1.1Ground basalt filler
Ground basalt with particles smaller than 150 micrometers fills spaces between coarser particles. The cement paste binds the basalt particles as hydration proceeds.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Ground basalt with particles smaller than 150 micrometers fills spaces between coarser particles. The cement paste binds the basalt particles as hydration proceeds.
Hollow glass microspheres lower the density of the grout by enclosing gas within rigid shells. Low-shear mixing disperses the microspheres in the cement paste and limits shell breakage.
An aqueous epoxy dispersion and a compatible amine hardener form the liquid phase for mixing with screened char. The epoxy and hardener react to form a cross-linked matrix that holds the particles as water evaporates.
The dry blend contains 3% screened char, 70% hydraulic cement, and 27% ground limestone by mass. The limestone supplies fine particles for packing, and cement hydration binds both fillers.
The dry blend contains 30% hydraulic cement, 15% screened char, and 55% graded quartz fines by mass. The grading reduces void volume, and the hydrated cement paste fills spaces between particles and binds the grout.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A grout of screened coal pyrolysis char, hydraulic cement and water fills the gap between a precast drainage channel and its prepared concrete base. Shims set the channel elevation and slope, and temporary edge forms retain the grout. The grout enters along one side and flows beneath the channel until it emerges along the opposite side. The shims support the channel during curing as the grout forms a continuous bearing layer.
A 150 micrometer sieve limits the top particle size of coal pyrolysis char for filling gaps 2 to 4 millimeters thick. A mixer combines 10 kilograms of the screened char with 40 kilograms of hydraulic cement and 30 kilograms of water, giving a water-to-cement mass ratio of 0.75. A low-pressure grout pump feeds the sealed gap from a low port until grout emerges from a high vent. Plugs close both openings during curing.
A grout skid combines a high-shear mixer, an agitated holding tank and a progressive cavity pump. The mixer disperses a dry blend of screened coal pyrolysis char and hydraulic cement into metered water, then discharges the batch into the holding tank. The tank agitator keeps the solids suspended while the pump feeds the placement hose. A return valve routes pump discharge back to the holding tank during short pauses in placement.
A steel splice sleeve embedded in a precast concrete element receives reinforcing bars from adjoining elements and provides a lower grout inlet and an upper vent. A pump fills the sleeve with a grout of screened coal pyrolysis char, hydraulic cement and water until a steady stream exits the vent. Plugs close the ports and temporary bracing holds the elements in alignment during curing. A full-size connection test measures bar slip and tensile capacity for the selected grout and sleeve geometry.
An in-line microwave moisture sensor measures wet-basis moisture in screened coal pyrolysis char as it enters a weigh hopper. A controller uses the measured moisture fraction to convert the target dry char mass to a wet dosing mass, then subtracts the water carried by that dose from the batch water target. The controller meters the corrected water dose through a flowmeter after the char and separately weighed cement enter the mixer. Each batch record stores the estimated dry char mass, measured cement mass and total water mass.
Coal undergoes thermal decomposition under oxygen-limited conditions. The resulting char passes through a 250-micrometer sieve before dry blending with cement.
The cement fraction consists of ground calcium silicate clinker interground with gypsum. The calcium silicates hydrate to form a binding gel, and gypsum regulates the early aluminate reaction.
The cement fraction contains 75% calcium silicate cement and 25% ground granulated blast furnace slag by mass. Cement hydration provides an alkaline pore solution that activates the slag and contributes to formation of the hardened binder.
A batch contains 20 kilograms of dry char and 80 kilograms of cement. The mixer receives 48 kilograms of water for a water-to-cement mass ratio of 0.60.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
In its most general form, the blended cement composition of the present invention includes portland cement (or other hydraulic cement), slag, and supplementary cementitious materials such as fly ash or naturally occurring calcined pozzolans.A · US 2007/0095255 A1 · ¶ 31
The cement compositions are comprised of Ordinary Portland Cement, or blended cements or non-Portland cements made with Supplementary Cementitious Materials (SCMs).B · US 9,731,999 B2 · ¶ 2
Upon mixing the blended cement product with water and aggregates, a highly durable concrete mixture can be produced.A · US 2007/0095255 A1 · ¶ 48
(i) Addition of admixtures, as solutions, suspensions, slurries or solids, during any stage of the preparation of the cement paste, mortar or concrete, and as typified by the addition of admixtures to the mixing water; andB · US 9,731,999 B2 · ¶ 163
An empty cell means only that no passage was reproduced there.
There is a growing trend to try and develop a lower cost cementitious mixture that either reduces or eliminates the dependency on portland cement, i.e., iron, clay, and cement rock/limestone.A · US 2007/0095255 A1 · ¶ 4
There is further a concern that portland cement production releases a large amount of greenhouse gases, and it would be desirable to formulate a more environmentally-friendly product that requires less portland cement.A · US 2007/0095255 A1 · ¶ 4
This invention generally relates to a new class of chemical admixtures for hydraulic cement compositions such as pastes, mortars, grouts and concretes.B · US 9,731,999 B2 · ¶ 2
The admixtures improve the properties of cement compositions, including setting, hardness, compressive strength, shrinkage, and freeze-thaw resistance.B · US 9,731,999 B2 · ¶ 2
patent.fyi, US 2026/0356752 A1, claim 1, first published 2026-11-20T06:49:46-05:00, https://patent.fyi/US20260356752/, SHA-256 520a135c3856bbdc7b70f7e1f84e9c70c776024a8ebc578737eb1444801b43ff