patent.fyi
Applications  /  US 2026/0356693
United States Patent Application Publication

US 2026/0356693 A1

Published
Nov 12, 2026
Filed
Nov 24, 2023
Earliest date on the face
Nov 29, 2022
Classification
C01G 53/84
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Sulfur and carbon feedstock

What ifWhat if the precursor contains elemental sulfur and porous carbon and supplies sulfur for a lithium–sulfur cathode?
Claim language“containing a transition metal”

Heat a mixture of elemental sulfur and mesoporous carbon to about 155 °C under nitrogen so molten sulfur infiltrates the pores. The carbon provides electronic conduction, and the sulfur converts to lithium sulfide during discharge.

1.1Larger hydroxide crystal domains

What ifWhat if the precursor has a coherent domain size of 35 to 50 nm normal to the (001) planes?
Claim language“20 nm or less”

Precipitate a mixed nickel, manganese, and cobalt hydroxide from aqueous metal salts, then age the slurry until the (001) diffraction width corresponds to the target domain size. Wash and dry the hydroxide, blend it with lithium hydroxide, and calcine the blend in oxygen to form a layered oxide.

1.1Amorphous mixed metal gel

What ifWhat if the precursor is an amorphous citrate gel with no crystal grains?
Claim language“having a crystal grain size”

Complex dissolved lithium, nickel, manganese, and cobalt ions with citric acid and concentrate the solution into an amorphous gel. Heat the gel in air to remove the organic material, then calcine the residue in oxygen to crystallize the layered oxide.

1.1Electron microscopy fringe measurement

What ifWhat if the precursor domain size is determined from lattice images acquired by transmission electron microscopy?
Claim language“as measured by XRD”

Index the (001) lattice fringes in high-resolution images and measure contiguous fringe runs in the direction normal to the planes. Sample multiple particles and use the resulting length distribution to check the hydroxide batch before lithiation.

1.1Neutron diffraction domain measurement

What ifWhat if neutron powder diffraction provides the precursor domain-size measurement?
Claim language“as measured by XRD”

Collect a neutron powder pattern and fit indexed basal reflections with an anisotropic line-broadening model. Use an instrument resolution reference and refine strain separately to estimate the coherent domain length normal to the basal planes.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Nickel hydroxide for alkaline electrolysis

Coprecipitate nickel and iron hydroxides from aqueous metal salts with sodium hydroxide to form a layered nickel–iron hydroxide powder. Use powder X-ray diffraction to select batches with a coherent domain size of 20 nm or less normal to the (001) planes. Disperse the powder in a suspension containing an alkaline-stable binder and coat it onto porous nickel foam. Use the coated foam as the oxygen-evolving anode in an alkaline water electrolyzer.

Component substitution

Cobalt replaces nickel in hydroxide

Use cobalt sulfate as the transition-metal feed for a cobalt hydroxide precursor. Precipitate layered cobalt hydroxide from the aqueous feed with sodium hydroxide under a nitrogen blanket and limit slurry aging to restrict crystal growth. Verify the hydroxide phase and a coherent domain size of 20 nm or less normal to the (001) planes by powder X-ray diffraction. Mix the dried precursor with lithium carbonate and calcine it in air to form lithium cobalt oxide.

Parameter or scale variation

Micrometer granules with smaller domains

Precipitate a layered nickel–manganese–cobalt hydroxide and adjust the precipitation and aging conditions to target a coherent domain size of 8 to 12 nm normal to the (001) planes. Wash the solids and spray-dry the slurry to form secondary granules with a median diameter of 6 to 10 µm. Measure the granule diameter by laser diffraction and verify the domain size in the dried powder by X-ray diffraction with an instrumental broadening correction.

Combination with existing systems

Continuous lithiation in a roller kiln

Feed a layered transition-metal hydroxide with a (001) coherent domain size of 20 nm or less and lithium hydroxide monohydrate into a continuous powder mixer using separate loss-in-weight feeders. Set the feed rates from the precursor metal assay and the target lithium-to-metal molar ratio. Dispense the blend into ceramic trays and convey them through a roller-hearth kiln with independently controlled temperature zones and an oxygen supply. Heat the blend through dehydration and lithiation, then cool the resulting layered oxide before unloading the trays.

Countercurrent washing with membrane filtration

Pass the precipitated layered transition-metal hydroxide through two crossflow ceramic membrane stages that retain the suspended particles. Add deionized water to the second stage and return its permeate to the first stage so that wash water flows countercurrent to the solids. Monitor first-stage permeate conductivity to control the wash water feed and concentrate the second-stage retentate for drying. Verify a coherent domain size of 20 nm or less normal to the (001) planes in the dried precursor by powder X-ray diffraction.

Automated or data-driven variant

Diffraction feedback for slurry aging

Equip a precipitation line with a stirred aging tank and a sampler that withdraws slurry at fixed intervals. Filter, rinse, and dry each sample, then fit its (001) diffraction peak with an automated powder diffractometer. Calculate the coherent domain size from the fitted width after correcting for instrumental broadening. Use the size trend and the tank residence time to adjust the slurry discharge rate, and route powder above the 20 nm limit to a separate collection bin.

Specific version of a part

Nickel rich ternary hydroxide

Coprecipitate nickel, manganese, and cobalt hydroxide at an 80:10:10 metal molar ratio using sodium hydroxide and aqueous ammonia. Control slurry residence time to obtain a coherent domain size of 12 to 18 nm normal to the (001) planes, as determined by X-ray diffraction line broadening.

Equal metal ternary hydroxide

Feed nickel, manganese, and cobalt sulfates in equal molar proportions into a stirred alkaline reactor under nitrogen. Wash and dry the mixed hydroxide and determine its (001) coherent domain size from the instrument-corrected X-ray diffraction peak width using a 20 nm upper limit.

Binary nickel cobalt hydroxide

Precipitate a layered hydroxide from a 90:10 nickel-to-cobalt molar feed at approximately pH 11 using sodium hydroxide and aqueous ammonia. Adjust precipitation and aging conditions to obtain a coherent domain size of 15 to 20 nm normal to the (001) planes, as measured by X-ray diffraction.

Fine layered nickel hydroxide

Precipitate beta nickel hydroxide by adding sodium hydroxide to an aqueous nickel sulfate solution. Limit the aging time to obtain a coherent domain size of 10 to 20 nm from the (001) X-ray diffraction peak before blending the hydroxide with lithium hydroxide for calcination.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2021/0098787 A1
Published
Apr 1, 2021
Filed
Mar 28, 2019
Class
H01M 4/525
Document BUS 2021/0384502 A1
Published
Dec 9, 2021
Filed
Apr 14, 2021
Class
H01M 4/525
Claim 1
Document A
Document B
1.1A precursor for preparing a cathode active material, characterized by containing a transition metal and having a crystal grain size of 20 nm or less on (001) plane, as measured by XRD.
A cathode active material precursor according to exemplary embodiments includes nickel (Ni) and cobalt (Co) and includes an excess amount of Ni, and A101/A001 is 1 or more and I101/I001 is 1 or more. A101 is a peak area of (101) plane, and A001 is a peak area of (001) plane by an X-ray diffraction (XRD) analysis, and I101 is a peak intensity of (101) plane, and I001 is a peak intensity of (001) plane by the XRD analysis.
A · US 2021/0098787 A1 · ¶ 9
Preparation of the first lithium-transition metal composite oxide particle Ni0.82Co0.13Mn0.10(OH)2 as an NCM precursor and LiOH as a lithium source were mixed for about 20 minutes while grinding.
B · US 2021/0384502 A1 · ¶ 83

An empty cell means only that no passage was reproduced there.

Statements in these documents
However, as the nickel amount becomes greater, a reliability of the cathode active material may be degraded due to a mismatch or a side-reaction with lithium.
A · US 2021/0098787 A1 · ¶ 5
According to an aspect of the present invention, there is provided a cathode active material precursor providing improved power and stability.
A · US 2021/0098787 A1 · ¶ 7
In the lithium secondary battery, a lithium metal oxide is used as a cathode active material, and it is preferable to have a high capacity, a high output, and high life-span characteristics.
B · US 2021/0384502 A1 · ¶ 6
However, when designing the lithium metal oxide for a high output composition, thermal and mechanical stabilities may be deteriorated, and thereby life-span characteristics and operational stability of the lithium secondary battery may be deteriorated.
B · US 2021/0384502 A1 · ¶ 6
Cite aspatent.fyi, US 2026/0356693 A1, claim 1, first published 2026-11-20T05:32:13-05:00, https://patent.fyi/US20260356693/, SHA-256 e3f60c1e93d948824b7e51cca307697e3755becf6df7772a041cea97763fa511
First published
Permanent addresshttps://patent.fyi/US20260356693/
Content fingerprint (SHA-256)e3f60c1e93d948824b7e51cca307697e3755becf6df7772a041cea97763fa511
Methodv2026-11-18.2 · automated, not reviewed by a person