1.1Char slurry mixed with cement
A high-shear mixer disperses the char in part of the batch water before the slurry enters the main mixer. The main mixer blends in the dry cement and the remaining ingredients to produce a damp feed for pressing.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A high-shear mixer disperses the char in part of the batch water before the slurry enters the main mixer. The main mixer blends in the dry cement and the remaining ingredients to produce a damp feed for pressing.
Screened pumice particles form a lightweight granular skeleton in the pressed mix. The mixer coats the particles with cement paste, which hardens around the compacted grains during moist curing.
The sand forms the main granular skeleton, and screened char contributes a smaller porous fraction. Pressing compacts the damp mixture, and cement hydration binds the grains during moist curing.
Dry blending distributes fine metakaolin through the cement and aggregate before water addition. During moist curing, metakaolin reacts with calcium hydroxide from cement hydration and forms additional binding solids.
The mixer distributes the powder through the dry constituents before water addition. The dissolved polymer disperses cement particles so the paste coats the char at a lower water content.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Cured bricks made from a dry blend of pyrolysis char and cement and a wet blend of water, silica fume, and additives form piers beneath greenhouse growing benches. Brick courses sit on level concrete pads with staggered vertical joints and full mortar beds. A precast cap on each pier distributes the reactions from the bench rails across the top course.
Finely ground metakaolin replaces silica fume at 3% of total batch mass. A high-shear mixer disperses the metakaolin in water containing a polycarboxylate water reducer. The slurry blends with dry pyrolysis char and cement, and the mix undergoes pressing, initial curing in the mold, demolding, and moist curing.
A steel mold with a 200 mm by 100 mm cavity receives the blended char, cement, water, silica fume, and additives for each brick. A hydraulic platen applies 2 MPa for 5 seconds, retracts 1 mm for 2 seconds to let air escape through the punch clearance, then applies 10 MPa for 10 seconds. The compact stays in the covered mold for initial curing before demolding and moist curing.
Pressed and cured char bricks form the infill of an interior partition between steel posts. Mortar beds support the brick courses, and steel ties fastened to the posts extend into the horizontal mortar joints to restrain the infill out of plane. A compressible strip fills the gap between the top course and the overhead beam and accommodates beam movement.
A microwave moisture sensor measures the moisture fraction of the pyrolysis char in the feed chute, and a weigh hopper measures its as-fed mass. A programmable controller adjusts the char feed to reach the target dry char mass and subtracts the water carried by the char from the target batch water mass. A metering valve delivers the corrected water dose to the wet mixer with silica fume and additives before the wet blend is combined with the char and cement.
A servo-hydraulic press uses a platen displacement sensor and a load cell to monitor each charge of the combined dry and wet mixtures. The controller advances the platen until the mold gap reaches the target brick thickness or the load reaches a preset limit, whichever occurs first. It flags any charge that reaches the load limit before the thickness target and holds accepted charges at the target gap for a preset dwell before releasing the platen for initial curing.
A pan mixer blends the char, cement, silica fume, and powdered additives before the spray nozzles open. The mixer distributes the metered water through the moving solids until the feed reaches a uniform damp consistency for pressing.
Crushing and screening produce wood pyrolysis char particles between 0.25 and 2 millimeters. The mixer blends the screened char with dry cement before adding the wet mixture.
The binder contains ground calcium silicate clinker and gypsum. Water hydrates the calcium silicates to form a binding gel, and gypsum regulates early setting.
A high-shear mixer disperses silica fume in a portion of the batch water before the wet mixture contacts the dry blend. The batch water calculation includes all water used to prepare the dispersion.
Calcium formate dissolves in the batch water before the wet mixture enters the mixer. It accelerates early cement hydration and increases the strength of the compact before demolding.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Example char bricks were fabricated by initially combining all dry ingredients together including cement, sand/gravel, and pyrolysis char.A · US 2021/0061714 A1 · ¶ 109
TABLE 8 UHPCs compositions AmSR (% of total binder) 0 6.0 10.0 14.0 20.0 Materials kg/m3 %* kg/m3 %* kg/m3 %* kg/m3 %* kg/m3 %* Water 201.25 201.25 201.25 201.25 210.7113 10.4 Silica fume 175 8.6 122.5 6.0 87,5 4.3 52.5 2.6 0 0,0 Cement 700 34.4 700 34.4 700 34.4 700 34.4 700 34.4 Quartz powder 210 10.3 210 10.3 210 10.3 210 10.3 210 10.3 Quartz sand 950 46.7 950 46.7 950 46.7 950 46.7 950 46.7 AmSR 0 0.0 52.5 2.6 87.5 4.3 122.5 6.0 175 8.6 Water adjusted 175 175 175 175 182.B · US 2023/0060611 A1 · ¶
Water was then added until the damp mixture obtained a suitable consistency, for example, a consistency suitable for molding into a brick morphology.A · US 2021/0061714 A1 · ¶ 109
A mortar composition is further understood as a thick pasty mixture of water, generally a fine aggregate, mineral additions and hydraulic binder (cement) that upon hardening is used to hold building materials together.B · US 2023/0060611 A1 · ¶ 68
It is disclosed the use of amorphous silica reagent produced from serpentine as pozzolane additive material, and more particularly a concrete mixture, such as high performance and ultra-high performance concrete, comprising a hydraulic binder; sand; aggregates, chemical admixture, mineral admixture as silica fume and an amorphous silica reagent (AmSR), wherein the AmSR is admixed for example with General Use Portland Cement and provides synergistic effect when combined with sB · US 2023/0060611 A1 · abstract
Three different compositional ratios were made for char brick fabrication: the mass ratio of cement, sand, pyrolysis char, and water in these compositions are 1:2.1:0.9:1.05, 1:1.8:1.2:1.35, and 1:1.5:1.5:1.65.A · US 2021/0061714 A1 · ¶ 109
An empty cell means only that no passage was reproduced there.
Therefore, there is a need for improved building materials derived from coal, such as char clay plaster, char brick, and foam glass, and methods of fabrication thereof.A · US 2021/0061714 A1 · ¶ 7
Such materials can be manufactured using thermo-chemical processing that does not liberate anthropogenic carbon dioxide.A · US 2021/0061714 A1 · ¶ 8
It is still desirable to find new pozzolane additives with low cost and reliable quality for improving mechanical properties and extending the life span of concrete, with environmental benefits.B · US 2023/0060611 A1 · ¶ 6
It is provided the use of amorphous silica reagent as a pozzolane additive in concrete preparation.B · US 2023/0060611 A1 · ¶ 2
patent.fyi, US 2026/0356751 A1, claim 1, first published 2026-11-20T06:49:46-05:00, https://patent.fyi/US20260356751/, SHA-256 af6f2b7817f1b901d9f2b6953ebc4984d486d9c4ffc2f54cf27c4b59f0531e73