1.1Tungsten bronze particle dispersion
Cesium tungsten bronze nanoparticles disperse in an acrylic resin solution with a polymeric dispersant. After drying, charge carriers in the particles absorb near-infrared light.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Cesium tungsten bronze nanoparticles disperse in an acrylic resin solution with a polymeric dispersant. After drying, charge carriers in the particles absorb near-infrared light.
A squaraine dye dissolves with acrylic resin in a compatible organic solvent. The solvent evaporates after coating, leaving the dye in the resin, where it absorbs light in a band set by its molecular structure.
A heated extruder disperses carbon black in molten polyethylene. A flat die spreads the melt onto a substrate, and a chill roll solidifies the absorbing layer.
An electrostatic spray gun deposits carbon-black-filled polyester powder onto grounded metal. In an oven, the powder melts, flows across the surface, and cures into an absorbing film.
An air-assisted spray gun applies the dilute absorber and binder mixture in thin passes. Solvent evaporates between passes, and successive coats build the dry absorber loading needed for the target optical density.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Anhydrous copper(II) phosphate particles supply the copper and phosphorus light absorber. A bead mill disperses the particles in water with a polyacrylate dispersant, and a waterborne acrylic binder is added after milling. Water addition sets the total dry mass ratio to 35% before coating. Drying removes the water and fixes the particles in the binder.
A stirred vessel on load cells receives a concentrated dispersion of a copper and phosphorus light absorber and a compatible solvent through separate metering pumps. An automated gravimetric analyzer weighs a batch sample before and after drying it to constant mass. A controller uses the measured dry mass ratio and vessel mass to calculate solvent additions above a 35% setpoint and concentrate additions below it. The controller repeats mixing and sampling until the measured ratio is within one percentage point of the setpoint.
A slot die deposits a 30-micrometer wet layer of an ethyl acetate formulation containing a copper and phosphorus light absorber and an acrylic binder at 30% dry mass onto a polyester web. At 3 meters per minute, the web spends 30 seconds in a 1.5-meter drying zone supplied with air at 45 °C, then 60 seconds in a 3-meter zone supplied with air at 70 °C. The first zone allows the wet layer to level during initial evaporation, and the second removes additional solvent. A chill roll cools the coated web before winding.
Copper(II) ions coordinate with alkyl phosphate ligands to form the absorber. Electronic transitions at the copper centers absorb near-infrared light, and the alkyl groups aid compatibility with the organic coating medium.
A blend of methyl ethyl ketone and cyclohexanone dissolves a compatible copper alkyl phosphate absorber and acrylic binder. Methyl ethyl ketone evaporates faster, while cyclohexanone gives the wet film more time to level.
A 100 g batch contains 30 g of nonvolatile absorber and binder and 70 g of volatile solvent. Drying a representative aliquot to constant mass under conditions that preserve the absorber and binder gives a dry mass fraction of 30%.
A 100 g batch contains 50 g of nonvolatile absorber and binder and 50 g of solvent. A metering bar sets the wet coat thickness, and a forced-air oven evaporates the solvent.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
The component (B) is composed of a copper complex obtained by a reaction of a phosphonic acid compound represented by Formula (I), two or more kinds of phosphoric acid ester compounds or sulfonic acid ester compounds having different structures, and a copper compound.B · US 2022/0171107 A1 · ¶ 127
The percent solids by weight (w/w %) is the weight of dry solids in a given volume of a composition divided by the total weight of the composition multiplied by 100%. w/w % is calculated using the following formula:A · US 2021/0032164 A1 · ¶ 22
In addition, when the ratio of the solid content to the near-infrared absorbing composition is within the range of 5 to 30% by mass, a suitable concentration of the solid matter (for example, copper complex particles) is obtained, and the particles aggregate during the storage period is suppressed, and more excellent storage stability (dispersion stability of copper complex particles and near-infrared light absorbing ability) may be obtained, which is preferable.B · US 2022/0171107 A1 · ¶ 138
An empty cell means only that no passage was reproduced there.
Although usable for other purposes, in some embodiments, the composition is used to make ceramic pieces, e.g., via casting, pressing, jiggering or jollying, especially when the ceramic formulation has solids, chemistry and viscosity suitable for shaping before drying, sintering, and optionally finishing.A · US 2021/0032164 A1 · ¶ 1
One disadvantage of Ball Clay is difficulty reaching a stable viscosity, without aging Ball Clay slurry for one to seven days prior to production of a full slip.A · US 2021/0032164 A1 · ¶ 8
More specifically, the present invention relates to a near-infrared absorbing composition having excellent dispersing, transparency in the visible region, and light absorption of near-infrared light, a near-infrared absorbing film capable of reducing the film thickness, and an image sensor for a solid-state imaging element provided with the near-infrared absorbing film.B · US 2022/0171107 A1 · ¶ 1
The near-infrared absorption is mainly exhibited by the copper complex, and in order to impart sufficient near-infrared absorption to the color filter when the film is thinned as described above, it is necessary to improve the absorption characteristics in the near-infrared region of the copper complex.B · US 2022/0171107 A1 · ¶ 8
patent.fyi, US 2026/0356740 A1, claim 1, first published 2026-11-20T06:11:26-05:00, https://patent.fyi/US20260356740/, SHA-256 47c9750d2915a946ce0ba139096d3f2682cbaef3775f093eabe9f7fe8158f1b3