patent.fyi
Applications  /  US 2026/0356993
United States Patent Application Publication

US 2026/0356993 A1

Published
Nov 12, 2026
Filed
Nov 25, 2023
Earliest date on the face
Nov 25, 2022
Classification
C08F 2/50
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Stainless steel mixing vessel

What ifWhat if the porogen solvent is prepared in a stainless steel vessel?
Claim language“in a glass container”

A graduated glass syringe dispenses 6.75 mL of acetonitrile and 0.75 mL of toluene into a stainless steel cup. Gentle swirling combines the two miscible solvents.

1.3Magnetic mixing after addition

What ifWhat if a magnetic stir bar mixes the solution after the template and monomer are added?
Claim language“sonicate the contents for about 15 minutes”

A polytetrafluoroethylene-coated stir bar rotates at 400 rpm for 15 minutes in the capped vessel. The circulating liquid distributes the template and methacrylic acid throughout the porogen.

1.4Argon purge after cross-linker addition

What ifWhat if argon displaces oxygen after the cross-linker is added?
Claim language“purge the glass container with nitrogen gas”

A submerged needle bubbles argon through the mixture for 120 seconds while a second needle vents the headspace. The bubbles strip dissolved oxygen and displace air above the liquid.

1.8Blade coating on substrate

What ifWhat if a gap blade spreads the mixture over the semiconducting surface?
Claim language“is immersed in the pre polymer mixture”

A pipette deposits the mixture at one edge of a horizontal polyaniline-coated slide. A blade set 100 µm above the surface draws the liquid across the slide, and ultraviolet exposure in a nitrogen-filled chamber cures the wet film.

1.9Ultraviolet diode array

What ifWhat if an ultraviolet light-emitting diode array supplies the radiation for photopolymerization?
Claim language“using a 8 W UV bulb”

A 350 nm diode array illuminates the sealed glass vessel at room temperature. A radiometer measures irradiance at the substrate plane so the exposure time can be set to reproduce the radiant dose of the bulb process.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Cured coating headspace monitoring

A flat test chamber holds a coated panel below a polyaniline sensor bearing a molecularly imprinted layer for a residual coating solvent. A spacer keeps the sensor above the panel, and a thermistor measures the chamber temperature. After a fixed equilibration interval, a resistance meter records the sensor response and a calibration curve converts the response to headspace concentration.

Component substitution

Visible light initiation of imprinting

Ethyl phenyl(2,4,6-trimethylbenzoyl)phosphinate replaces the azo initiator in the precursor containing the template, methacrylic acid, ethylene glycol dimethacrylate, and porogen. A glass cover and perimeter spacers confine the nitrogen-purged precursor against the polyaniline-coated substrate. A 405 nm light-emitting diode illuminates the precursor through the cover to cure the film, and a methanol and acetic acid wash extracts the template.

Parameter or scale variation

Spacer controlled thin imprinted films

A polyaniline-coated glass coupon forms the bottom of a casting cell, and a UV-transmitting release sheet forms the top. Perimeter spacers set the wet-film gap to 25, 50, or 100 micrometers, and a fill port admits the nitrogen-purged precursor. After UV curing, the release sheet lifts away and exposes the film for template extraction. Each coupon uses the same electrode geometry for comparing resistance response across the three casting gaps.

Combination with existing systems

Imprinted detector for gas chromatography

A short transfer line connects a gas chromatography column outlet to a low-volume flow cell holding an imprinted polyaniline chip on interdigitated electrodes. A temperature controller holds the cell at a fixed setpoint, and the column carrier gas sweeps separated vapor bands across the film. A resistance logger synchronizes its readings with the injection trigger and records the response by retention time.

Thermal preconcentration ahead of vapor sensing

A sampling pump draws air through a packed tube of porous polymer sorbent while a switching valve isolates the imprinted sensor cell. After sampling, the valve connects the tube to the cell, and a heater releases retained vapor into a low-flow carrier stream that passes over the polyaniline chip. The readout records the peak resistance change during the vapor pulse, and clean carrier gas then flushes the cell before the next sample.

Automated or data-driven variant

Automated calibration with humidity compensation

A flow manifold blends a reference vapor stream with dry and humidified carrier gas and directs the mixture over an imprinted chip and a template-free reference chip. Software steps through preset vapor concentrations and humidity levels, records both chip resistances and measured humidity, and fits a regression using the normalized resistance changes and humidity as inputs. During sampling, the controller applies the stored calibration to estimate vapor concentration and runs a clean-carrier baseline cycle between samples.

Specific version of a part

Ultrasonic bath with vial rack

A 40 kHz water bath sonicates the porogen for 60 seconds. A rack holds the capped glass vial with the bath water above the solvent level and the vial clear of the tank floor.

Bath sonication after purging

The capped glass vial sits in a 40 kHz ultrasonic bath for 10 minutes after the cross-linker addition and nitrogen purge. A recirculating water loop holds the bath at 25 °C.

Ten-minute magnetic stirring

An 8 mm polytetrafluoroethylene-coated stir bar rotates at 350 rpm for 10 minutes after sonication. The vial stays capped during stirring.

Azo initiator under nitrogen

A solids funnel delivers 12 mg of 2,2′-azobisisobutyronitrile to the glass vial under a nitrogen blanket. A magnetic stir bar mixes the contents for 15 minutes under nitrogen to distribute the initiator before substrate immersion.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 10,246,538 B2
Published
Apr 2, 2019
Filed
Sep 2, 2015
Class
C08F 220/18
Document BUS 2022/0105491 A1
Published
Apr 7, 2022
Filed
Dec 15, 2021
Class
B01J 20/268
Claim 1
Document A
Document B
1.1preparing a porogen solvent in an ratio of 6.75 and 0.75 mL v/v, in a glass container;
123.4 mg (about 1 mmoL) of nicotinamide was weighed and placed in a 250 mL round-bottomed flask, mixed and dissolved with 80 mL of methanol-water (the volume ratio of methanol to water is 90:10).
B · US 2022/0105491 A1 · ¶ 45
1.2sonicate the porogen solvent for about 30-90 seconds;
1.3add a mixture containing template volatile organic compound and about 20-30 μL monomer into the glass container and sonicate the contents for about 15 minutes;
123.4 mg (about 1 mmoL) of nicotinamide was weighed and placed in a 250 mL round-bottomed flask, mixed and dissolved with 80 mL of methanol-water (the volume ratio of methanol to water is 90:10). Then 0.9 g of acyl-modified silica gel and 0.34 mL of MAA (4 mmol) were added and sonicated for 30 min.
B · US 2022/0105491 A1 · ¶ 45
1.4add about 110-120 μL cross-linker and purge the glass container with nitrogen gas for about 120 seconds, the ratio of template volatile organic compound, monomer, and cross-linker are kept constant at as n:4:8, wherein ‘n’ ranges about 1-5;
Examples of the bifunctional monomer include, although not particularly limited thereto, ethylene glycol di(meth)acrylate, diethylene glycol di(meth)acrylate, triethylene glycol di(meth)acrylate, tetraethylene glycol dimethacrylate, 1,6-hexanediol di(meth)acrylate, 1,9-nonanediol di(meth)acrylate, glycerin di(meth)acrylate, neopentyl glycol di(meth)acrylate, stearic acid modified pentaerythritol di(meth)acrylate, dicyclopentenyl diacrylate, di(meth)acryloylisocyanurate, and a
A · US 10,246,538 B2 · ¶ 38
A cross-linking agent EGDMA (the molar ratio of the cross-linking agent EGDMA to the functional monomer MAA is 7:1) and AIBN (40 mg) were added to the mixture, and high-purity nitrogen was aerated for 20 min to maintain an inert atmosphere in the flask.
B · US 2022/0105491 A1 · ¶ 45
1.5sonicate the contents for about 10 minutes;
1.6stir the contents for about 10 minutes;
1.7about 10-15 mg of initiator is added to the above content and stirred for about 15 minutes in a nitrogen atmosphere, to obtain a pre polymer mixture;
The present invention relates to a photocurable resin composition containing the following component (A) to component (D): component (A): leuco dye; component (B): photoacid generating agent; component (C): radical polymerizable compound; and component (D): α-hydroxy acetophenone-based radical initiator which has a 5% weight loss temperature (thermal decomposition temperature) in a nitrogen atmosphere of 200° C., or higher as determined by a TGA method at a temperature increa
A · US 10,246,538 B2 · abstract
1.8semiconducting layer coated substrate is immersed in the pre polymer mixture and purged with nitrogen for about 2 minutes before carefully sealing the glass container;
A cross-linking agent EGDMA (the molar ratio of the cross-linking agent EGDMA to the functional monomer MAA is 7:1) and AIBN (40 mg) were added to the mixture, and high-purity nitrogen was aerated for 20 min to maintain an inert atmosphere in the flask. The flask was sealed under the protection of nitrogen, and polymerization was thermally initiated in a 333 K water bath for 24 h.
B · US 2022/0105491 A1 · ¶ 45
1.9the sealed glass container is placed in a UV chamber and photopolymerization is carried out at room temperature at wavelength (λ) of about 350 nm for about 60-100 min using a 8 W UV bulb;
Subsequently, by using an LED illuminator (wavelength: 365 nm), the test specimen was irradiated with ultraviolet light at conditions of 100 mW/cm2×120 seconds to obtain a cured product.
A · US 10,246,538 B2 · ¶ 94
1.10the semiconducting layer coated substrate were removed after about 6-10 min and dried in normal atmospheric conditions;
The obtained material was washed with methanol to neutral, and dried in vacuum at 323 K for 6 h to prepare the nicotinamide dummy template surface molecularly imprinted polymer (DMIP).
B · US 2022/0105491 A1 · ¶ 45
1.11a thick white layer of molecularly imprinted polymer forms on the surface of the semiconducting layer coated substrate in about 5-10 seconds;
If the amount of the modified silica gel is too small, a part of the template molecules and functional monomers will not be polymerized on the surface of the modified silica gel, thus making the imprinting layer thicker and affecting the specific adsorption effect.
B · US 2022/0105491 A1 · ¶ 53
1.12the molecularly imprinted polymer-semiconducting layer coated substrates are immersed in a mixture of about 20-50 μL acetic acid and about 150-200 mL methanol solution, and extracted for about 12 hours using a soxhlet apparatus at about 80-90 °C for the removal of template volatile organic compounds and creation of template-voids; to obtain molecular imprinted over semiconducting layer coated substrate; wherein the porogen solvent is acetonitrile and toluene, 2-methoxyethanol, methanol, chloroform, tetrahydrofuran (THF), dichloroethane, and ionic liquids as 1-Butyl-3 methylimidazolium hexafluorophosphate [BMIM][PF6], 1-Butyl-3 methylimidazolium tetrafluoroborate [BMIM][BF4], 1-Methyl-3-octyl-imidazolium-hexafluorophosphate [OMIM][PF6], 1-Hexyl-3-methyl-imidazolium-hexafluorophosphate [HMIM][PF6], wherein the substrate is selected from ceramic alumina, glass slides, fabrics, fluorine doped tin oxide substrates, indium doped tin oxide substrates, flexible polymer substrates.
Using V (methanol) and V (acetic acid)=9:1 as a solvent, the template was removed by Soxhlet extraction.
B · US 2022/0105491 A1 · ¶ 45

An empty cell means only that no passage was reproduced there.

Statements in these documents
However, since most of active energy ray such as ultraviolet light is absorbed by carbon black while the concealability is obtained, there is a problem that an occurrence of a poor curability is caused if the pigment concentration is excessively high.
A · US 10,246,538 B2 · ¶ 2
The present invention is devised under the circumstances described above, and an object of the invention is to provide a photocurable resin composition which allows obtainment of a cured product with high concealability, while being suppressed in fading due ultraviolet light, a cured product of the composition, and a method for producing the cured product.
A · US 10,246,538 B2 · ¶ 5
However, in order to reduce the loss of tea polyphenols in the process of pesticide removal and ensure the quality and purity of final products, it is necessary to choose a material with high selectivity to imidacloprid and acetamiprid.
B · US 2022/0105491 A1 · ¶ 2
Dummy template molecular imprinting is a technology that can effectively avoid template leakage.
B · US 2022/0105491 A1 · ¶ 3
Cite aspatent.fyi, US 2026/0356993 A1, claim 1, first published 2026-11-20T08:53:13-05:00, https://patent.fyi/US20260356993/, SHA-256 c94732093c21029f995224c0505f64d8be17a8f27ddde2bc209d708ef0c51b3c
First published
Permanent addresshttps://patent.fyi/US20260356993/
Content fingerprint (SHA-256)c94732093c21029f995224c0505f64d8be17a8f27ddde2bc209d708ef0c51b3c
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi