
B · US 2020/0303612 A1 · ¶ 102
1.2wherein x represents a concentration (at. %) of tin (Sn) in the powder blend and is in a range of about 0.5-40 at. %.
The first sintered oxide of the present invention is required to have a tin content of 0.001 to 0.15 in terms of the atomic ratio of Sn/(In+Sn).
A · US 2015/0206615 A1 · ¶ 46

An empty cell means only that no passage was reproduced there.

Statements in these documents
The present invention relates to a sintered oxide and a tablet obtained by processing the same, and more specifically, to a tablet for ion plating which allows high speed formations of transparent conductive films suitable for solar cells and allows continuous film formation without causing cracks, breakage or splashing, and to a sintered oxide used for obtaining the tablet.
A · US 2015/0206615 A1 · ¶ 1
When tablets for ion plating have excessively high or low density, sintered oxides may easily have cracks or breakage and be damaged.
A · US 2015/0206615 A1 · ¶ 8
The present invention relates to a magnesium-based thermoelectric conversion material having excellent thermoelectric conversion efficiency, a magnesium-based thermoelectric conversion element, a thermoelectric conversion device, and a method for manufacturing a magnesium-based thermoelectric conversion material.
B · US 2020/0303612 A1 · ¶ 1
Consequently, unfortunately, even though the thermoelectric conversion element is formed using a material with high ZT, because the thermoelectric conversion efficiency of the low-temperature side is low, the amount of power generated by the whole thermoelectric conversion element is not necessarily high.
B · US 2020/0303612 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0356662 A1, claim 1, first published 2026-11-20T04:54:27-05:00, https://patent.fyi/US20260356662/, SHA-256 422b319177f000ea3509bc4b7dd2377d79136b45edcbc4fc83561dbc58dfaec7
First published
Permanent addresshttps://patent.fyi/US20260356662/
Content fingerprint (SHA-256)422b319177f000ea3509bc4b7dd2377d79136b45edcbc4fc83561dbc58dfaec7