Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Silicon carbide composite substrate
What ifWhat if the coating stack covers a silicon carbide fiber composite with a silicon carbide matrix?
A woven silicon carbide fiber preform carries structural loads, and chemical vapor infiltration deposits silicon carbide around the fibers to form a rigid matrix. Exposed silicon carbide at the surface oxidizes to silica, which slows oxygen transport into the composite.
1.2Boron nitride interface layer
What ifWhat if a crystalline boron nitride undercoat separates the carbon-carbon substrate from the ceramic overcoat?
Claim language“a crystallized metal carbide undercoat”
Chemical vapor deposition forms a thin hexagonal boron nitride film on the carbon-carbon surface. Basal planes oriented along the surface permit interfacial shear and reduce stress transfer during thermal cycling. The continuous ceramic overcoat limits oxygen access to the boron nitride.
1.4Single graded ceramic layer
What ifWhat if the overcoat consists of one crystallized ceramic layer with a continuous composition gradient?
Claim language“a plurality of crystallized ultra-high melting point overcoat layers”
A vacuum plasma spray torch co-deposits zirconium diboride and silicon carbide while the feed system continuously changes their ratio during buildup. The gradient distributes changes in thermophysical properties through the coating thickness without discrete composition boundaries.
1.5Matched properties across layers
What ifWhat if the overcoat layers share the same coefficient of thermal expansion, thermal conductivity, porosity, and thermal stability?
Claim language“have at least one of a different coefficient of thermal expansion, thermal conductivity, porosity, or thermal stability”
Each coat uses the same silicon carbide precursor formulation, hafnium carbide particle loading, and argon heat treatment. Finished layers have matching bulk properties within measurement resolution. Successive wet coats fill surface-connected defects in the preceding coat before pyrolysis, reducing continuous paths through the stack.
1.6Vapor deposited ceramic matrix
What ifWhat if vapor infiltration forms the crystallized ceramic matrix around the refractory ceramic particles?
Claim language“crystallized ultra-high melting point polymer-derived ceramic matrix”
Dry-deposited hafnium carbide particles form a porous bed on the undercoat. Thermal decomposition of methyltrichlorosilane in a hydrogen carrier deposits crystalline silicon carbide on the particle surfaces, bridging adjacent grains and filling the interconnected pores.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Coated setters for ceramic sintering
A carbon-carbon setter supports ceramic parts during pressureless sintering in an argon furnace. A crystalline silicon carbide undercoat covers the setter, and two sequentially fired silicon carbide matrix layers containing zirconium carbide particles cover the undercoat. The inner layer uses a lower particle volume fraction to limit thermal expansion mismatch with the undercoat, and the outer layer uses a higher particle volume fraction to provide a wear surface at the part contact points.
Component substitution
Titanium carbide as refractory filler
Titanium carbide powder replaces the refractory filler in a polycarbosilane slurry applied to a crystalline silicon carbide undercoat on carbon-carbon. The same powder grade is used in both coats, with a higher filler volume fraction in the outer coat to reduce the fraction of material that shrinks during pyrolysis. Each coat is dried and fired separately in argon at 1600 °C to form a crystalline silicon carbide matrix around the titanium carbide particles.
Parameter or scale variation
Thin coating with three fired layers
Three overcoat layers with target fired thicknesses of 25, 35, and 40 micrometers cover a crystalline silicon carbide undercoat on carbon-carbon. Each layer contains zirconium carbide powder with a median particle diameter of 2 micrometers in a polycarbosilane precursor, and the middle layer uses a lower filler volume fraction to produce a higher fired porosity than the face layers. Masked witness coupons establish the wet film thickness needed for each target, and each layer receives a separate argon firing cycle before application of the next coat.
Controlled porosity through vacuum infiltration
Two layers of a zirconium carbide and polycarbosilane slurry are applied and fired separately over a crystalline silicon carbide undercoat on carbon-carbon. After the second layer fires, a shallow bath of dilute polycarbosilane solution contacts its outer face at 10 kilopascals absolute for 5 minutes, followed by a return to atmospheric pressure to drive solution into open pores. A final argon firing at 1600 °C converts the infiltrant to crystalline silicon carbide. A polished witness cross section verifies that the infiltration front stays within the outer layer and that the outer layer has lower porosity than the inner layer.
Combination with existing systems
Coated liners for vacuum hot pressing
A split carbon-carbon liner fits inside a graphite die for vacuum hot pressing of ceramic powder. A crystalline silicon carbide undercoat and two crystalline polymer-derived silicon carbide layers containing zirconium carbide cover the powder-facing bore and exposed edges of each liner segment. The bore-facing layer uses a higher filler loading than the inner layer to limit pyrolysis shrinkage at the wear surface, and the die backs the liner during pressing.
Automated or data-driven variant
Robot spray control using thickness maps
A robot sprays zirconium carbide and polycarbosilane slurries onto a carbon-carbon panel with a crystalline silicon carbide undercoat. After each layer dries, a laser triangulation sensor scans the panel and registers the scan to fixture fiducials so the controller can calculate local thickness from the precoat surface map. The controller adds spray passes to thin areas, then the panel enters an argon furnace for pyrolysis and crystallization. Separate slurry recipes set the filler volume fraction of the inner and outer layers.
Specific version of a part
Needled carbon fiber substrate
Stacked carbon fiber plies are needle punched to carry fibers through the thickness. Chemical vapor infiltration deposits pyrolytic carbon around the fibers, and repeated infiltration densifies the carbon matrix.
Vapor deposited hafnium carbide
Chemical vapor deposition uses hafnium tetrachloride and methane in hydrogen to grow a crystalline hafnium carbide undercoat on the carbon-carbon surface. The deposited film covers exposed fibers and carbon matrix and provides a carbide surface for the overcoat.
Porous inner and dense outer layers
A hafnium carbide filled inner layer receives one precursor application and pyrolysis cycle, leaving open porosity. The outer layer undergoes repeated infiltration with the same preceramic polymer followed by pyrolysis, filling connected pores and lowering its open porosity.
Hafnium carbide in silicon carbide
Hafnium carbide powder is dispersed in an allylhydridopolycarbosilane precursor, and the mixture is applied as a thin coat. Argon pyrolysis converts the polymer to ceramic, and subsequent heat treatment crystallizes the silicon carbide matrix around the hafnium carbide grains.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.2a crystallized metal carbide undercoat on a surface of the carbon-carbon composite substrate; and
In some embodiments, one or more inner layers between the substrate and refractory layer comprise a carbide, nitride, carbonitride, oxycarbonitride, oxide or boride of one or more metallic elements selected from the group consisting of aluminum and metallic elements of Groups IVB, VB and VIB of the Periodic Table.
A · US 2016/0160346 A1 · ¶ 21
1.3an overcoat on a surface of the crystallized metal carbide undercoat,
Alternatively, a plurality of inner layers can collectively achieve thickness of at least 5 CVD of the refractory layer directly on the substrate or on an inner layer can begin with an alumina sublayer or Group IVB metal nitride sublayer.
A · US 2016/0160346 A1 · ¶ 22
1.4wherein the overcoat comprises a plurality of crystallized ultra-high melting point overcoat layers,
Briefly, a coated article described herein comprises a substrate and a coating deposited by CVD adhered to the substrate, the coating including a refractory layer comprising a plurality of sublayer groups, a sublayer group comprising a Group IVB metal nitride sublayer and an adjacent layer alumina sublayer, the Group IVB metal nitride sublayer comprising a plurality of nodules interfacing with the alumina sublayer.
A · US 2016/0160346 A1 · ¶ 3
1.5wherein at least two overcoat layers of the plurality of overcoat layers have at least one of a different coefficient of thermal expansion, thermal conductivity, porosity, or thermal stability,
1.6wherein each of the plurality of overcoat layers comprises a crystallized ultra-high melting point polymer-derived ceramic matrix that includes a plurality of ultra-high melting point refractory ceramic particles,
Parts made of oxide/oxide composite material are generally produced by draping in a mould a plurality of fibrous layers made from refractory oxide fibres, the layers each being previously impregnated with a slurry filled with refractory oxide particles.
B · US 2020/0339480 A1 · ¶ 2
1.7wherein the ultra-high melting point refractory ceramic particles have a melting point of at least about 2400 degrees Celsius (°C), and
In this case, the fibrous layers are made from silicon carbide (SiC) or carbon fibres and are impregnated with a slurry filled with carbide (for example SiC), boride (for example TiB2), silicide (for example MoSi2) or nitride (for example Si3N4) particles.
B · US 2020/0339480 A1 · ¶ 2
1.8wherein an outermost layer of the overcoat comprises an outermost overcoat layer of the plurality of overcoat layers.
The refractory layer comprising the plurality of sublayer groups can be the outermost layer of the coating.
A · US 2016/0160346 A1 · ¶ 23
An empty cell means only that no passage was reproduced there.
Statements in these documents
While effective in inhibiting wear and extending tool lifetime in a variety of applications, refractory coatings based on single or multi-layer constructions of the foregoing refractory materials have increasingly reached their performance limits, thereby calling for the development of new coating architectures for cutting tools.
A · US 2016/0160346 A1 · ¶ 2
In some embodiments, the Group IVB metal nitride sublayer and the adjacent alumina sublayer of a sublayer group are nanolayers.
A · US 2016/0160346 A1 · ¶ 3
Indeed, its removal from the fibrous texture can be tricky and lead to a degradation of the injected fibrous texture.
B · US 2020/0339480 A1 · ¶ 4
Thus, by using a filtration layer that is an integral part of the final composite material part, the problem of removing a filtration element used in the prior art is eliminated.
B · US 2020/0339480 A1 · ¶ 12
Cite aspatent.fyi, US 2026/0356769 A1, claim 1, first published 2026-11-20T06:49:46-05:00, https://patent.fyi/US20260356769/, SHA-256 be07eaa634fb0ce0fdcf17ffb7909fc9c67318342de898369d25597b68aba3aa