1.1Crossflow breakup of molten lithium
A heated feed nozzle injects molten lithium across a pressurized stream of dry heptane. The crossflow breaks the jet into droplets, and a downstream heat exchanger solidifies the droplets before collection.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A heated feed nozzle injects molten lithium across a pressurized stream of dry heptane. The crossflow breaks the jet into droplets, and a downstream heat exchanger solidifies the droplets before collection.
A heated capillary feeds molten lithium into a stirred heptane bath held below the lithium melting point. Solvent flow shears droplets from the capillary tip, and the bath removes heat from each droplet during formation and detachment.
A heated centrifugal disk throws molten lithium into an argon-filled chamber as droplets. The chamber provides flight time for the droplets to solidify, and a sealed hopper collects the dry particles under argon.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A battery materials laboratory uses the melt, stir and cool sequence to prepare lithium particles for contact tests with solid electrolytes. A sealed sieve assembly separates the cooled particles by size under argon, and a vacuum chamber removes residual solvent from the selected fraction. The laboratory presses a weighed portion against a solid electrolyte pellet at a set load and records the impedance of the assembly over time.
An inline helical static mixer replaces the rotating agitator. Separate metering lines feed molten lithium and heated organic solvent into the mixer, where fixed elements divide and redirect the flow to form lithium droplets. Heat tracing keeps lithium molten through the mixer, and back pressure keeps the solvent liquid. A downstream heat exchanger cools the stream and solidifies the droplets before they enter a collection vessel.
A 2 L pressure vessel runs batches at nominal solvent charges of 0.6 L and 1.0 L, measured at room temperature. A height-adjustable impeller sits one impeller diameter below the operating liquid surface in each batch. Each batch uses the same lithium-to-solvent mass ratio and impeller speed. The vessel jacket cools the dispersion, and samples from both batches provide particle size distributions for assessing the effect of fill level.
The cooled dispersion flows to a sealed filter that retains the solid lithium particles. A polishing filter captures entrained particles from the filtrate before the liquid enters a solvent recovery still. The still separates the solvent from higher-boiling residues, and a condenser returns the recovered solvent to an inerted feed tank. A metering pump blends recovered solvent with fresh solvent for the next batch.
A recirculation loop carries cooled slurry through a sealed optical flow cell with a backlight and a camera. Software identifies isolated particle silhouettes and calculates the diameter of a circle with the same projected area as each silhouette. The controller compares the median diameter with a target band and adjusts the impeller speed for the next batch within preset limits.
A radial-blade turbine disperses molten lithium in pressurized liquid n-heptane at about 190 °C. Vertical wall baffles limit bulk rotation, and flow near the blade tips breaks the molten lithium into droplets.
After droplet formation, a recirculating coolant loop removes heat through the vessel jacket. The impeller continues to circulate the solvent as the temperature falls through about 180.5 °C and the lithium droplets solidify.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
The molten lithium metal is then dispersed such as by agitating or stirring vigorously to apply high sheer forces. The dispersion step using high sheer or other equivalent forces is conducted to form uniform droplets or particles of the lithium metal, and to facilitate distributing the droplets or particles in the hydrocarbon oil while avoiding agglomeration.A · US 8,021,496 B2 · ¶ 16
The lithium metal powders disclosed in the above references are formed by dispersing molten lithium metal in an inert medium and cooling the dispersion to below the melting point of the lithium.B · US 8,318,358 B2 · ¶ 128
An empty cell means only that no passage was reproduced there.
The present invention relates to stabilized lithium metal powder (“SLMP”) having better stability and a longer storage life.A · US 8,021,496 B2 · ¶ 2
Such improved SLMP can be used in a wide variety of applications including organo-metal and polymer synthesis, rechargeable lithium batteries, and rechargeable lithium ion batteries.A · US 8,021,496 B2 · ¶ 2
A general need exists to improve the processability of lithium materials for use in batteries for a wide variety of applications.B · US 8,318,358 B2 · ¶ 3
More particularly, better lithium materials are needed for use in polymer electrolyte batteries and thin film structures.B · US 8,318,358 B2 · ¶ 3
patent.fyi, US 2026/0356858 A1, claim 1, first published 2026-11-20T08:11:50-05:00, https://patent.fyi/US20260356858/, SHA-256 fc5660415be73e7f22023fc2640c6f7d57588fccbf02cc50e0580c6395ef06ca