Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Mixed oxide precursor
What ifWhat if the titanium and dopant enter the process as a coprecipitated hydrous oxide?
Claim language“T-Ti(E) intermetallic compounds with E elements in solid solution”
Mix aqueous titanium and zirconium oxychloride solutions at a zirconium-to-titanium molar ratio of 0.05, then add ammonium hydroxide to coprecipitate the hydrous oxides. Wash out chloride and react the wet precipitate with barium hydroxide under hydrothermal conditions to crystallize zirconium-doped barium titanate.
1.2Acid leaching and carbonate firing
What ifWhat if an acidic leach removes zinc and a solid carbonate supplies sodium for titanate formation?
Claim language“an alkaline solution mainly composed of NaOH/KOH”
Leach a powdered zinc-titanium alloy containing zirconium with dilute hydrochloric acid to dissolve zinc, then wash the titanium-rich residue. Oxidize the residue in air and fire the resulting oxide with sodium carbonate to form sodium titanate.
1.3Electrochemical proton exchange
What ifWhat if a membrane cell supplies protons from water for sodium exchange?
Claim language“with a dilute acid”
Circulate the sodium titanate slurry through a compartment bounded by a bipolar membrane and a cation-exchange membrane. Under direct current, water dissociation at the bipolar membrane supplies protons to the slurry, and displaced sodium ions migrate through the cation-exchange membrane into an adjacent compartment.
1.4Dense equiaxed titanic acid particles
What ifWhat if the titanic acid intermediate consists of dense equiaxed nanoparticles?
Exchange sodium from dense, equiaxed sodium titanate nanoparticles using dilute acid at room temperature. Wash the resulting protonated particles and keep them dispersed in water for reaction with barium hydroxide.
1.5Crystallization from a mixed solution
What ifWhat if barium titanate crystallizes from dissolved precursors?
Mix soluble titanium and zirconium lactate complexes with barium hydroxide and heat the mixture in a sealed aqueous reactor. Hydrolysis releases titanium and zirconium species, which react with dissolved barium to nucleate and grow zirconium-doped barium titanate particles.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Radiopaque filler for polymer inspection
The alloy dealloying and barium conversion stages produce near-spherical doped barium titanate powder. A twin-screw extruder disperses the dried powder into a polyethylene masterbatch, which a second extrusion pass dilutes into marker strips for molded parts. An X-ray transmission station locates the strips through the surrounding polymer by measuring the greater attenuation of the barium-containing regions.
Component substitution
Lithium acetate feed for titanate conversion
Aqueous lithium acetate replaces lithium hydroxide as the lithium source for conversion of the proton-exchanged titanate intermediate. The intermediate and lithium acetate solution enter a stirred pressure vessel, with the lithium feed set from the measured titanium content and the target lithium titanate composition. The heated slurry takes up lithium, and the recovered solids are rinsed to remove soluble acetate. A controlled calcination step completes crystallization, and powder diffraction and electron microscopy check the resulting phase and particle shape.
Parameter or scale variation
Parallel conversion in small pressure vessels
A single washed batch of doped titanate intermediate is dispersed in the barium-containing conversion liquor and divided among eight 50 mL rated pressure vessels at 25 mL of slurry per vessel. The vessels occupy one heated block and run at the same temperature and dwell time. The vessels cool together, and the slurries are pooled before filtration and washing.
Combination with existing systems
Membrane washing between reaction stages
A crossflow ceramic ultrafiltration loop connects to the cooled alkaline dealloying slurry tank. The membrane retains the titanate particles while dissolved alkali and soluble aluminum or zinc species leave in the permeate. Water enters the tank at the permeate withdrawal rate, and the washed retentate transfers to the barium or lithium conversion vessel when the permeate conductivity reaches the selected set point.
Automated or data-driven variant
Hydrogen monitoring for dealloying endpoints
A condenser and demister connect the alkaline dealloying vessel to a vent line fitted with a gas flowmeter and a hydrogen analyzer. A controller calculates the hydrogen evolution rate from the two signals and integrates it over the batch. When the rate remains below a calibrated threshold for a set interval and the cumulative hydrogen reaches the range established for that alloy feed, the controller stops heating and starts cooling. Residual aluminum or zinc measurements from qualification batches establish the endpoint settings.
Image analysis for conversion dwell control
Pressure-rated sampling hardware withdraws slurry from the conversion vessel at fixed intervals and delivers quenched aliquots to an automated electron microscopy sample preparation station. Image analysis segments individual particles and calculates projected circularity as four pi times the particle area divided by the squared perimeter. A controller ends the conversion dwell once the fraction of particles above the selected circularity threshold meets the batch target in two consecutive samples.
Specific version of a part
Zirconium in aluminum titanide
Melt aluminum, titanium, and zirconium under argon and anneal the solidified alloy to form an aluminum titanide phase with zirconium in solid solution. Measure the zirconium-to-titanium molar ratio in that phase by electron probe microanalysis and target 0.05.
Sodium hydroxide conversion to nanosheets
React powdered aluminum titanide containing zirconium with aqueous sodium hydroxide in a stirred reactor with a hydrogen outlet. Aluminum dissolves as aluminate, hydrogen evolves, and the titanium-rich solid converts to layered sodium titanate nanosheets.
Hydrochloric acid exchange of nanosheets
Stir zirconium-doped sodium titanate nanosheets in 0.1 mol/L hydrochloric acid at room temperature to replace interlayer sodium with protons. Filter the protonated nanosheets and wash them with deionized water to remove dissolved sodium and chloride.
Hydrothermal conversion with barium hydroxide
Disperse zirconium-doped sodium titanate nanosheets in aqueous barium hydroxide and hold the suspension in a sealed reactor at 180 °C for 12 hours under autogenous pressure. Barium uptake and sodium release accompany reconstruction of the nanosheets into near-spherical zirconium-doped barium titanate nanoparticles.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1at step 1, preparing an initial alloy including T elements, Ti elements, and E elements; the phase composition of the initial alloy includes T-Ti(E) intermetallic compounds with E elements in solid solution or T-Ti-E intermetallic compounds containing E elements; wherein the molar ratio of E elements to Ti elements in the T-Ti(E) or T-Ti-E intermetallic compounds is 0≤CE/CTi≤0.30; the T elements include at least one of Al and Zn, and the E elements include at least one of Zr, Hf, Cr, V, Nb, Ta, W, Mo, Mn, Fe, Ni, Co, Sn, Pb, Bi, B, Be, Au, Pt, Pd, Ru, Rh, Re, Os, Ir, Ag, Cu, and RE, wherein RE includes at least one of rare earth elements;
No. 4,879,092 to Huang discloses a titanium aluminide intermetallic composition having an approximate formula of Ti46-50Al46-50Cr2Nb2, or nominally about Ti-48 Al-2 Cr-2 Nb.
A · US 2013/0248061 A1 · ¶ 3
To synthesize hierarchical porous CuTi catalyst, an Al—CuTi precursor alloy was first prepared by arc melting pure Al (Alfa Aesar, 99.99%), Cu (Alfa Aesar, 99.999%) and Ti (Alfa Aesar, 99.99%) at an atomic ratio of 80:19:1 Al:Cu:Ti under an argon atmosphere.
B · US 9,994,961 B2 · ¶ 73
1.2at step 2: the initial alloy is subjected to hydrogen evolution and T removal reaction with an alkaline solution mainly composed of NaOH/KOH to obtain intermediate powder products; the intermediate powder product mainly includes at least one of the following: nano sodium/potassium titanate thin-film powder with in-situ doped E element, irregular nanoporous sodium/potassium titanate powder with in-situ doped E element, nano sodium/potassium titanate tubes (or/and rods) with in-situ doped E element;
In a following step, the pristine electrodes were immersed in a 6 M KOH solution to remove Al, thereby forming hierarchical porous CuTi (np-CuTi).
B · US 9,994,961 B2 · ¶ 73
1.3alternatively, reacting the intermediate powder product composed of nano sodium/potassium titanate with in-situ doped E element with a dilute acid to obtain a hydrogen-ion-exchanged titanic acid intermediate powder product with in-situ doped E element, which mainly includes at least one of the following: nano titanic acid thin-film powder with in-situ doped E element;
1.4irregular nanoporous titanic acid powder with in-situ doped E element, nano titanic acid tubes (or/and rods) with in-situ doped E element;
1.5at step 3: reacting the intermediate powder product obtained in step 2 with a barium/lithium source material containing Ba2+/Li+ at a specific temperature, pressure, and medium atmosphere for a period of time, causing cation displacement reaction and “spheroidization” morphology change of such non spherical intermediate powder product, to obtain spherical or near-spherical barium/lithium nanoparticle powder product with in-situ doped E element.
An empty cell means only that no passage was reproduced there.
Statements in these documents
In view of the above, a method is needed that is capable of processing TiAl intermetallics, including but not limited to net-shape geometries of the 48-2-2 alloy, to yield a duplex microstructure containing equiaxed and lamellar morphologies.
A · US 2013/0248061 A1 · ¶ 7
The present invention provides methods capable of processing compositions containing titanium and aluminum, and especially titanium aluminide intermetallic compositions (TiAl intermetallics) based on the TiAl (gamma) intermetallic compound, to yield desirable microstructures.
A · US 2013/0248061 A1 · ¶ 8
Regardless of acidic or basic conditions, Pt, along with its alloys, is the benchmark electrocatalyst that requires very small overpotentials to drive the reaction, while the scarcity and high cost of Pt hinder its large-scale use for H2 production.
B · US 9,994,961 B2 · ¶ 3
In some aspects, the invention provides a water electrolyzer or a hydrogen fuel cell employing the foregoing alloy as a HER or HOR electrocatalyst, respectively.
B · US 9,994,961 B2 · ¶ 7
Cite aspatent.fyi, US 2026/0356688 A1, claim 1, first published 2026-11-20T05:32:13-05:00, https://patent.fyi/US20260356688/, SHA-256 32d03e5bf38d6c264cad53120128e62a1ef63006f7151e7becad1a02b11c7ad7