Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Vacuum immersion of the blank
What ifWhat if the porous mill blank takes up the magnesium-containing solution while submerged under reduced pressure?
Claim language“painting a surface”
A vacuum chamber removes air from the open pores of the blank before a magnesium nitrate solution floods the chamber. Restoring atmospheric pressure drives the solution into the connected pores, and drying deposits the salt on the pore walls.
1.1Magnesium oxide vapor deposition
What ifWhat if gas-phase deposition supplies magnesium oxide to the porous blank?
Claim language“a magnesium-containing solution”
An atomic layer deposition reactor alternates pulses of a volatile magnesium precursor and water vapor, with inert gas purges between pulses. Extended exposure times allow the reactants to enter open pores and deposit magnesium oxide on accessible pore walls.
1.1Magnesium mixed into powder
What ifWhat if magnesium enters the zirconia powder before the mill blank is formed?
Claim language“painting a surface of a porous yttria-stabilized zirconia mill blank”
An attrition mill disperses fine magnesium oxide powder throughout a slurry of yttria-stabilized zirconia. Spray drying produces granules for pressing, and presintering gives the compact enough strength for milling while retaining open porosity.
1.1Higher yttria content in powder
What ifWhat if higher yttria content controls translucency in a magnesium-free zirconia formulation?
Claim language“a magnesium-containing solution”
The starting powder contains about 5 mol% yttria, which increases the fraction of optically isotropic cubic zirconia after firing. The cubic grains reduce light scattering associated with birefringence, and near-full densification limits scattering from residual pores.
1.2Grinding fully dense zirconia stock
What ifWhat if diamond grinding shapes a restoration from fully densified magnesium-doped zirconia stock?
Claim language“sintering the painted mill blank”
A computer-controlled grinder cuts the finished geometry from dense stock using water-cooled diamond tools. Fine diamond abrasives polish the ground surfaces, and the finished restoration retains the grain structure and density of the stock.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Translucent covers for instrument indicators
A porous yttria-stabilized zirconia blank is milled into an instrument indicator cover with a flat viewing face and a mounting rim. A brush applies an aqueous magnesium acetate solution to the viewing face while a removable mask protects the mounting rim. After drying, the cover is sintered and fitted over a visible-light emitter in the instrument housing.
Component substitution
Magnesium oxide suspension for brush application
An aqueous suspension of submicrometer magnesium oxide particles replaces the magnesium-containing solution. An ammonium polyacrylate dispersant and continuous stirring keep the particles suspended during brushing onto the porous yttria-stabilized zirconia blank. The coating dries before firing, and the sintering cycle includes a low-temperature hold in air to burn out the dispersant before densification.
Parameter or scale variation
Two-pass coating at lower magnesium concentration
An aqueous magnesium acetate solution contains 1.0 wt % elemental magnesium and is applied to a porous zirconia blank stabilized with 3.0 mol % yttria. The target face receives two brush passes of 8 microliters per square centimeter each, with 20 minutes of drying at 60 °C between passes and after the second pass. The furnace ramps at 5 °C per minute to 1450 °C and holds for two hours in air.
Graded magnesium loading across a crown
A porous yttria-stabilized zirconia crown is divided along its height into three equal bands running from the cervical margin to the biting edge. A brush applies a magnesium acetate solution containing 2.0 wt % elemental magnesium at cumulative volumes of 5, 10, and 15 microliters per square centimeter across the three bands, respectively. Each pass delivers 5 microliters per square centimeter where applied, with 15 minutes of drying at 60 °C between passes and after the final pass. The crown is sintered in air at 1450 °C for two hours.
Automated or data-driven variant
Gravimetric control of robotic brush coating
A robot carries a brush supplied by a syringe pump and follows a surface path generated from a scan of the porous yttria-stabilized zirconia blank. A load cell weighs the blank before and immediately after each pass, and the controller divides the wet mass gain by the coated area to estimate solution uptake per unit area. The controller adjusts pump delivery for the next pass until the target uptake is reached, then the blank dries and enters the sintering furnace.
Specific version of a part
Single coat of magnesium nitrate
A fine synthetic brush spreads an aqueous magnesium nitrate solution over the porous face of a presintered yttria-stabilized zirconia blank. Capillary suction draws the liquid below the surface, and warm-air drying leaves magnesium nitrate in the wetted region.
Metered magnesium acetate brush coats
A pipette dispenses a fixed volume of aqueous magnesium acetate solution onto a flat brush for each pass. Two coats applied in perpendicular directions distribute the liquid over the blank face, with drying between coats.
Air firing with burnout dwell
A programmable furnace heats the painted blank in air and holds it near 600 °C to decompose the deposited magnesium salt before substantial pore closure. A subsequent hold near 1,500 °C densifies the zirconia body.
Two-stage zirconia sintering cycle
An electric furnace heats the dried painted blank to a brief peak near 1,500 °C to initiate rapid densification. The furnace then drops to a lower hold near 1,400 °C to continue densification while limiting grain growth.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1painting a surface of a porous yttria-stabilized zirconia mill blank with a magnesium-containing solution; and
Aqueous or alcoholic metal solutions of Fe, Mn, Cr can be used, for example as chlorides or acetates. Milled green prostheses 26 are dipped into the solution or can be brushed for specific tooth shade effects.
B · US 11,051,916 B2 · ¶ 79
1.2sintering the painted mill blank resulting in a sintered ceramic body.
Finally, SSC and SDC powders at a weight ratio of about 7:3 were mixed with a binder (V-006, Heraeus, Germany) and acetone to form a cathode slurry, which was brush-painted on the SDC electrolyte, followed by pre-firing at about 950° C. for about 2 hours to form a porous SSC-SDC cathode.
A · US 2014/0227624 A1 · ¶ 22
When each of the different layers of zirconia body 21, 22, 23, with an increasing amount of Y2O3, was deposited into one body 20, 26, 29 and dipped into a specific color (hue) liquid 31, the subsequently sintered body 32, 33 showed a graded color intensity (chroma).
B · US 11,051,916 B2 · ¶ 105
An empty cell means only that no passage was reproduced there.
Statements in these documents
Thus, a new SOFC configuration based upon a thin film, bi-layer electrolyte membrane (SSZ/SDC) supported by a conventional Ni-YSZ substrate is needed to lower the operating temperature and to improve the performance.
A · US 2014/0227624 A1 · ¶ 6
The SSZ electrolyte film was thin enough (about 1 μm) to reduce the ohimic resistance but thick enough to block the electronic conduction of the SDC electrolyte membrane.
A · US 2014/0227624 A1 · ¶ 7
These fillers are usually crystalline but can also be particles of a higher melting glass.