patent.fyi
Applications  /  US 2026/0356765
United States Patent Application Publication

US 2026/0356765 A1

Published
Nov 12, 2026
Filed
Nov 2, 2023
Earliest date on the face
Nov 2, 2022
Classification
C04B 35/486
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Cubic spinel ceramic

What ifWhat if a cubic magnesium aluminate spinel provides the translucent ceramic body?
Claim language“zirconia, and a stabilizer”

Fine magnesium aluminate spinel powder is compacted and sintered to close the open porosity. Hot isostatic pressing shrinks the remaining pores, and the cubic grains limit scattering from changes in crystal orientation.

1.1Optical reference tile

What ifWhat if a retained zirconia reference tile supplies the comparison value for the short firing?
Claim language“at 1,550 °C for 120 minutes”

The reference tile comes from a previously qualified production lot and has the same nominal thickness, shade, and surface finish as the short-fired specimen. Both specimens are measured over the same white and black backings to obtain the two lightness differences.

1.1Shorter peak temperature hold

What ifWhat if the short firing uses a five-minute hold at 1,600 °C?
Claim language“at 1,550 °C for 10 minutes”

A fine-grained pre-sintered compact with uniform density is heated rapidly in a low-thermal-mass furnace. The higher peak temperature increases the rate of diffusion during the five-minute hold, and a polished coupon provides the optical measurement.

1.1Direct transmission threshold

What ifWhat if a minimum total luminous transmittance determines whether the short-fired ceramic meets the optical requirement?
Claim language“satisfying the formula (1)”

An integrating sphere collects direct and diffuse visible light transmitted through a polished 1.0 mm coupon. The instrument weights the transmitted spectrum by photopic sensitivity, and the resulting value is compared with the minimum established for the application.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Diffuse windows for instrument lighting

A partially sintered stabilized zirconia blank is machined into a flat disk for a backlit instrument panel. The disk is fired at 1,550 °C with a 10-minute peak hold, then ground on both faces to the specified thickness. A retaining ring holds the disk in front of a light source, where it transmits diffuse light through the panel. Witness disks from the same blank are finished to equal thickness and checked for a short-hold to 120-minute white-minus-black lightness difference ratio of at least 0.85.

Component substitution

Zirconia stabilized with cerium oxide

Cerium dioxide serves as the phase stabilizer in place of yttria. A co-precipitated zirconia powder containing 12 mol% cerium dioxide is calcined in air, milled, pressed into blanks and fired to partial consolidation. Matched coupons are then sintered in air at 1,550 °C with peak holds of 10 and 120 minutes and finished to the same thickness and surface roughness. The white-minus-black lightness differences determine whether the short-hold coupon retains at least 85% of the long-hold value.

Parameter or scale variation

Seven-minute hold for thin plates

A partially sintered stabilized zirconia blank is machined with a shrinkage allowance for a final plate thickness of 0.8 mm. The plates rest on flat zirconia setters in a single layer with at least 5 mm between adjacent edges. The furnace holds at 1,550 °C for seven minutes after a thermocouple beside the load reaches the setpoint. Equal-thickness witness plates fired for seven and 120 minutes provide the white-minus-black lightness differences for a retention check at 0.85.

Automated or data-driven variant

Automatic measurement of lightness retention

A motorized fixture places each fired zirconia coupon over white and black backing tiles beneath a reflectance spectrophotometer. A thickness gauge verifies that the 10-minute and 120-minute coupons have the same finished thickness within a preset tolerance, and a barcode reader associates both coupons with the pressing lot. Software records the CIELAB lightness on each backing, subtracts the black-backed reading from the white-backed reading for each coupon and divides the 10-minute difference by the 120-minute difference. The software records whether the ratio reaches 0.85 and flags results with a reference difference below the instrument’s quantification limit.

Combination with existing systems

Rapid firing followed by isostatic pressing

A partially sintered stabilized zirconia blank is fired at 1,550 °C for 10 minutes and checked for closed porosity before transfer to a hot isostatic press. The press holds the fired part in argon at 1,400 °C and 150 MPa for one hour to collapse residual closed pores. Polishing and an air anneal provide a common surface finish and restore oxygen lost during the press cycle. The 10-minute and 120-minute air-fired witness coupons establish lightness retention before pressing, and a separate pressed coupon measures the optical effect of the added step.

Specific version of a part

Yttria stabilized zirconia powder

Zirconia powder contains 5 mol% yttria distributed throughout the particles. Yttrium in solid solution suppresses transformation to the monoclinic phase during cooling from the final sintering temperature.

Matched coupon lightness comparison

Two coupons from the same pre-sintered blank are fired at 1,550 °C with holds of 120 minutes and 10 minutes, then polished to the same thickness and finish. A spectrophotometer measures L* over white and black backings for each coupon, and the short-hold difference divided by the long-hold difference meets the criterion at 0.85 or above.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2010/0041542 A1
Published
Feb 18, 2010
Filed
Dec 28, 2007
Class
C04B 35/48
Document BUS 8,877,664 B2
Published
Nov 4, 2014
Filed
Aug 20, 2010
Class
C04B 35/486
Claim 1
Document A
Document B
1.1zirconia, and a stabilizer capable of preventing a phase transformation of zirconia, and satisfying the formula (1) below when ΔL1*(W−B) related to a first sintered body fabricated by sintering the zirconia pre-sintered body at 1,550 °C for 120 minutes is compared to ΔL2*(W−B) related to a second sintered body fabricated by sintering the zirconia pre-sintered body at 1,550 °C for 10 minutes, ΔL2*(W−B)/ΔL1*(W−B)≥0.85 (1).
sintering the zirconia green body at a temperature no greater than 1200° C. and for a time sufficient to form a partially sintered zirconia green body;
A · US 2010/0041542 A1 · ¶ 36
Therefore, stabilized zirconia and partially-stabilized zirconia (PSZ) have been used, in which the phase transition is inhibited by adding oxide, such as calcium oxide, magnesium oxide, yttrium oxide and cerium oxide, as a stabilizing agent to zirconia.
B · US 8,877,664 B2 · ¶ 3

An empty cell means only that no passage was reproduced there.

Statements in these documents
Therefore, there is a continuing need for ceramic bodies that have both high strength and translucency.
A · US 2010/0041542 A1 · ¶ 3
In one embodiment, there is provided a translucent zirconia sintered body comprised of primary particles and having a density of at least 99 percent of full density, the primary particles having:
A · US 2010/0041542 A1 · ¶ 4
When the partially-stabilized zirconia is heated to 200 degrees Celsius under the existence of water, for example, the phase transition from the tetragonal system to the monoclinic system occurs, and this degrades the strength of the partially-stabilized zirconia (referred as “low-temperature degradation” hereinafter).
B · US 8,877,664 B2 · ¶ 4
Accordingly, an art for manufacturing the zirconia sintered body has been developed to inhibit the low-temperature degradation (see Patent Document 1 and Patent Document 2, for example).
B · US 8,877,664 B2 · ¶ 4
Cite aspatent.fyi, US 2026/0356765 A1, claim 1, first published 2026-11-20T06:49:46-05:00, https://patent.fyi/US20260356765/, SHA-256 3a13ec325e9acbc9037d45f18f37ffacc82ff94464dfb5c2352808efc66e63df
First published
Permanent addresshttps://patent.fyi/US20260356765/
Content fingerprint (SHA-256)3a13ec325e9acbc9037d45f18f37ffacc82ff94464dfb5c2352808efc66e63df
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi