Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Core under residual tension
What ifWhat if the window has a tensile core between two compressive surface layers?
Claim language“a base layer having a compressive stress value of zero”
Both faces of a sodium aluminosilicate sheet undergo potassium ion exchange. Residual tension in the interior balances the compression at the faces, and stress passes through zero at the boundary of each compressive layer.
1.2Single smooth stress profile
What ifWhat if the compressive stress decreases along a single smooth diffusion profile with no separate steep region?
Claim language“a second compressive stress change rate that is at least 5 times”
A single molten potassium nitrate bath exchanges potassium ions for sodium ions in the glass. The potassium enrichment falls smoothly with depth, and the resulting surface compression reduces the opening of shallow surface cracks.
1.3Stress gradients across the face
What ifWhat if the three rates describe changes in surface compression with distance inward from the window edge?
Claim language“according to a depth in a thickness direction”
A removable ion exchange barrier covers the central field of the window during an additional potassium nitrate treatment. A graded barrier opening controls salt access across the border, and the exposed perimeter receives added compression to protect edge flaws.
1.4Shallower stress transition
What ifWhat if the inflection region begins 8 to 12 μm below the surface?
Claim language“about 15 to 30 μm”
A first potassium exchange and a heat hold establish the deeper compression profile. A brief second potassium exchange concentrates additional compression near the surface, and its duration sets the depth of the transition.
1.5Thinner compressive surface layer
What ifWhat if the compressive layer extends only 45 to 60 μm into the glass?
Claim language“about 80 to 100 μm”
A shorter initial potassium exchange limits the depth of ion penetration, and a brief second exchange raises compression near the surface. The 45 to 60 μm depth is measured from the surface to the zero crossing, and compression within that layer reduces opening of shallow scratches.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Protective window for conveyor imaging
A chemically strengthened, lithium-free glass pane sits between a line-scan camera and a conveyor carrying loose aggregate. Both faces carry potassium-enriched compressive layers, each with a steep near-surface stress gradient that transitions into a shallower gradient at greater depth. A perimeter gasket supports the pane in a removable frame so the camera images the belt through the central opening while the pane intercepts airborne grit.
Component substitution
Potassium sulfate in the first bath
Potassium sulfate supplies the exchange potassium in the first bath in place of potassium nitrate, and molten sodium nitrate serves as the carrier. The bath operates at 450 °C with the sulfate loading below its solubility limit at operating temperature, and potassium from the melt exchanges with sodium in the lithium-free glass. After the intermediate heat treatment redistributes potassium inward, a second bath of molten potassium nitrate adds potassium near the surface and steepens the near-surface stress gradient.
Parameter or scale variation
Deeper compression in a thick pane
A 1.2 mm sodium aluminosilicate pane has two treated faces, each with a target compression depth of 125 to 145 μm and a target transition onset of 32 to 40 μm below the surface. A first potassium exchange establishes the subsurface potassium profile, and an 8-hour hold at 480 °C redistributes potassium farther inward. A second potassium exchange restores the steep near-surface stress gradient, and depth-resolved stress measurements on witness panes guide adjustment of the two bath dwell times.
Different compression depths on opposing faces
A 1.0 mm lithium-free sodium aluminosilicate pane receives two potassium exchanges on each face, with an intermediate heat treatment between exchanges. Separate molten salt reservoirs and high-temperature perimeter seals permit independent dwell times for the two faces. The first exchanges target finished compression depths of 105 to 115 μm on the exposed face and 65 to 75 μm on the interior face, and the second exchanges establish the steeper near-surface stress gradients. Measurements of stress versus depth and pane bow guide dwell adjustments to limit bending caused by the unequal compressive layers.
Combination with existing systems
Strengthened cover for capacitive touch sensing
A lithium-free glass cover with two-stage compressive stress profiles on both faces is bonded to a projected capacitive sensor using an optically clear dielectric adhesive. The sensor carries intersecting transparent transmit and receive electrodes on a separate film beneath the adhesive. The controller measures coupling at the electrode intersections and uses a baseline recorded after lamination to detect finger position through the glass.
Automated or data-driven variant
Batch control using measured stress profiles
A production line processes witness coupons from the same glass lot alongside the windows through both salt baths and the intermediate heat treatment. A depth-resolved optical stress instrument records the finished profiles, and software fits a shallow slope, a transition interval and a steep slope to each profile. The controller uses a calibration table indexed by glass lot and bath composition to adjust the intermediate hold for compression depth and the second bath dwell for transition depth in the next batch.
Specific version of a part
Two stage potassium exchange
An initial potassium nitrate exchange and a four-hour heat hold at 450 °C produce the deeper, shallow-gradient region. A second potassium nitrate exchange establishes the steep near-surface region, with target slope magnitudes of 12 MPa/μm near the surface and 2 MPa/μm deeper in the layer. The slope magnitude increases continuously between the two regions when moving toward the surface.
Optical stress gradient measurement
A scattered-light polarimeter uses a calibrated stress-optic coefficient to reconstruct compressive stress as a function of depth along the surface normal. Straight-line fits give the rates in the two outer regions, and the derivative of a smooth fit gives the changing rate through the transition, all in MPa/μm.
Transition at twenty micrometers
A second potassium nitrate exchange creates a steep near-surface region on glass that already has a deeper, gradual compression profile. The second soak duration is calibrated so the boundary of the transition nearest the surface lies 20 μm below it.
Ninety micrometer compression depth
A potassium nitrate exchange followed by a 450 °C heat hold forms a deep compressive layer in sodium aluminosilicate glass. The first exchange duration is calibrated so the final stress profile after the second exchange crosses zero at 90 μm from the treated surface.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1wherein the window includes: a base layer having a compressive stress value of zero; and a compressive stress layer disposed on at least one of an upper surface or a lower surface of the base layer,
A compressive stress layer 142 is deposited over the top surface of semiconductor substrate 101 and is patterned to form the structure shown in FIG. 1H.
A · US 8,035,166 B2 · ¶ 34
1.2wherein the compressive stress layer includes: a first region having a first compressive stress change rate; a second region having a second compressive stress change rate that is at least 5 times the first compressive stress change rate; and an inflection region having a third compression stress change rate that increases from the first compressive stress change rate to the second compressive stress change rate, and which is formed between the first region and the second region,
1.3wherein each of the first compressive stress change rate, the second compressive stress change rate, and the third compressive stress change rate is defined as a compressive stress change rate according to a depth in a thickness direction,
Still further, while method 100 is described as generating residual stress profiles as a function of depth of a workpiece, in alternative embodiments, the method 100 may be generalized and configured to provide residual stress profiles as a function of a variation in surface location along a predetermined translational path of the workpiece, such as a path along an external surface of the workpiece.
B · US 9,068,908 B2 · ¶ 22
1.4a minimum depth from a surface of the window to the inflection region in the thickness direction is about 15 to 30 μm, and
1.5the compressive stress layer has a thickness of about 80 to 100 μm.
In one embodiment compressive stress layer 142 is a layer of silicon nitride (SiN) having a thickness of approximately 250 Angstroms that is deposited at 480 degrees centigrade such that it has intrinsic compressive stress.
A · US 8,035,166 B2 · ¶ 34
An empty cell means only that no passage was reproduced there.
Statements in these documents
Accordingly, there is a need for NMOS devices and PMOS devices that have higher performance levels than traditional non-stressed NMOS and PMOS devices, but not as high as the performance characteristics provided by conventional DSL fabrication processes.
A · US 8,035,166 B2 · ¶ 4
Thereby, NMOS devices and PMOS devices are provided that have stress levels and performance levels that are higher than non-stressed NMOS and PMOS devices, but less than the stress levels and performance levels of devices formed by conventional dual stress layer processes.
A · US 8,035,166 B2 · ¶ 7
Workpieces, such as, but not limited to, gears, may be exposed to loads that exceed material limits of the workpieces.
B · US 9,068,908 B2 · ¶ 4
In some cases, repeated or cyclic exposure to loads may lead to fatigue failure of a workpiece, especially when a workpiece is exposed to loads of vastly different directional components.
B · US 9,068,908 B2 · ¶ 4
Cite aspatent.fyi, US 2026/0356745 A1, claim 1, first published 2026-11-20T06:11:26-05:00, https://patent.fyi/US20260356745/, SHA-256 512916b350bc3fb02834949c496e6c2bbdc5e899ea878e08506d120e00366996