1.1Acrylate groups accept thiols
A tertiary amine catalyzes thiol addition across the carbon–carbon double bonds of a multifunctional acrylate at room temperature. A multifunctional thiol links the acrylate molecules into a crosslinked binder.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A tertiary amine catalyzes thiol addition across the carbon–carbon double bonds of a multifunctional acrylate at room temperature. A multifunctional thiol links the acrylate molecules into a crosslinked binder.
A liquid aliphatic diamine reacts with a difunctional epoxy resin after mixing at room temperature. Its primary amines open epoxide rings, and the resulting secondary amines react with additional epoxide groups to build the network.
A rotor–stator mixer disperses air into the mixed resin, and a silicone surfactant stabilizes the bubbles during application. The epoxy–thiol reaction gels the coating at room temperature and fixes the cellular structure.
A water-in-resin emulsion uses a compatible surfactant and a high volume fraction of water to form closely packed droplets. The continuous epoxy–thiol phase gels at room temperature, and drying then removes water through connected pore openings.
A thin cured polymer layer limits the distance heat travels through the resin to the aluminum backing. The continuous backing spreads heat along the panel and conducts it to a heat sink attached at the edge.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A two-part epoxy and polythiol paste contains boron nitride powder and thermally expandable polymer microspheres. The mixed paste fills the annular clearance between a removable metal mold insert and a temperature-controlled holder. The epoxy and polythiol react at room temperature, and a subsequent heating cycle expands the microspheres while the insert remains clamped in place. The boron nitride conducts heat across the liner during mold operation.
Surface-treated aluminum nitride powder replaces the conductive filler in a two-part epoxy and polythiol formulation containing thermally expandable polymer microspheres. The powder is dispersed in the epoxy side before the microspheres are folded into the paste at low shear. A static mixer combines the two parts and dispenses the paste into a shallow mold, where the epoxy and polythiol react at room temperature. Heating expands the microspheres against the mold stops, and the aluminum nitride conducts heat through the electrically insulating pad.
Expandable graphite flakes serve as the thermally expandable material in a two-part epoxy and polythiol coating with silicon carbide powder as the conductive filler. The silicon carbide is dispersed into the epoxy side, and the graphite flakes are folded in at low shear to preserve their structure. The two parts are mixed, spread on a metal panel, and reacted at room temperature. During heating, the graphite flakes expand through the coating thickness as gas forms between their layers.
A room-temperature-reactive epoxy and polythiol paste contains alumina powder and thermally expandable polymer microspheres. A dispenser lays parallel beads on 8 mm centers, with nominal bead heights of 0.8 mm in shallow regions and 1.4 mm in deeper regions. A mating plate seats against hard stops that set local gaps of 1.0 mm and 1.7 mm. After the paste gels at room temperature, the clamped assembly heats to the microsphere activation temperature, and bead expansion closes the remaining clearance.
A bolted liquid cold plate receives a two-part epoxy and polythiol interface paste loaded with alumina powder and thermally expandable polymer microspheres. The mixed paste is dispensed between the cold plate base and a metal heat spreader, and shoulder bolts set the bond line. The epoxy and polythiol react at room temperature before a controlled heating cycle expands the microspheres into residual gaps. During operation, the alumina conducts heat from the spreader into the cold plate, where circulating coolant carries it away.
A laser displacement sensor maps a baseplate against a fixture datum, and software subtracts this profile from the height map of the mating surface to calculate local gap depths. A gantry feeds a room-temperature-reactive epoxy and polythiol formulation containing boron nitride and thermally expandable microspheres through a static mixer. The controller selects the dispense volume per unit length from a calibration table that relates gap depth to bead volume and measured expansion. A fixture holds the mating surface in position through ambient gelation and the heating cycle that activates the microspheres.
A bisphenol A diglycidyl ether resin supplies terminal epoxide groups at both ends of the principal resin molecule. Thiolate opens the epoxide rings to form thioether bonds and pendant hydroxyl groups.
Pentaerythritol tetrakis(3-mercaptopropionate) supplies four terminal thiol groups per molecule. These groups connect multiple epoxy molecules as the mixture cures and form junctions in the polymer network.
Microspheres contain a volatile hydrocarbon within a thermoplastic shell. Heating raises the internal vapor pressure and softens the shell, allowing the microspheres to expand while the surrounding resin remains deformable.
The resin contains two size fractions of spherical alumina, with median diameters near 3 and 30 micrometers. The smaller particles occupy gaps between larger particles, increasing the packing density and reducing the thickness of resin between conductive particles.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Generally, the epoxide composition utilized to form the mixture for the mercaptan-crosslinked epoxy adhesive comprises an epoxide having at least two epoxide groups; or alternatively, comprises epoxide molecules having an average of at least two epoxide groups per epoxide molecule.A · US 2007/0112100 A1 · ¶ 51
A bio-based epoxy resin obtained from a reaction mixture comprising a glycidyl ether component and a bio-based component comprising a fatty acid and a rosin acid, wherein the glycidyl ether component comprises at least two epoxide groups.B · US 2021/0139640 A1 · abstract
Mercaptanized soybean oil was prepared having about 8.6 wt. % mercaptan sulfur and a functionality of about 2.6. The prepared mercaptanized soybean oil was evaluated for use as an epoxy polymer crosslinking agent as a function of epoxy resin type, catalyst type, catalyst concentration, cure profile, and solvent, as shown in Table 6.A · US 2007/0112100 A1 · ¶ 226
Curing agents can have active hydrogen atoms that react with epoxy groups of the epoxy resin to form an extended or cross-linked resin. The active hydrogen atoms can be present in functional groups comprising primary or secondary amines, phenols, thiols, carboxylic acids, or carboxylic acid anhydrides.B · US 2021/0139640 A1 · ¶ 57
In an embodiment, including a solvent with the thiol ester composition and/or the epoxide composition lowers the temperature needed to cure the mercaptan-hardened epoxy polymer or can even allow the mercaptan-hardened epoxy polymer to cure at ambient temperature.A · US 2007/0112100 A1 · ¶ 65
An empty cell means only that no passage was reproduced there.
The polymer compositions of the present invention have desirable physical properties that make the compositions useful in various applications.A · US 2007/0112100 A1 · ¶ 7
In some embodiments, the two substrates can be the same material; or alternatively, the two substrates can be different materials.A · US 2007/0112100 A1 · ¶ 10
Epoxy resins are useful in the manufacture of articles and components for a wide range of applications, such as adhesives, coatings, laminates, castings, encapsulations and moldings.B · US 2021/0139640 A1 · ¶ 5
There accordingly remains a need in the art for bio-based epoxy resins that provide improved mechanical strength and thermal stability while, maintaining good toughness and flexibility.B · US 2021/0139640 A1 · ¶ 8
patent.fyi, US 2026/0357005 A1, claim 1, first published 2026-11-20T08:53:13-05:00, https://patent.fyi/US20260357005/, SHA-256 610425b163eb8ac68f25981b3f85cd86d7de538a55f42aadbd76eb8861702abf