patent.fyi
Applications  /  US 2026/0356742
United States Patent Application Publication

US 2026/0356742 A1

Published
Nov 12, 2026
Filed
Jul 20, 2026
Earliest date on the face
Dec 5, 2022
Classification
C03C 17/245
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Sapphire as the substrate

What ifWhat if a polished sapphire plate supports the optical coating?
Claim language“a glass substrate”

The crystalline alumina plate transmits visible light and provides a hard support for the coating. The coating thicknesses are tuned for the refractive index of sapphire to reduce front-surface reflection.

1.2Graded porosity for antireflection

What ifWhat if a single silica film with a continuous porosity gradient reduces reflection above the scratch-resistant layer?
Claim language“alternating high refractive index and low refractive index layers”

Oblique-angle deposition forms a silica film with progressively higher porosity toward the air-facing surface. The increasing air fraction lowers the effective refractive index toward the surface and reduces reflection across a band of wavelengths.

1.2Scratch resistance within the glass

What ifWhat if the bulk glass supplies scratch resistance and carries only a thin antireflective coating?
Claim language“a scratch-resistant layer”

A high-hardness aluminosilicate glass resists penetration by abrasive particles. A thin dielectric stack controls reflection, and ion exchange puts the glass surface into compression to limit crack growth during abrasive contact.

1.2Etched glass for antireflection

What ifWhat if a subwavelength texture etched directly into the glass reduces reflection?
Claim language“disposed on the first major surface of the glass substrate”

A temporary mask defines tapered features with a pitch of approximately 150 nm, and the mask is stripped after etching. The glass fraction increases from the feature tips toward the bulk, creating a gradual effective refractive index transition.

1.3Hardness with a cube-corner tip

What ifWhat if a cube-corner diamond tip measures indentation hardness?
Claim language“Berkovich Indenter Hardness Test”

An instrumented indenter records force and displacement as the three-sided cube-corner tip penetrates the coating. The measured peak force divided by the projected contact area from the calibrated tip area function gives the indentation hardness.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Coated viewing window for food processing

A flat glass panel forms a viewing window in the door of a food processing enclosure. The washdown-facing surface carries alternating high- and low-index films below and above a scratch-resistant layer. A compressible perimeter gasket seals the panel in a retaining frame, and each film above the scratch-resistant layer is thinner than 200 nm. The alternating films reduce reflections from overhead lighting, and the scratch-resistant layer limits abrasion during cleaning.

Component substitution

Diamondlike carbon scratch layer for infrared optics

An infrared-transmitting chalcogenide glass plate carries alternating zinc sulfide and magnesium fluoride films beneath a 700 nm hydrogenated diamondlike carbon scratch-resistant layer. A second set of alternating zinc sulfide and magnesium fluoride films covers the carbon layer, with each upper film thinner than 200 nm. An optical transfer-matrix calculation uses measured refractive indices and absorption coefficients to set the film thicknesses for low reflection near 1.55 µm. The carbon layer supplies the hard bearing layer beneath the outer films.

Parameter or scale variation

Visible coating for oblique viewing

A glass plate carries two high- and low-index film pairs below a 1.2 µm scratch-resistant layer and two pairs above it. Each upper film has a physical thickness between 35 and 140 nm. A thin-film calculation varies the individual film thicknesses to minimize mean reflectance from 450 to 650 nm over incidence angles from 30 to 50 degrees, using equal weights for the two linear polarizations. The calculation includes the measured refractive index and thickness of the scratch-resistant layer.

Combination with existing systems

Coated cover for capacitive touch displays

The user-facing side of a glass cover carries alternating high- and low-index films below and above a scratch-resistant layer. An optically clear adhesive bonds the opposing glass surface to a projected-capacitive touch sensor, and a second adhesive layer bonds the sensor to a flat-panel display. The touch controller calibrates its baseline capacitance after lamination and detects finger position through the coated cover. The front film stack reduces ambient reflections, and the adhesive fills the air gaps between the bonded parts.

Automated or data-driven variant

Optical feedback during coating deposition

A vacuum deposition system places a glass witness coupon on the same moving carrier as the production panels. A broadband optical monitor measures the coupon reflectance as the system deposits the lower alternating films, the scratch-resistant layer, and the upper alternating films in sequence. Software fits each spectrum to a thin-film model and closes the source shutter when the fitted thickness reaches the layer target. The controller also closes the shutter at a preset time limit calculated from a calibrated upper bound on the deposition rate.

Automated mapping of coating uniformity

A motorized stage moves the coated glass beneath a broadband reflectometer after both sets of alternating films and the intervening scratch-resistant layer are in place. The reflectometer records spectra on a 10 mm grid, and software fits each spectrum using the measured optical constants and the target layer sequence. The software maps visible reflectance and applies one fitted thickness multiplier to each set of alternating films to estimate spatial variation. The deposition controller uses repeatable variation across panels to update the carrier speed profile for the next batch.

Specific version of a part

Flat aluminosilicate glass substrate

A 0.8 mm lithium aluminosilicate sheet has two opposing, polished major surfaces. The glass contains 7.5 mol % lithium oxide and 5.0 mol % sodium oxide, giving a lithium oxide to sodium oxide molar ratio of 1.5.

Oxide layers around silicon nitride

A 2.0 µm silicon nitride scratch-resistant layer sits between alternating tantalum pentoxide and silicon dioxide layers deposited by reactive sputtering. Each layer above the nitride is 30 to 120 nm thick, and the layer thicknesses are tuned to reduce visible reflection.

Depth-controlled diamond indentation

An instrumented three-sided pyramidal diamond tip advances from the coated surface to a nominal depth of 600 nm. The test uses a calibrated tip area function and unloading stiffness to determine contact area, then calculates hardness from force divided by contact area and reports the maximum over the specified evaluation interval.

Face-down drop onto coarse abrasive

A guided release drops the coated article face down onto a fresh sheet of 80 grit sandpaper backed by a rigid plate. The test records the first height that produces fracture in an increasing-height sequence, with 50 cm as the minimum specified failure height.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2014/0131091 A1
Published
May 15, 2014
Filed
Nov 9, 2012
Class
C03C 17/22
Document BUS 11,231,526 B2
Published
Jan 25, 2022
Filed
Apr 17, 2019
Class
G02B 1/14
Claim 1
Document A
Document B
1.1a glass substrate comprising a first major surface and a second major surface, wherein the first major surface and the second major surface are opposing sides of the glass substrate,
A glass article comprises a glass main body having opposing major surfaces, and a layer provided over a majority of a first major surface.
A · US 2014/0131091 A1 · ¶ 19
The substrate 110 includes opposing major surfaces 112, 114 and opposing minor surfaces 116, 118.
B · US 11,231,526 B2 · ¶ 59
1.2an optical coating disposed on the first major surface of the glass substrate, the optical coating forming an anti-reflective surface, wherein the optical coating comprises a scratch-resistant layer and an anti-reflective coating comprising a plurality of alternating high refractive index and low refractive index layers disposed between the scratch-resistant layer and the glass substrate and over the scratch-resistant layer, wherein the thickness of the scratch-resistant layer is from about 500 nm to about 5000 nm, and wherein each of the plurality of alternating high refractive index and low refractive index layers disposed over the scratch-resistant layer have a thickness of less than 200 nm; and
The phase-transformable layer may comprise an optically-transparent hard coat that imparts scratch-resistance to the glass substrate.
A · US 2014/0131091 A1 · ¶ 20
A device comprising: a cover article, the cover article comprising a substrate comprising a substrate surface, and an optical film disposed on the substrate surface forming a coated surface, wherein the optical film comprises a scratch-resistant layer and an optical interference layer disposed between the scratch-resistant layer and the substrate, the optical interference layer comprising at least one set of sub-layers, the set of sub-layers comprising a first low refractive
B · US 11,231,526 B2 · claim 20
1.3wherein the coated glass article exhibits a maximum hardness of from about 10 GPa to about 30 GPa measured at an indentation depth of about 600 nm from the anti-reflective surface of the optical coating, the maximum hardness measured by a Berkovich Indenter Hardness Test; and
An example phase-transformation layer can have a Berkovich indenter hardness for an indentation that is shallower than 100 nm of at least 10 GPa, e.g., a Berkovich indenter hardness of between 10 and 30 GPa.
A · US 2014/0131091 A1 · ¶ 58
The Berkovich Indenter Hardness Test includes indenting the coated surface 101 of the article or the surface of the optical film (which may include the scratch resistant layer, described herein) with the diamond Berkovich indenter to form an indent to an indentation depth in the range from about 50 nm to about 1000 nm (or the entire thickness of the optical film, whichever is less) and measuring the maximum hardness from this indentation along the entire indentation depth ran
B · US 11,231,526 B2 · ¶ 62
1.4wherein the coated glass article has a failure height of greater than or equal to 50 cm as measured according to a Drop Test Method on 80 grit sandpaper.

An empty cell means only that no passage was reproduced there.

Statements in these documents
In view of the foregoing, it would be desirable to provide a hard, optically-transparent, scratch-resistant layer that can be provided on a rigid glass cover that is economical, and physically and chemically compatible with the underlying glass.
A · US 2014/0131091 A1 · ¶ 6
Such a scratch-resistant layer can minimize the formation of scratches and, in some embodiments, minimize the visibility of scratches that do form.
A · US 2014/0131091 A1 · ¶ 6
The disclosure relates to articles with scratch resistance, abrasion resistance or a combination thereof, which also exhibit retained optical properties and more particularly to articles that exhibit a high hardness and low color shift when viewed at different incident illumination angles.
B · US 11,231,526 B2 · ¶ 2
Cover and housing substrates may also be used in architectural articles, transportation-related articles, appliance articles, or any article that requires some transparency, scratch-resistance, abrasion resistance or a combination thereof.
B · US 11,231,526 B2 · ¶ 3
Cite aspatent.fyi, US 2026/0356742 A1, claim 1, first published 2026-11-20T06:11:26-05:00, https://patent.fyi/US20260356742/, SHA-256 ccc720efb94b6b9e6fb55ebcc53fff5f0dc4ebc46183e1f2a2e724bd55d22848
First published
Permanent addresshttps://patent.fyi/US20260356742/
Content fingerprint (SHA-256)ccc720efb94b6b9e6fb55ebcc53fff5f0dc4ebc46183e1f2a2e724bd55d22848
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi