Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Spinel ferrite in silicone
What ifWhat if nickel–zinc spinel ferrite supplies the magnetic loss in the sheet?
Claim language“magnetoplumbite-type ferrite”
Calcined nickel–zinc spinel powder disperses in silicone and dissipates microwave energy through magnetic loss near its resonance band. A conductive backing reflects the transmitted field through the composite, and the layer thickness sets the frequency of minimum reflection.
1.2Resin infiltration of porous granules
What ifWhat if the powder compacts to 2.7 g/cm³ and liquid silicone infiltrates its porous granules?
Claim language“compression density of 3.00 g/cm3 or more”
Vacuum degassing removes air from open pores before liquid silicone fills them. The cured silicone forms a continuous flexible phase, and the embedded ferrite grains provide magnetic loss.
1.2Classified powder with fewer fines
What ifWhat if the powder has a D10 of 1.2 μm and the sheet uses a low-viscosity silicone binder?
Claim language“D10 of 0.8 μm or less”
Air classification removes fines, reducing the particle surface area that the binder must wet. The silicone wets the remaining particles during mixing, and the dispersed ferrite supplies magnetic loss in the cured sheet.
1.2Coarser powder in thicker sheets
What ifWhat if the powder has a D90 of 20 μm and is cast into a 1.5 mm silicone sheet?
Claim language“D90 of 8.6 μm or less”
A thixotropic silicone formulation holds the larger particles in suspension during cure. The sheet embeds the coarse fraction throughout its thickness, where the ferrite dissipates microwave energy.
1.2Particle sizing by electrical sensing
What ifWhat if electrical sensing determines D10 and D90 from individual particles suspended in an electrolyte?
Claim language“determined by a laser diffraction method”
Each particle displaces electrolyte as it passes through a sensing aperture, producing an impedance pulse proportional to its displaced volume. Calibrated apertures cover the fine and coarse fractions, and the resulting volume-weighted distribution supplies D10 and D90.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Absorbing liner for microwave moisture gauges
Flexible strips filled with the ferrite powder line the metal sidewalls of a microwave moisture gauge mounted over a grain conveyor. The strips sit outside the direct path between the antenna and the grain bed, with their exposed faces oriented toward the measurement region. The ferrite dissipates part of the microwave energy that strikes the sidewalls, reducing reflected signals that reach the receiving antenna.
Component substitution
Cobalt and titanium substituted barium ferrite
Cobalt replaces manganese in a magnetoplumbite-type barium ferrite with nominal composition BaFe10TiCoO19. Divalent cobalt and tetravalent titanium replace two trivalent iron ions per formula unit and preserve nominal charge balance. Milling and classification set the powder to a D10 of 0.8 μm or less and a D90 of 8.6 μm or less, as measured by laser diffraction. The substituted ferrite supplies magnetic loss when dispersed in a flexible sheet.
Parameter or scale variation
Absorber with graded ferrite loading
A 2.0 mm sheet contains three silicone layers filled with the same ferrite powder. From the incident face to the rear face, the layers have thicknesses of 0.5, 0.5, and 1.0 mm and ferrite volume fractions of 15%, 30%, and 45%, respectively. The three uncured layers are cast in sequence and cured together. The lower loading at the incident face reduces the initial impedance transition, and the higher loading deeper in the sheet increases the amount of magnetic material along the propagation path.
Combination with existing systems
Ferrite cartridges for waveguide terminations
A rectangular waveguide termination contains a tapered dielectric carrier lined on two opposing faces with ferrite-filled strips. The narrow end of the carrier faces the incoming wave, and the wide end sits against a conductive end plate. The taper gradually increases the amount of absorbing material in the waveguide cross section, and the ferrite dissipates energy on both the incoming and reflected paths.
Ferrite cladding for planar transmission lines
A ferrite-filled film mounts over a microwave microstrip board on dielectric spacers. The film overlaps the board perimeter and the gaps between adjacent channels, with openings over the signal traces and tuning elements. Fringing fields that extend into the film lose energy through magnetic dissipation, reducing coupling between neighboring channels. Spacer thickness sets the distance between the ferrite and the traces and controls the loading of the transmission lines.
Automated or data-driven variant
Particle sizing control for powder classification
An automated sampler draws powder from the product outlet of an air classifier and disperses each sample in a laser diffraction analyzer. A controller raises classifier wheel speed when D90 exceeds 8.6 μm and routes the coarse fraction back to the mill. A separate gravimetric feeder meters fines into the product stream when the blended D10 exceeds 0.8 μm. An automated die press measures compact mass and volume at a fixed compaction pressure, and a diverter holds lots that measure below 3.00 g/cm³ for reblending.
Specific version of a part
Strontium ferrite with paired substitutions
Strontium occupies the large cation site in the magnetoplumbite structure, and titanium and manganese replace two of the twelve iron atoms per formula unit in equal proportions. A milled mixture of strontium carbonate, iron oxide, titanium dioxide and manganese oxide reacts during firing to form the ferrite phase.
Barium and strontium site mixture
Barium and strontium occupy the large cation site in a nominal 70:30 molar ratio, with x set to 1.0. The batch uses y = 3.0 and z = 0.50, giving 1.5 titanium atoms and 1.5 manganese atoms per formula unit.
Classified powder with controlled packing
Milling and air classification yield a powder with a laser diffraction D10 of 0.7 μm and D90 of 7.5 μm. Fine particles fill spaces between larger particles during compression, and the compact has a density of 3.1 g/cm³ under the specified test load.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1magnetoplumbite-type ferrite represented by a chemical formula: AxF(12-y)(TizMn(1-z))yO19
With reference to the Z-type ferrite in which cobalt (Co) is substituted by 2 (Co2) includes two molecules per unit cell, and an M-type is laminated by RS and a Y-type is laminated by TS.
A · US 2014/0176380 A1 · ¶ 51
In accordance with one aspect of the present invention, there is provided a ferrite magnetic material comprising a primary phase of a magnetoplumbite-type hexagonal ferrite, the primary phase having a composition represented by formula (I): Ca(1-x-y-z)SrxBayAzFe(2n-m1-m2)Mm1M′m2O19 (I) wherein, A is at least one element selected from rare earth elements including La, Nd, Pr and Sm, and Bi, with La being essentially contained in A;
B · US 10,141,091 B2 · ¶ 12
1.2wherein A is at least one selected from Ba, Sr, Ca, and Pb, x is 0.9 to 1.1, y is 5.0 or less, and z is 0.35 to 0.65, the ferrite particle powder having a compression density of 3.00 g/cm3 or more, and having a D10 of 0.8 μm or less and a D90 of 8.6 μm or less determined by a laser diffraction method.
Therefore, the heat-treated powder is subjected to fine pulverization to obtain a fine powder having a mean particle diameter ranging from 0.3 μm to 0.8 μm.
B · US 10,141,091 B2 · ¶ 40
An empty cell means only that no passage was reproduced there.
Statements in these documents
The present invention relates to a multilayer ferrite sheet, an antenna device using the same, and a manufacturing method thereof, and more particularly, to a multilayer ferrite sheet capable of performing communications in a wideband frequency, an antenna device using the same, and a manufacturing method thereof.
A · US 2014/0176380 A1 · ¶ 3
Thus, an antenna device, which may satisfy the requirements of being used in a wideband or multiple bands and having a small size, is required.
A · US 2014/0176380 A1 · ¶ 9
The present invention relates to a magnetoplumbite-type (hexagonal) ferrite magnetic material having improved magnetic properties, and a segment-type permanent magnet derived therefrom which is used in the manufacture of small type motors for automobiles, motors for electric equipments as well as for home appliances, and other devices.
B · US 10,141,091 B2 · ¶ 2
To meet such demand, there have recently been conducted many studies to develop a permanent magnet having improved magnetic properties in terms of the residual magnetic flux density (Br), intrinsic coercive force (iHc), squareness (Hk/iHc), and maximum energy product (B.Hmax).
B · US 10,141,091 B2 · ¶ 5