patent.fyi
Applications  /  US 2026/0356672
United States Patent Application Publication

US 2026/0356672 A1

Published
Nov 12, 2026
Filed
Nov 22, 2023
Earliest date on the face
Dec 5, 2022
Classification
C01B 25/084
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.2Reactor assembly around the charge

What ifWhat if the reactor shell is assembled around a prepositioned charge?
Claim language“filling a reactor with the homogeneous mixture of reactants”

The blended powder is compacted into a self-supporting pellet and placed on an insulating pedestal on the bottom flange. A tubular shell is lowered over the pellet and joined to the flange.

1.4Uncovered charge in a heated chamber

What ifWhat if the top of the charge faces an open headspace inside the sealed reactor?
Claim language“an upper layer of chemically inert thermal insulator”

The base and side insulation surround a shallow compacted charge whose upper face remains exposed. An external furnace heats the upper chamber wall, reducing radiative heat loss from the charge during the reaction and subsequent hold.

1.5Welded tubular neck closure

What ifWhat if the reactor is sealed by welding its integral tubular neck shut?
Claim language“sealing the reactor with a lid”

The vessel is evacuated and backfilled with argon through the neck. The neck is flattened and welded across the flattened section to form a gas-tight closure.

1.6Laser ignition through a window

What ifWhat if an external laser ignites the charge through a sealed optical window?
Claim language“the heating element, in contact with the mixture”

A focused beam passes through a window at the cool end of a recessed optical port and heats a small spot on an exposed edge of the charge. The beam is switched off once the exothermic front moves away from the ignition spot.

1.10Stoichiometric magnesium charge

What ifWhat if the magnesium dose matches the amount required to bind the precursor oxygen?
Claim language“the magnesium being in excess”

For B12P2O23 feed, the batch contains 23 moles of magnesium per mole of precursor, with magnesium oxide as the oxygen-bearing product. Fine magnesium is dispersed throughout the precursor powder, and a sealed chamber with a small headspace limits magnesium transport away from the charge.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Powder production for abrasive ceramics

A ceramic tooling line uses a sealed, insulated reactor with a contact heater to produce boron subphosphide by a self-propagating reaction. After leaching, rinsing, and drying, an air classifier separates the powder by particle size. The selected fraction feeds a ceramic mixing station, where it is dispersed in a vitrifiable binder for abrasive compacts.

Component substitution

Optical ignition through a sealed window

An external laser replaces the internal contact heater. A pressure-rated optical window in the lid aligns with a refractory sight tube that passes through the upper insulation and terminates at the powder surface. A shutter admits the focused beam to heat a small region of the bed until the reaction front forms, then closes while the reactor remains sealed.

Removable boron nitride insulation cassette

Machined hot-pressed hexagonal boron nitride panels replace the loose insulating material around the powder. A recessed base locates the side panels, and a matching top panel seats over the side panels and the charge. An aperture in one end panel locates the heater tip against the powder, and lifting the cooled cassette out of the vessel gives access to the reacted solids.

Parameter or scale variation

Four horizontal reaction cells per vessel

A common sealed vessel houses four independently insulated reaction cells in a two-by-two array. Each cell holds a powder bed 60 mm long, 25 mm wide, and 15 mm deep, with a contact heater at one end. The controller fires one heater per cycle, and the vessel returns to its preset starting temperature before the next cell is fired.

Combination with existing systems

Integrated filtration and batch washing

An agitated filter dryer receives the cooled reaction product through an enclosed solids transfer chute. The agitator suspends the solids in the leach liquid, and a porous bottom plate retains the solids while the spent liquid drains. The same vessel reslurries the retained solids for additional leaching, rinses them with water, and dries them under vacuum.

Automated or data-driven variant

Sensor tracking of reaction front speed

Three sheathed thermocouples sit in blind bores in the side insulation, with their tips at known distances from the ignition point and close to the powder bed. A data acquisition unit records the temperature histories and detects front arrival from the peak rate of temperature rise at each position. Software divides the spacing between adjacent sensors by the difference in arrival times and flags batches with a missing arrival or a speed outside a configured interval.

Specific version of a part

Two-stage phosphate powder blending

Magnesium and boron phosphate powders are screened separately under argon to break up agglomerates. A small portion of the phosphate is blended with the magnesium first, then the remaining phosphate is added and the batch is tumbled to distribute the magnesium throughout.

Boron nitride base and liner

A hot-pressed hexagonal boron nitride disk covers the reactor floor, and a matching sleeve lines the cylindrical inner wall. The sleeve seats on the disk and keeps the powder charge separated from the metal wall.

Axial propagation through a pellet

Ignition starts at one end of a cylindrical powder pellet, and the exothermic front travels along its axis. A two-color pyrometer views the passing front through an optical port to verify that its temperature exceeds 1500 °C.

Pressed charge with radial restraint

A binder-free powder compact fits closely inside a rigid ceramic sleeve. The sleeve limits radial expansion, and the compact maintains particle contacts as the reaction front advances.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 7,939,044 B2
Published
May 10, 2011
Filed
Feb 11, 2008
Class
C01B 31/36
Document BUS 2017/0203965 A1
Published
Jul 20, 2017
Filed
Jan 19, 2016
Class
C01B 25/084
Claim 1
Document A
Document B
1.1a step of homogeneous mixing of reactants, in the form of powders, comprising at least: an alkaline-earth metal such as magnesium or calcium, and a compound comprising boron and phosphorus, or a compound comprising boron and a compound comprising phosphorus, such as boron phosphate BPO4 or B12P2O23
For example, according to the invention, in order to produce 1 kg of the final silicone carbide powder, one needs approximately 735-770 g, preferably about 752.5 g of Si, approximately 240-270 g, preferably about 255 g of C; approximately 97-194 g, preferably about 120 g, of activated additive such as the aforementioned polytetrafluoroethylene. This stage also includes thorough mixing of the components for obtaining a homogeneous reactant mixture, which is known as a green mixture.
A · US 7,939,044 B2 · ¶ 37
The improved high yield synthesis of boron phosphide (BP) as disclosed herein starts with thoroughly mixing fine boron phosphate (BPO4) and magnesium metal particles, in a mass ratio of 1.0+/−0.5 but most preferably 1.0+/−0.2, and then packed, with or without added pressure into a column of any shape and length.
B · US 2017/0203965 A1 · ¶ 21
1.2a step of filling a reactor with the homogeneous mixture of reactants,
A method of manufacturing a silicon carbide powder with submicron size of powder particles comprising: preparing a homogeneous reactant mixture comprising at least a carbon source, silicon source, and an activated additive for initiating an exothermic self-propagating reaction in the aforementioned homogeneous reactant mixture when this mixture is locally preheated to a temperature sufficient to initiate the aforementioned exothermic self-propagating reaction; loading the hom
A · US 7,939,044 B2 · claim 1
1.3the reactor comprising at least: a heating element, a layer or base of thermal insulator on an inner wall of the bottom of the reactor and a side insulating layer on one or more inner side walls, the thermal insulator being chemically inert and intended to surround the homogeneous mixture of reactants during the reaction and to separate it from the walls of the closed reactor,
The sealable reaction chamber can be lined with a graphite brick for protecting the reactor walls from interaction with the reagents and can be provided with a water cooling jacket. The reaction chamber is further provided with an igniter device, e.g., in the form of a tungsten wire, for local preheating and initiation of the reaction.
A · US 7,939,044 B2 · ¶ 20
1.4a step of covering the top of the homogeneous mixture of reactants, as well as the side insulating layer, with an upper layer of chemically inert thermal insulator, enabling the homogeneous mixture of reactants to be confined in the reactor, this mixture being completely surrounded by the base insulating layer, the side thermal insulating layer, and the upper thermal insulating layer,
1.5a step of hermetically sealing the reactor with a lid,
Prior to initial local heating, the reaction chamber is sealed, evacuated, and purged with inert gas for several times and then filled with inert gas to a desired pressure.
A · US 7,939,044 B2 · ¶ 20
Typically, a precursor mixture is heated in a sealed tube to a high temperature or dropped directly into a superheated reaction zone in excess of 1000° C.
B · US 2017/0203965 A1 · ¶ 6
1.6a step of initiating, in the closed reactor, a high-temperature exothermic reaction in the homogeneous mixture of reactants, by triggering the heating element, in contact with the mixture,
The reaction chamber is further provided with an igniter device, e.g., in the form of a tungsten wire, for local preheating and initiation of the reaction. Prior to initial local heating, the reaction chamber is sealed, evacuated, and purged with inert gas for several times and then filled with inert gas to a desired pressure.
A · US 7,939,044 B2 · ¶ 20
1.7a step of high-temperature exothermic reaction, at a temperature higher than 1500 °C, which self-propagates throughout the reactant mixture of the reactor to obtain the boron subphosphide B12P2,
After the powder is locally heated by the igniter, the power is turned off, and the reaction propagates through the reaction mixture under the effect of the exothermic heat developed after initiation of the reaction (Step 3).
A · US 7,939,044 B2 · ¶ 21
The pellet was then heated with the flame of a gas burner to initiate the reaction, but the product of the reaction, however, was found to contain a significant amount (up to 30%) of the impurity boron subphosphide (B12P2). It was suggested that the impurity arose from immediate decomposition of the as-synthesized BP microcrystals due to an unexpected high reaction temperature of over 1227° C.
B · US 2017/0203965 A1 · ¶ 7
1.8the insulating material allowing the residual heat to be retained for longer in the homogeneous mixture of reactants, to promote self-purification phenomena and favor the synthesis of boron subphosphide B12P2 over the synthesis of boron phosphide, the mixture of reactants being said to be confined in the reactor,
Such rapid and efficient conductive heat transfer, the heat originating from both the ignition source and the synthesis reaction, can lead to high reaction temperatures and the production of reaction products that are not desired, including impurities.
B · US 2017/0203965 A1 · ¶ 19
1.9the reactant powder thus has a low capacity for expansion, so that the various precursors remain in contact with one another as the reaction propagates,
SHS synthesis of pellets as reported by Mukhanov was prepared by pressing the reactant powders at high pressures. These pellets are dense, relatively non-porous, and highly thermally conductive, especially when such pellets contain thermally conductive materials such as magnesium.
B · US 2017/0203965 A1 · ¶ 19
1.10the magnesium being in excess in the reactant mixture to enhance oxide reduction,
The reaction, in which boron phosphate functions as an oxidizer for the oxidization of magnesium to magnesium oxide (MgO) while it is reduced to BP, is highly exothermic. Mukhanov described mixing fine boron phosphate and magnesium powders at a 1.0/4.1 molar ratio, and pressing the mixture at an extraordinarily high pressure of 0.6 GPa into a pellet 40 mm in diameter and 20 mm in length.
B · US 2017/0203965 A1 · ¶ 7
1.11a step of extracting the product of the exothermic reaction, the product extracted from the reactor being subjected to washing that comprises leaching one or more times, followed by rinsing, in order to obtain the boron subphosphide B12P2.
The product from the combustion is then continuously scrubbed mechanically into a downsteam recovery vessel where the BP is separated and recovered.
B · US 2017/0203965 A1 · ¶ 22

An empty cell means only that no passage was reproduced there.

Statements in these documents
It is well recognized that under such conditions (i.e. high temperatures and long duration of synthesis) it is essentially impossible to produce pure silicon carbide powder with a particle size of less than 5 micron.
A · US 7,939,044 B2 · ¶ 5
The present invention relates to synthesis of materials using combustion in powder metallurgy and, more specifically, to a chemically activated combustion synthesis (CACS) of pure sub-micron powders of silicon carbide (SiC) used for production of abrasives, advance ceramics, composites, etc.
A · US 7,939,044 B2 · ¶ 2
Synthesis of boron phosphide typically requires use of toxic components or complex processes that are unsafe and expensive.
B · US 2017/0203965 A1 · ¶ 6
More specifically, this invention relates to high yield synthesis of boron phosphide in a self-propagating high-temperature synthesis reaction by combining boron phosphate and magnesium metal without the need for diluents into a homogenous mixture, loosely packing the mixture, and then igniting the mixture with a minimum amount of energy that can be supplied by a pyrotechnic igniter.
B · US 2017/0203965 A1 · ¶ 2
Cite aspatent.fyi, US 2026/0356672 A1, claim 1, first published 2026-11-20T05:32:13-05:00, https://patent.fyi/US20260356672/, SHA-256 ab22aa3b33933d2c24abe58f77a1f7a426f785fa306e8861e1d1b7f7430abe7d
First published
Permanent addresshttps://patent.fyi/US20260356672/
Content fingerprint (SHA-256)ab22aa3b33933d2c24abe58f77a1f7a426f785fa306e8861e1d1b7f7430abe7d
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi