patent.fyi
Applications  /  US 2026/0356738
United States Patent Application Publication

US 2026/0356738 A1

Published
Nov 12, 2026
Filed
Jun 11, 2026
Earliest date on the face
Dec 25, 2023
Classification
C03C 10/0045
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

No entries.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Component substitution

Potassium oxide for partial sodium replacement

In a reference batch containing 6.0 mol % Na₂O and 5.0 mol % Li₂O, replace 0.5 mol % Na₂O with 0.5 mol % K₂O while keeping the other oxide proportions fixed. Cast and ceram the plate to form a (Zn, Mg)Al₂O₄ main phase and a tetragonal ZrO₂ secondary phase. Immerse the plate in molten sodium nitrate to exchange sodium ions for lithium ions from both faces, and measure the stress profile after cooling.

Specific version of a part

Seven-oxide center composition

The center contains 43.00 mol % SiO2, 29.00 mol % Al2O3, 4.00 mol % ZrO2, 5.00 mol % MgO, 9.00 mol % ZnO, 5.00 mol % Na2O, and 5.00 mol % Li2O. The melt is homogenized before forming, and staged heat treatment develops spinel and tetragonal zirconia.

Center ratio near one tenth

The center contains 42.00 mol % SiO2, 28.00 mol % Al2O3, 5.00 mol % MgO, 8.00 mol % ZnO, and 6.00 mol % Li2O, with 5.00 mol % ZrO2 and 6.00 mol % Na2O completing the composition. The denominator is 57.00 mol %, giving a lithium oxide ratio of 0.1053.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2019/0194057 A1
Published
Jun 27, 2019
Filed
Mar 4, 2019
Class
C03C 3/085
Document BUS 11,447,415 B2
Published
Sep 20, 2022
Filed
Sep 23, 2021
Class
C03C 3/093
Claim 1
Document A
Document B
1.1a composition at a center of the strengthened glass ceramic comprises: SiO2 35.00 mol % to 60.00 mol %, Al2O3 20.00 mol % to 40.00 mol %, ZrO2 2.00 mol % to 8.00 mol %, MgO 3.00 mol % to 7.50 mol %, ZnO 7.00 mol % to 13.00 mol %, Na2O 1.00 mol % to 10.00 mol %, and Li2O 2.50 mol % to 10.00 mol %, based on a mole percentage of oxides;
S-6 Sample sheet thickness (mm) 0.55 0.558 0.558 0.558 0.558 0.558 Composition SiO2 67.58 67.58 67.58 67.58 67.58 67.58 component Al2O3 10.08 10.08 10.08 10.08 10.08 10.08 (mol %) B2O3 0.00 0.00 0.00 0.00 0.00 0.00 P2O5 0.00 0.00 0.00 0.00 0.00 0.00 Li2O Na2O 14.17 14.17 14.17 14.17 14.17 14.17 K2O 0.05 0.05 0.05 0.05 0.05 0.05 MgO 8.01 8.01 8.01 8.01 8.01 8.01 CaO 0.06 0.06 0.06 0.06 0.06 0.06 SrO 0.01 0.01 0.01 0.01 0.01 0.01 BaO ZnO TiO2 ZrO2 0.04 0.04 0.04 0.04 0.04 0.04
A · US 2019/0194057 A1 · ¶
FIG. 1 shows NMR spectra for samples of the glasses described herein having the composition 67.45 mol % SiO2, 12.69 mol % Al2O3, 3.67 mol % B2O3, 13.67 mol % Na2O, 2.36 mol % MgO, and 0.09 mol % SnO2.
B · US 11,447,415 B2 · ¶ 21
1.2the composition at the center of the strengthened glass ceramic satisfies:
1.36.82 mol %≤Na2O+Li2O≤15.00 mol %,
1.40.26≤Na2O/Li2O≤3.00, and
1.50.06≤Li2O/(Al2O3—(MgO+ZnO)+SiO2)≤0.20,
1.6based on the mole percentage of each oxide in the composition of the strengthened glass ceramic;
The value of X is calculated based on the formula, X=SiO2×329+Al2O3×786+B2O3×627+P2O5×(−941)+Li2O×927+Na2O×47.5+K2O×(−371)+MgO×1230+CaO×1154+SrO×733+ZrO2×51.8, by using the contents in mole percentage on an oxide basis of components.
A · US 2019/0194057 A1 · abstract
Unless otherwise specified, all compositions and concentrations described herein are expressed in mole percent (mol %).
B · US 11,447,415 B2 · ¶ 14
1.7wherein W[(Zn, Mg)Al2O4] is a weight percentage of the (Zn, Mg)Al2O4 crystalline phase based on the strengthened glass ceramic, W[Al2O3] is a weight percentage of Al2O3 based on the strengthened glass ceramic, W[MgO] is a weight percentage of MgO based on the strengthened glass ceramic, and W[ZnO] is a weight percentage of ZnO based on the strengthened glass ceramic, A=(1−W[(Zn,Mg)Al2O4]/2)×W[Al2O3]/2, B=(1−W[(Zn,Mg)Al2O4])×(W[MgO]+W[ZnO]), C=A/B, and in the strengthened glass ceramic, 1.50≤C≤1.85.

An empty cell means only that no passage was reproduced there.

Statements in these documents
More particularly, the disclosure relates to such glasses that are strengthened by ion exchange and possess resistance to damage by abrasion, scratching, indentation, and other forms of sharp contact.
B · US 11,447,415 B2 · ¶ 2
The ion exchange process provides a substantial improvement of glasses that are capable of being strengthened by this process to resist damage by sharp impact or indentation.
B · US 11,447,415 B2 · ¶ 3
Cite aspatent.fyi, US 2026/0356738 A1, claim 1, first published 2026-11-20T06:11:26-05:00, https://patent.fyi/US20260356738/, SHA-256 a9c11e3162d16a4625e6caccf54431e786086a79cac5b9b507135197537a7934
First published
Permanent addresshttps://patent.fyi/US20260356738/
Content fingerprint (SHA-256)a9c11e3162d16a4625e6caccf54431e786086a79cac5b9b507135197537a7934
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi