patent.fyi
Applications  /  US 2026/0356757
United States Patent Application Publication

US 2026/0356757 A1

Published
Nov 12, 2026
Filed
Oct 17, 2023
Earliest date on the face
Oct 18, 2022
Classification
C04B 28/006
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Calcined clay as precursor

What ifWhat if metakaolin supplies the reactive aluminosilicate and the mixture contains no fly ash?
Claim language“fly ash”

Calcining kaolinite-rich clay at 650 to 800 °C produces metakaolin. Sodium hydroxide solution dissolves aluminium and silicon from the metakaolin, and the dissolved species form a binding gel during curing.

1.1Ground slag as precursor

What ifWhat if ground granulated blast furnace slag supplies the reactive powder and the mixture contains no fly ash?
Claim language“fly ash”

Water quenching produces a glassy slag that is ground into a fine powder. Sodium hydroxide solution activates the slag, which releases calcium, silicon and aluminium to form a calcium aluminosilicate hydrate binder.

1.2Sodium silicate activation

What ifWhat if aqueous sodium silicate serves as the activator and no alkali metal hydroxide is added?
Claim language“an alkali metal hydroxide”

A sodium silicate solution with a molar silicon dioxide to sodium oxide ratio of about 1.5 supplies alkalinity and dissolved silicate. The alkaline solution dissolves reactive phases in the fly ash, and the dissolved silicate participates in gel formation during curing.

1.3Reactive slag strength additive

What ifWhat if ground granulated blast furnace slag replaces the oxide or hydroxide strength additive?
Claim language“calcium oxide and/or calcium hydroxide, and/or (ii) magnesium oxide and/or magnesium hydroxide”

The dry blend contains 80 parts fly ash and 20 parts finely ground glassy slag by mass. Sodium hydroxide solution activates the slag, forming a calcium aluminosilicate hydrate gel that fills space between particles and binds them together.

1.4Four percent calcium hydroxide

What ifWhat if calcium hydroxide makes up 4 weight % of the combined fly ash and additive mass?
Claim language“5 to 30 weight %”

The dry blend contains 96 parts reactive fly ash and 4 parts calcium hydroxide by mass. Sodium hydroxide solution activates the fly ash, and sealed curing at 60 °C for 24 hours accelerates early gel formation.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Cast weights for stationary laboratory equipment

A fly ash binder activated with aqueous sodium hydroxide fills a steel shell that serves as a counterweight for stationary laboratory equipment. Calcium hydroxide accounts for 15 weight percent of the combined dry mass of fly ash and calcium hydroxide. Internal steel tabs retain the hardened fill, and the shell carries the mounting loads. The filled shell rests under a cover until the binder hardens, then receives a sealed lid.

Component substitution

Calcined kaolin in place of fly ash

Calcined kaolin supplies the reactive aluminosilicate in place of fly ash. The dry blend contains 90 parts calcined kaolin and 10 parts calcium hydroxide by mass. An aqueous potassium hydroxide and potassium silicate solution activates the blend, and the mixer disperses the solids until the paste is uniform. The paste is cast and cured in covered moulds that limit moisture loss.

Parameter or scale variation

Warm curing of thin cast panels

A fly ash paste activated with aqueous sodium hydroxide contains calcium hydroxide at 8 weight percent of the combined dry mass of fly ash and calcium hydroxide. The paste is cast into 20 mm deep moulds and consolidated on a vibrating table. The covered moulds remain in a curing chamber at 60 °C for 18 hours. The panels cool in the covered moulds to below 30 °C before demoulding.

Automated or data-driven variant

Automatic water correction for damp ash

A moisture sensor at the fly ash feeder estimates ash moisture on a wet mass basis, and a hopper scale measures the mass delivered to the mixer. A batch controller calculates dry fly ash mass by multiplying the delivered mass by one minus the measured moisture fraction. The controller meters calcium hydroxide to 15 weight percent of the combined dry mass of fly ash and calcium hydroxide and doses sodium hydroxide solution of known concentration to a set ratio of dissolved sodium hydroxide to dry ash. It subtracts the water in the ash and activator solution from the total recipe water to set the separate water dose.

Combination with existing systems

Twin stream feed for extrusion printing

An agitated hopper feeds a water slurry of fly ash and magnesium hydroxide to an extrusion printer through a progressive cavity pump. Magnesium hydroxide accounts for 12 weight percent of the combined dry mass of fly ash and magnesium hydroxide. A separate metering pump supplies aqueous potassium hydroxide to an inline mixer immediately upstream of the extrusion nozzle. The printer synchronizes both pumps with nozzle travel to control bead size and covers the deposited part during early curing.

Specific version of a part

Glassy low calcium fly ash

The precursor is dry, low-calcium fly ash with a median particle diameter of 15 to 25 µm and a high glass content. Its aluminosilicate glass supplies dissolved silicon and aluminium during alkaline activation.

Aqueous sodium hydroxide activator

The activator is an aqueous sodium hydroxide solution prepared at 8 mol/L. The solution cools to room temperature before mixing with the fly ash and additive.

Finely ground calcium hydroxide

Finely ground calcium hydroxide is dry blended with fly ash before the activator is added. The calcium hydroxide supplies calcium for the formation of calcium-bearing hydrate gels.

Fifteen percent additive loading

The dry blend contains 85 kg of fly ash and 15 kg of calcium hydroxide per 100 kg of combined fly ash and additive. The activator solution is weighed separately.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2013/0032061 A1
Published
Feb 7, 2013
Filed
Oct 28, 2010
Class
C04B 7/02
Document BUS 8,562,735 B2
Published
Oct 22, 2013
Filed
Aug 24, 2012
Class
C04B 18/04
Claim 1
Document A
Document B
1.1fly ash,
In this “ash to energy and cement” (ATEC) process, coal fly ash and ancillary fuels are fed into a thermal reactor along with oxide materials, such as limestone.
A · US 2013/0032061 A1 · abstract
A geopolymer concrete formed by mixing about 3% to about 43% by weight incinerator fly ash, about 3% to about 35% by weight coal fly ash, about 7% to about 38% by weight alkaline activator liquid, and about 31% to about 70% by weight aggregate.
B · US 8,562,735 B2 · abstract
1.2an alkali metal hydroxide, and
The alkaline activator liquid may include a sodium hydroxide solution and sodium silicate.
B · US 8,562,735 B2 · abstract
1.3a strength-enhancing additive comprising (i) calcium oxide and/or calcium hydroxide, and/or (ii) magnesium oxide and/or magnesium hydroxide
The bed materials 103 may be used to produce hydraulically active cementitious material from CFA 101. The bed materials 103 may include limestone or other materials with sufficient calcium oxide content.
A · US 2013/0032061 A1 · ¶ 30
1.4wherein the strength-enhancing additive is present in an amount of 5 to 30 weight % based on the total weight of fly ash and strength-enhancing additive in the geopolymerisation mixture.
The weight proportion of the Class C coal fly ash to crushed limestone in this example was 2:1. This proportion may vary depending on the amount of calcium oxides needed to reach the desired Ca:Si elemental composition ratio in the overall material.
A · US 2013/0032061 A1 · ¶ 75

An empty cell means only that no passage was reproduced there.

Statements in these documents
One reason that the high carbon CFA cannot be used in concrete is that the carbon interferes with air entrainment (the intentional creation of tiny air bubbles in concrete), introduced to increase the durability of hardened concrete.
A · US 2013/0032061 A1 · ¶ 6
Still more particularly, the present invention relates to the production of SCM from high carbon coal fly ash, wherein carbon in the fly ash and coal is thermally processed to produce synthesis or combustion gas for generating steam to produce electrical power and wherein oxides are added to the thermal process to form cementitious materials having desired properties.
A · US 2013/0032061 A1 · ¶ 1
A method for decreasing the toxicity of incinerator fly ash, the method including activating the incinerator fly ash with an alkaline activator liquid to form a geopolymer.
B · US 8,562,735 B2 · ¶ 4
In another embodiment, a composition of matter is formed by the mixing of the components including: about 3% to about 43% by weight incinerator fly ash; about 3% to about 35% by weight coal fly ash; about 7% to about 38% by weight alkaline activator liquid; and about 31% to about 70% by weight aggregate.
B · US 8,562,735 B2 · ¶ 3
Cite aspatent.fyi, US 2026/0356757 A1, claim 1, first published 2026-11-20T06:49:46-05:00, https://patent.fyi/US20260356757/, SHA-256 a94bcfed75ad0cc723db9ad3edcb6b64ba8eb5f77dd398816e3abaed1e4e1c9f
First published
Permanent addresshttps://patent.fyi/US20260356757/
Content fingerprint (SHA-256)a94bcfed75ad0cc723db9ad3edcb6b64ba8eb5f77dd398816e3abaed1e4e1c9f
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi