1.1Micrometer grains form sintered bricks
The classified grains are pressed in a die and heated in an electric furnace. At the sintering temperature, mineral grains bond at their points of contact and the compact densifies.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
The classified grains are pressed in a die and heated in an electric furnace. At the sintering temperature, mineral grains bond at their points of contact and the compact densifies.
The screened aggregate is mixed with ground slag, water, and a sodium silicate solution. The slag reacts to form a hardened binder that transfers compressive loads between the aggregate grains.
An electric furnace heats the screened clasts above the feed's liquidus temperature. The melt is poured into a refractory mold and cooled through its annealing range to limit residual thermal stress.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
An abrasion liner contains hydraulic cement, graded basalt aggregate, and a water dispersion of regolith particles sized 20 to 80 nm. A high-shear mixer disperses the regolith in part of the batch water before the dispersion enters the mortar mixer. The mortar is cast around recessed mounting inserts, compacted on a vibrating table, and moist-cured before installation in the chute.
An aqueous colloidal silica dispersion with particles sized 10 to 30 nm replaces the nano-regolith in a mortar for precast paving tiles. The mortar contains hydraulic cement and graded silica sand, with silica solids dosed at 2 percent of the cement mass. The water in the dispersion counts toward the batch water, and the mortar is vibrated in shallow molds and cured under humid conditions.
Milled basaltic regolith with a median particle diameter of 600 nm supplies 20 percent of the dry mass in a clay and feldspar tile body. The blended powder is granulated at 6 percent moisture and uniaxially pressed at 35 MPa. The pressed tiles are dried at 110 °C and fired at a peak temperature of 1150 °C for 30 minutes.
A gantry-mounted extrusion printer deposits a mortar made from hydraulic cement, fine sand, and a water dispersion of regolith particles sized 30 to 90 nm. A progressive-cavity pump feeds the mixed mortar through a hose to a 25 mm nozzle. The controller synchronizes pump output with gantry speed as the nozzle deposits successive 10 mm layers on a rigid build bed.
A two-hopper vibropress forms a concrete masonry block with a 6 mm facing layer containing cement, fine sand, and regolith particles sized 15 to 70 nm. A high-shear mixer disperses the regolith in the facing mix water before the facing ingredients enter the first hopper. The press places the facing mix against the mold bottom, adds a stiffer concrete backing from the second hopper, and compacts both layers together before demolding and humid curing.
A recirculating stirred-media mill grinds basaltic regolith in water before the slurry enters a cement mortar batching line. An automated sampler dilutes slurry to a fixed solids concentration and measures hydrodynamic particle diameter by dynamic light scattering. A controller continues recirculation until three consecutive samples have an intensity-weighted mean diameter of 60 to 90 nm. A load cell and an inline density meter provide inputs for dosing the slurry and deducting its water from the mortar batch.
A stirred media mill with zirconia beads reduces a suspended regolith powder by abrasion and impact. Centrifugal classification recovers a 40 to 90 nm particle fraction for addition to a cement slurry.
A thermal plasma vaporizes regolith feed and an inert gas cools the vapor to form solid particles. Aerosol classification selects particles with mobility diameters of 10 to 40 nm, and a liquid collector transfers them into mixing water.
patent.fyi, US 2026/0356749 A1, claim 1, first published 2026-11-20T06:49:46-05:00, https://patent.fyi/US20260356749/, SHA-256 a53c99080ef4de9d8c765d0a119064a70995b5446d239b5ed4cabef1a0f64931