Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
No entries.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Component substitution
Magnesium oxide replaces calcium oxide
The oxide batch contains 68.5 mol % SiO2, 3.5 mol % Al2O3, 1.2 mol % P2O5, 3.0 mol % ZrO2, 23.0 mol % Li2O, and 0.8 mol % MgO. Magnesium oxide takes the place of calcium oxide on an equal-mole basis, and the melt is cast and annealed as a precursor plate. Differential scanning calorimetry guides the selection of nucleation and growth holds for the modified batch. X-ray diffraction identifies the resulting phases, and visible-light haze measurements screen plates for a transparent petalite and lithium disilicate microstructure.
Parameter or scale variation
Staged firing of meter wide sheets
An annealed precursor sheet measuring 1000 by 600 by 3 mm rests on a flat alumina setter in a furnace with separately controlled edge and center heating zones. A 1 °C per minute ramp brings the sheet to a composition-specific nucleation temperature for a 60-minute hold, followed by a second 1 °C per minute ramp to the crystal growth temperature for a 30-minute hold. Thermocouples positioned near the sheet center and corners track the temperature spread, and the zone setpoints maintain a spread of 5 °C or less during each hold.
Automated or data-driven variant
Optical feedback controls crystal growth
A furnace holds a witness coupon cut from the same precursor sheet as the production plates, with an optical port on each side of the coupon. An external modulated light source and two detectors measure direct transmission and off-axis scatter through the ports during the growth hold. A controller compares the scatter-to-transmission ratio with a time trace from runs whose cooled coupons meet phase and haze targets. The controller adjusts the hold duration within preset limits and starts controlled cooling when the measured trace reaches the calibrated endpoint.
Specific version of a part
Oxide mole percentage calculation
The composition calculation divides the mass of each oxide by its molar mass and normalizes the resulting mole amounts to 100 mol %. Lithium carbonate contributes one mole of Li2O per mole of carbonate to the oxide calculation.
Nine oxide batch formulation
The formulation contains 66.50 mol % SiO2, 3.00 mol % Al2O3, 1.20 mol % P2O5, and 3.00 mol % ZrO2. It also contains 0.30 mol % Na2O, 0.10 mol % K2O, 25.00 mol % Li2O, 0.80 mol % CaO, and 0.10 mol % B2O3.
Three oxide ratio settings
A formulation uses 25.00 mol % Li2O, 1.20 mol % P2O5, 3.00 mol % ZrO2, and 0.80 mol % CaO, with Na2O, K2O, and B2O3 totaling 0.50 mol %. The three molar ratios in the listed order are 20.833, 5.100, and 21.739.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1based on molar percentage of oxides, a composition of the transparent glass-ceramic comprises:
The invention relates to a filter of which the filtering portion is made from an inorganic material comprising grains of SiC bonded by a vitroceramic phase, to form a porous structure of which the apparent porosity is between 20 and 70%, said vitroceramic bonding phase comprising at least the following components, in molar percentage of the total oxides present in said phase: SiO2: 30% to 80% Al2O3: 5% to 45% MO: 10% to 45%, where MO is an oxide of a divalent cation or the su
A · US 2011/0185690 A1 · abstract
In general, the compositions described herein have low amounts of non-lithium alkali oxides.
B · US 2023/0242442 A1 · ¶ 88
1.2SiO2: 60.90 mol % to 72.65 mol %, Al2O3: 1.50 mol % to 5.00 mol %, P2O5: 0.85 mol % to 1.50 mol %, ZrO2: 2.00 mol % to 4.00 mol %, Na2O: 0.00 mol % to 1.00 mol %, K2O: 0.00 mol % to 0.50 mol %, Li2O: 20.00 mol % to 30.00 mol %, CaO: 0.00 mol % to 1.60 mol %, and B2O3: 0.00 mol % to 1.00 mol %;
At concentrations greater than 4 mol %, ZrO2 can form a primary liquidus phase at a high temperature, which significantly lowers the liquidus viscosity.
B · US 2023/0242442 A1 · ¶ 90
1.3based on a content expressed as the molar percentage of each oxide in the composition of the transparent glass-ceramic, the composition of the transparent glass-ceramic satisfies: 18.200≤Li2O/P2O5≤25.500; 4.100≤(Li2O+Na2O+K2O+B2O3)/(P2O5+ZrO2+CaO)≤6.000; and 14.000≤2×Li2O/(0.5×ZrO2+CaO)≤23.000.
An empty cell means only that no passage was reproduced there.
Statements in these documents
While the use of recrystallized SiC (R-SiC), combined with filter segmentation techniques, has significantly improved the thermomechanical strength of filters, and thereby lengthened filter service life while sharply lowering the risks of cracking, the production of such filters incurs substantial extra costs in comparison with cordierite filters for example.
A · US 2011/0185690 A1 · ¶ 6
It is therefore the object of the present invention to provide a filter of which the production cost is lowered, but which has thermomechanical strength properties at least comparable to those observed with a R-SiC filter.
A · US 2011/0185690 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0356736 A1, claim 1, first published 2026-11-20T06:11:26-05:00, https://patent.fyi/US20260356736/, SHA-256 17889f0e0ed3f5915394e49e2f4407bb44b2e3e4ed20172271bb65698f2b8264