patent.fyi
Applications  /  US 2026/0356987
United States Patent Application Publication

US 2026/0356987 A1

Published
Nov 12, 2026
Filed
Jan 16, 2024
Earliest date on the face
Jan 16, 2023
Classification
C08B 11/12
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Regenerated cellulose feed

What ifWhat if the slurry uses regenerated cellulose as its polymer feed?
Claim language“suspending non-regenerated cellulose”

Wet-mill washed regenerated cellulose into short fibers and disperse them in a water and isopropanol mixture. Sodium hydroxide swells the fibers and activates cellulose hydroxyl groups for carboxymethylation.

1.1Water as the liquid phase

What ifWhat if water is the sole liquid during cellulose alkalization?
Claim language“a mixture of water/alcohol solvent”

Meter concentrated aqueous sodium hydroxide into shredded cellulose in a high-solids kneader to form a moist, workable mass. Control water loading and mix throughout the subsequent etherification to keep the mass workable as the product hydrates.

1.2Concurrent reagent addition

What ifWhat if sodium hydroxide and sodium monochloroacetate feeds start together in the cellulose slurry?
Claim language“then adding”

Meter the two feeds through separate inlets into a vigorously mixed, cooled cellulose slurry so the concentrated streams disperse before they meet. After both feeds finish, warm the slurry to drive etherification.

1.3Mildly alkaline ph endpoint

What ifWhat if acid addition stops at an apparent slurry pH of 8.5?
Claim language“6.0 to 8.0”

Meter dilute acetic acid into the cooled, agitated slurry and stop dosing when a solvent-compatible electrode gives a stable reading of 8.5. Wash the separated solids with aqueous alcohol to extract soluble salts and residual alkalinity while keeping the polymer in the solid phase.

1.4Lower hydroxide feed ratio

What ifWhat if the feed contains 1.9 moles of sodium hydroxide per mole of sodium monochloroacetate?
Claim language“the ratio of alkalizing agent/monohaloacetic acid is above 2”

Use the sodium salt so the hydroxide charge does not have to neutralize free monochloroacetic acid. Limit free water and meter the salt into the mixed alkali cellulose to reduce competing hydrolysis to sodium glycolate.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Binder for waterborne ceramic coatings

Carboxymethyl cellulose from the water and alcohol slurry process serves as a binder in a waterborne ceramic coating. A mixing tank hydrates the dried polymer in water before a disperser incorporates the ceramic powder. A slot die applies the slurry to a porous ceramic substrate, and a dryer removes the water before firing.

Component substitution

Ethanol as the slurry alcohol

An ethanol and water mixture forms the liquid phase for suspending non-regenerated cellulose in a jacketed stirred vessel. The water fraction supplies the liquid needed to dissolve the alkalizing agent and wet the cellulose fibers. After carboxymethylation, an acid feed adjusts the stirred slurry to pH 6.0 to 8.0 before a filter separates the polymer from the solvent.

Acetic acid for slurry neutralization

An aqueous acetic acid solution supplies the acid for neutralizing the slurry after carboxymethylation. A metering pump injects the solution below the liquid surface near the impeller, where agitation distributes it through the slurry. The pump stops when the measured pH stabilizes between 6.0 and 8.0, and a centrifuge separates the solvent from the polymer.

Parameter or scale variation

Timed addition of the etherifying reagent

A metering pump feeds aqueous sodium monochloroacetate into the agitated alkalized cellulose slurry over 30 minutes. The formulation includes the feed water in the total water balance and uses a fixed pump rate that delivers the full reagent charge in that interval. The reactor holds the slurry at the reaction temperature after dosing, then receives acid to bring the pH to 6.0 to 8.0 before solvent separation.

Combination with existing systems

Solvent recovery with rectification and recycle

An enclosed filter sends alcohol-rich filtrate from the neutralized slurry to a collection tank that feeds a rectification column. A condenser collects the alcohol-rich overhead, and dissolved salts leave with the aqueous bottoms. A blend tank combines the recovered solvent with fresh alcohol and water to restore the slurry formulation for the next batch.

Automated or data-driven variant

Automated gel counts on hydrated samples

An at-line inspection station meters a weighed portion of dried carboxymethyl cellulose into water and hydrates it at a fixed solids concentration, mixing speed, and time. A spacer sets the thickness of the hydrated layer in a transparent inspection cell, and a camera records a backlit image of a 5 cm by 5 cm area. Image analysis segments visible particles by contrast, counts connected regions within a calibrated size band, and stores the count with the batch record.

Specific version of a part

Wood pulp in aqueous isopropanol

Disperse shredded dissolving-grade wood pulp in an isopropanol and water mixture. Meter aqueous sodium hydroxide into the stirred suspension and hold it at 20 to 30 °C for alkalization.

Sodium monochloroacetate slurry feed

Disperse powdered sodium monochloroacetate in a portion of the aqueous isopropanol and feed it to the alkalized cellulose under agitation. Heat the mixture to 60 to 70 °C and maintain agitation during etherification.

Acetic acid ph adjustment

Cool the reacted slurry and add dilute acetic acid near the impeller. Reduce the feed rate near pH 7.0 and continue mixing until the slurry reading stabilizes.

Centrifugal solvent removal

After the pH adjustment is complete, spin the slurry in a solvent-tight basket centrifuge fitted with a filter cloth that retains the polymer solids. Collect the aqueous alcohol in a closed receiver and discharge the dewatered cake.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2010/0311964 A1
Published
Dec 9, 2010
Filed
Nov 11, 2008
Class
C08B 11/00
Document BUS 10,875,933 B2
Published
Dec 29, 2020
Filed
Dec 18, 2018
Class
C08B 11/12
Document CUS 2013/0012696 A1
Published
Jan 10, 2013
Filed
Mar 30, 2010
Class
C08B 11/12
Claim 1
Document A
Document B
1.1(a) suspending non-regenerated cellulose in a mixture of water/alcohol solvent, adding an alkalizing agent, and reacting the non-regenerated cellulose with the alkalizing agent in the presence of the water/alcohol solvent, optionally adding hydrogen peroxide,
CMC has been industrially produced by a solvent method in which cellulose is treated and activated with a large amount of an aqueous alkali solution to produce an alkali cellulose (cellulose alkalization) and then the resulting alkali cellulose is dispersed in a water-containing organic solvent to react with a monohaloacetic acid. In the solvent method, a hydrophilic solvent such as isopropanol is used, so that side reactions between the solvent or water and the monohaloacetic acid inevitably occur.
A · US 2010/0311964 A1 · ¶ 3
A method of making non-oxidized, non-regenerated sodium carboxymethyl cellulose (Na-CMC) comprising: alkali treating non-oxidized, non-regenerated Na-CMC by exposing the non-oxidized, non-regenerated Na-CMC to an alkalization agent solution at a first temperature, wherein the alkalization agent solution comprises an alkalization agent, water, and an organic solvent; forming an acid solution comprising a monohaloacetic acid; forming a saturated solution comprising the alkali-t
B · US 10,875,933 B2 · claim 1
1.2(b) then adding a monohaloacetic acid or a salt thereof to the alkalized cellulose of step a), and reacting the alkalized cellulose of step a) with the monohaloacetic acid or the salt thereof,
For example, the base may be added by (i) a method in which after previously mixing the low-crystalline powdery cellulose with the monohaloacetic acid or the like, an aqueous solution of the base is dropped into the resulting mixture; or (ii) a method in which after previously mixing the low-crystalline powdery cellulose with the base, the monohaloacetic acid or the like is added to the resulting mixture.
A · US 2010/0311964 A1 · ¶ 45
The method includes reacting a non-oxidized cellulose with an alkalization agent in the presence of at least one solvent to form an alkali-cellulose, and reacting the alkali-cellulose with at least one of a monohaloacetic acid or a salt thereof to form a cellulose derivative.
B · US 10,875,933 B2 · ¶ 10
1.3(c) adding an acid to the reaction mixture of step b) to adjust the pH of the reaction mixture to 6.0 to 8.0, and
About 50 mL amounts of hydrochloric acid are added to adjust pH of the solution until pH is in the range of about 4 to about 4.5.
B · US 10,875,933 B2 · ¶ 78
1.4(d) removing the solvent after step c) is complete, wherein the ratio of alkalizing agent/monohaloacetic acid is above 2 and wherein the process after step d) is complete does not contain a further step of adding a base to adjust the pH of the reaction mixture and a further step of heat treating the reaction mixture.
For example, in JP 8-245701A and JP 6-199902A, there is described the method of separating and recovering the solvent from a water phase of the reaction system after the cellulose alkalization and the reaction with the etherifying agent, by adding thereto a polar solvent that is hardly compatible with water such as tert-butanol and methyl isobutyl ketone in the reaction.
A · US 2010/0311964 A1 · ¶ 11

An empty cell means only that no passage was reproduced there.

Statements in these documents
Owing to a poor reactivity of the monohaloacetic acid to cellulose, an excessive amount of the monohaloacetic acid must be used for the purpose of attaining a desired substitution degree thereof.
A · US 2010/0311964 A1 · ¶ 3
In addition, the above method has such a large burden that an additional purification step is needed for removing neutralized salts derived from an excessive amount of the alkali used, hydroxymethyl acetic acid salts as by-products, etc., by washing or the like.
A · US 2010/0311964 A1 · ¶ 3
While the absorbency of body fluids and the hemostatic action of currently available carboxylic-oxidized cellulose hemostats are adequate for applications where mild to moderate bleeding is encountered, they are not known to be effective for providing and maintaining hemostasis in cases of severe bleeding, and non-compressional or non-tourniquetable wounds.
B · US 10,875,933 B2 · ¶ 6
The present disclosure describes devices with improved hemostatic properties.
B · US 10,875,933 B2 · ¶ 8
Cite aspatent.fyi, US 2026/0356987 A1, claim 1, first published 2026-11-20T08:53:13-05:00, https://patent.fyi/US20260356987/, SHA-256 f8ad1e826529625fb80a8ee2bf935141fa1d41568714920555d7164ba8b2d9bd
First published
Permanent addresshttps://patent.fyi/US20260356987/
Content fingerprint (SHA-256)f8ad1e826529625fb80a8ee2bf935141fa1d41568714920555d7164ba8b2d9bd