1.2Drying acrylic and polymer beads
Solid polymer beads provide bulk and help control shrinkage as water evaporates. The acrylic particles coalesce into a continuous film that binds the beads and adheres to the board and joint tape.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Solid polymer beads provide bulk and help control shrinkage as water evaporates. The acrylic particles coalesce into a continuous film that binds the beads and adheres to the board and joint tape.
The installer mixes bead-filled epoxy resin with an amine hardener and presses the paste into the seam. The resin crosslinks at room temperature and holds the inert beads in a rigid matrix bonded to the seam faces.
Mixing disperses 3 mm polypropylene strands throughout the wet compound. As a crack opens, strands crossing it transfer load through interfacial friction and resist pullout.
The installer beds alkali-resistant glass mesh into the base coat and covers it with a finish coat. The compound keys through the mesh openings, and continuous strands transfer tension across the joint.
A predispersed cellulose slurry supplies 0.01 wt. % dry cellulose on a wet-compound basis. A woven polyester tape bedded across the seam carries tensile load between the boards.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A paste of water, ground gypsum, and chopped flax fiber fills parting seams on the cavity side of reusable gypsum molds for decorative plaster casting. A spatula presses the paste into the assembled seam and strikes it flush with the cavity surface. The paste dries before casting, and the flax fibers bridge the seam as the paste shrinks.
A progressive cavity pump feeds a paste of water, ground gypsum filler, and chopped flax fiber from a hopper to a paper tape applicator. The applicator draws tape from a reel past a slot that deposits paste on the face of the tape that contacts the board. A trailing roller presses the coated tape into the seam, and a wiper blade removes excess paste from the edges.
A paddle mixer combines metered water, ground gypsum filler, and chopped flax fiber in a vessel on load cells. A rotating paddle viscometer measures the mixed paste at a fixed speed and temperature and reports viscosity in BU. A controller targets 350 to 450 BU and doses water in increments of 0.1 percent of the starting batch mass when a reading exceeds the upper limit. The mixer runs for 60 seconds after each dose, and the controller releases the batch when the reading enters the target band.
Finely ground fired clay replaces the cementitious filler in a water based paste reinforced with chopped flax fiber. The dry blend contains fired clay screened through a 75 micrometer sieve and redispersible acrylic binder powder. A paddle mixer disperses the dry blend in water before the flax fiber is added. The acrylic binder forms a film as water evaporates and holds the clay particles and fibers together.
The mixer receives a measured charge of potable water at 20 °C before the dry blend is added. The water wets the filler, distributes the fibers during mixing, and supplies water for hydration.
Finely ground calcium sulfate hemihydrate provides solid bulk in the wet paste. After mixing with water, it forms interlocking calcium sulfate dihydrate crystals that stiffen and harden the filled joint.
Two-millimeter flax fibers make up 0.50 wt. % of the wet compound on a dry-fiber basis. The mixer disperses the fibers through the dry filler before water addition, and embedded fibers bridge cracks that form as the compound hardens.
A cellulose ether thickens the water phase of a gypsum-based paste. The batch measures 450 BU at 23 °C five minutes after mixing, using a fixed spindle and rotational speed.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
For example, the wetted starch can be mixed with the gauging water prior to the water manifold.B · US 8,303,159 B2 · ¶ 19
The hydraulic cementitious mixture includes in the range of from about 35% to about 65% by weight, based on the weight of the mixture, of ground, granulated blast furnace slag, and in the range of from about 35% to about 65% by weight, based on the weight of the mixture, of gypsum plaster.A · US 2008/0057206 A1 · ¶ 24
A useful form of paper fiber is bleached or unbleached virgin paper fibers. Other cellulosic fibrous materials can be used, alone or in combination with paper fiber.B · US 8,303,159 B2 · ¶ 49
An empty cell means only that no passage was reproduced there.
Due to their self-leveling ability, pourable floor underlayments require very little labor to finish the surface of the poured mixture to a “smoothness” suitable to receive finished floor goods.A · US 2008/0057206 A1 · ¶ 3
Excessive expansion or shrinkage can result in cracks or cause the surface to delaminate from the corresponding substrate.A · US 2008/0057206 A1 · ¶ 4
However, the fine ground starch requires extra energy and costs more to produce and it also produces a fine dust that is difficult to handle during its production and application.B · US 8,303,159 B2 · ¶ 5
In addition, larger particle sizes require less water in the slurry.B · US 8,303,159 B2 · ¶ 6
patent.fyi, US 2026/0356750 A1, claim 1, first published 2026-11-20T06:49:46-05:00, https://patent.fyi/US20260356750/, SHA-256 e57dc1cbd617eca2a12b5ff99751e6e6b28d7ce8a441cba6356a7f4d84c97c74