Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Manganese below five percent
What ifWhat if the pigment contained 3.0% MnO by weight?
Claim language“5.0% to 40.0% by weight”
Coprecipitation of manganese and iron salts produces a mixed hydroxide precursor with a low manganese fraction. Oxygen-controlled heat treatment forms an iron-rich spinel in which mixed-valence iron contributes to visible-light absorption.
1.1Lower phosphate surface loading
What ifWhat if the finished pigment contained 0.5% phosphate by weight?
Claim language“1.5% to 2.0% by weight”
A metered orthophosphate dose adsorbs onto the ferrite surface in an aqueous slurry. The adsorbed phosphate changes the surface charge, while bead milling breaks up agglomerates before the slurry enters the coating formulation.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Black contrast medium for crack inspection
Disperse manganese ferrite black pigment in water with a wetting agent and a water-soluble binder. Apply a thin coat to a cleaned, light-colored, nonporous ceramic surface and wipe the surface with a damp pad. Pigment retained in surface-breaking cracks produces dark lines for inspection under diffuse white light.
Component substitution
Ammonium phosphate as the phosphate source
Use diammonium hydrogen phosphate in place of sodium phosphate as the phosphate source. Dissolve it in water and spray the solution onto a blended iron oxide and manganese carbonate feed while mixing, with potassium carbonate supplied separately. Dry the mixture and calcine it in an oxygen-containing atmosphere to form manganese ferrite. Adjust the phosphate dose using the measured phosphate content of the fired pigment.
Parameter or scale variation
Small batch firing in shallow trays
Spread the dried iron, manganese, and phosphate precursor blend in alumina trays at a bed depth of 5 to 10 mm. Hold the trays at 750 °C for 60 minutes after a thermocouple in a representative powder bed reaches the setpoint. Cool the trays in air, deagglomerate the fired powder, and measure its phosphate content and B 1/9 blending ratio.
Combination with existing systems
Pigment dosing in a continuous extruder
Install a loss-in-weight pigment feeder above a downstream side feeder on a co-rotating twin-screw extruder. Melt the carrier polymer upstream, meter manganese ferrite black pigment into the melt, and disperse it with kneading blocks. Pass the filled melt through a strand die, cool the strands, and pelletize them to produce a color concentrate.
Spray dried granules for pigment feeding
Disperse milled manganese ferrite black pigment in water with a dispersant and a water-soluble binder, then pump the slurry through a two-fluid nozzle into a spray dryer. Recover the dried granules in a cyclone and screen them before feeding them into a batch mixer. The granules flow through the feeder and break apart under shear during wet mixing.
Automated or data-driven variant
Automated shade depth measurement by reflectance
Use a gravimetric dispenser to prepare a series of blends from each pigment lot and a white reference pigment in a common binder. Mix each blend for a fixed time, apply it at a fixed wet-film thickness, and measure the dried film with a reflectance spectrophotometer. Software interpolates between blends that bracket the reference depth of shade and records the corresponding B 1/9 blending ratio with the lot identifier.
Specific version of a part
Reflectance of a black drawdown
A clear binder carries the pigment at a fixed pigment volume concentration, and an applicator lays down a film thick enough to hide the substrate. A spectrophotometer measures visible reflectance from the dried film, and lower luminous reflectance indicates a darker masstone.
Iron-rich manganese ferrite
A manganese-poor feed and oxygen-controlled heat treatment produce a black spinel with 12.0% MnO by weight in the finished dry pigment. Wet milling disperses the product, which contains 1.8% phosphate by weight and has a B 1/9 blending ratio greater than −12.0.
Tint testing by bracketing
A black ferrite powder containing 18.0% MnO and 1.9% phosphate by weight disperses into a white tint base at several weighed proportions. Dried drawdowns bracket the B 1/9 depth of shade, and interpolation gives the blending ratio for comparison with the threshold of −12.0.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1Manganese ferrite black pigments having a content of MnO of 5.0% to 40.0% by weight and a content of phosphate of 1.5% to 2.0% by weight, that have a blending ratio for the depth of shade value B 1/9 in accordance with DIN 53235 Part 1 and 2 of >−12.0.
The reduction ratio RR was determined to DIN 53235-1 by using the FIAF method to match the depth of shade of the specimen to be tested to ⅓ of standard depth of shade.
A · US 8,026,361 B2 · ¶ 84
Further the pigment may be a manganese ferrite black spinel, Mn3Cu2FeO8.
B · US 2013/0064981 A1 · abstract
An empty cell means only that no passage was reproduced there.
Statements in these documents
The invention further relates to the preparation of the isoindoline pigments and to their use for the coloring of high-molecular-weight organic materials of natural and synthetic origin, and also to plastics colored with the isoindoline pigments.
A · US 8,026,361 B2 · ¶ 4
Their performance in the ease-of-dispersion test makes them unsuitable for direct use in plastics, and instead they first have to be converted into preparations in a complicated manner.
A · US 8,026,361 B2 · ¶ 6
Many of the known coating types do not, however, comply with the above requirements such as the requirement with regard to temperature and corrosion.
B · US 2013/0064981 A1 · ¶ 15
With the present invention is provided a cost effective method for making an absorber coating for solar heating, as well as a coating as such which is made according to the method.
B · US 2013/0064981 A1 · ¶ 18
Cite aspatent.fyi, US 2026/0356689 A1, claim 1, first published 2026-11-20T05:32:13-05:00, https://patent.fyi/US20260356689/, SHA-256 235a795dd16fe604e618b1f3e8f86adf69d6b0b072ec0d107866b9ce23c1d4c0