Six oxide precursor batch
The precursor contains 50 wt% SiO2, 25 wt% Al2O3, 17 wt% ZnO, 2 wt% Li2O, 2 wt% MgO, and 4 wt% TiO2 on an oxide basis. The batch is melted and homogenized, then formed and annealed before the crystallization heat treatment.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
No entries.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
The precursor contains 50 wt% SiO2, 25 wt% Al2O3, 17 wt% ZnO, 2 wt% Li2O, 2 wt% MgO, and 4 wt% TiO2 on an oxide basis. The batch is melted and homogenized, then formed and annealed before the crystallization heat treatment.
The precursor contains 3.0 wt% Li2O and 2.0 wt% TiO2, giving an oxide mass ratio of 1.5. Lithium carbonate supplies the lithium oxide on an oxide basis after carbon dioxide leaves the batch during melting.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Oxide Component Broad Range (wt %) Preferred Range (wt %) More Preferred Range (wt %) B2O3 40-85 45-81 55-80.5 Na2O 0-10 0.5-9.0 1-6.5 Al2O3 0-20 0.5-18.5 1.0-15.5 Li2O 0-2 0.3-1.8 0.5-1.6 TiO2 0-6 0.2-5.5 0.3-4.5 ZnO 0-15 0.2-11.5 0.3-10 Ta2O5 0-30 0-26 0-25 Nb2O3 0-16 0-15.5 0-15 BaO 0-45 0-20 0-10 ZrO2 0-5 0-4.6 0-3.8 SiO2 0-5 0-4.5 0-4.0A · US 2014/0314969 A1 · ¶
These positively photosensitive glasses have been previously described hereinabove, and comprise: from about 68 wt % to about 78 wt % SiO2 (68 wt %≤SiO2≤78 wt %); up to about 1 wt % K2O (0 wt %≤K2O≤1 wt %); from about 5 wt % to about 10 wt % ZnO (4 wt %≤ZnO≤8 wt %); up to about 10 wt % Br− (0 wt %≤Br−≤10 wt %); from about 5 wt % to about 14 wt % Al2O3 (5 wt %≤Al2O3≤12 wt %); from about 0.01 wt % to about 0.07 wt % CeO2 (0.01 wt %≤CeO2≤0.07 wt %); from about 0.01 wt % to aboutB · US 10,703,671 B2 · ¶ 58
An empty cell means only that no passage was reproduced there.
Recently the market, under environmental pressures, has demanded a composition that does not contain hazardous components such as lead, bismuth or vanadium, and can seal at a low temperature.A · US 2014/0314969 A1 · ¶ 7
The seal materials can be cured/fired at low temperatures—less than about 600° C.A · US 2014/0314969 A1 · ¶ 10
patent.fyi, US 2026/0356734 A1, claim 1, first published 2026-11-20T06:11:26-05:00, https://patent.fyi/US20260356734/, SHA-256 2523872e5905f3d79f29e13a58affcd5a6effb1e4051404c3f5c87b41d99b885