patent.fyi
Applications  /  US 2026/0357008
United States Patent Application Publication

US 2026/0357008 A1

Published
Nov 12, 2026
Filed
Jul 8, 2024
Earliest date on the face
Nov 6, 2023
Classification
C08G 69/28
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Sebacic acid polyamide matrix

What ifWhat if the matrix uses polyamide 510 made from 1,5-pentanediamine and sebacic acid?
Claim language“a polyamide 56 polymer”

Melt polycondensation forms chains with ten-carbon diacid residues and releases water. A small excess of sebacic acid supplies carboxyl termini that react with an exocyclic amino group of benzoguanamine.

1.1Hexamethylene adipamide matrix

What ifWhat if the matrix uses polyamide 66 made from 1,6-hexanediamine and adipic acid?
Claim language“a polyamide 56 polymer”

An aqueous hexamethylenediammonium adipate salt feed supplies the monomers for melt polycondensation. A small excess of adipic acid supplies carboxyl termini for reaction with benzoguanamine during finishing.

1.1Aromatic polyester matrix

What ifWhat if the matrix uses polybutylene terephthalate with benzoguanamine attached through a terminal amide bond?
Claim language“a polyamide 56 polymer”

Polycondensation of terephthalic acid and 1,4-butanediol produces a polyester backbone. An activated carboxyl terminus reacts with an exocyclic amino group of benzoguanamine to form the terminal amide bond.

1.2Phosphinate dispersed in the melt

What ifWhat if dispersed aluminum diethylphosphinate provides flame retardancy in polyamide 56 with uncapped chain ends?
Claim language“end-capped with benzoguanamine”

Twin-screw extrusion disperses aluminum diethylphosphinate particles throughout the molten polyamide. During burning, the phosphinate releases phosphorus-containing species that inhibit gas-phase combustion reactions.

1.2Melamine cyanurate particle dispersion

What ifWhat if melamine cyanurate particles provide flame retardancy in polyamide 56 with uncapped chain ends?
Claim language“end-capped with benzoguanamine”

Melt compounding disperses powdered melamine cyanurate through the polyamide matrix. Heat absorption and gas release during decomposition reduce the heat available to sustain burning.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Braided sleeves for electrical wiring

A melt spinner extrudes dried benzoguanamine-end-capped polyamide 56 through a multifilament die. Air cools the filaments, and heated rolls draw them before winding. A tubular braider interlaces the yarns around a removable mandrel to form a flexible sleeve that slides over a wire bundle.

Component substitution

Acetoguanamine as the terminal modifier

Acetoguanamine replaces benzoguanamine as the amino-functional triazine in a polyamide 56 formulation. A small molar excess of adipic acid supplies carboxyl end groups during condensation with 1,5-pentamethylenediamine. The acetoguanamine charge stays below the measured molar amount of carboxyl ends, and an exocyclic amino group forms an amide bond with a carboxyl end. End-group analysis measures the remaining carboxyl groups, and size-exclusion chromatography tracks chain coupling through the second exocyclic amino group.

Parameter or scale variation

Cast films at three thicknesses

A flat-die extruder feeds dried benzoguanamine-end-capped polyamide 56 onto a chilled roll to produce films with nominal thicknesses of 50, 100, and 200 micrometers. At constant melt delivery and film width, the take-up speeds for the three thicknesses start at a ratio of 4 to 2 to 1. A thickness gauge downstream of the chill roll measures the cooled film, and the take-up speed is adjusted to reach each target.

Combination with existing systems

Glass fabric laminates with polyamide matrix

Films of benzoguanamine-end-capped polyamide 56 alternate with woven glass plies that carry a polyamide-compatible sizing. A heated platen press raises the stack above the polyamide melting point and forces the melt into the fabric under pressure. The press maintains pressure during cooling so the matrix solidifies around the fibers and binds the plies.

Extruded jackets for electrical cables

A crosshead extruder applies benzoguanamine-end-capped polyamide 56 over a bundle of individually insulated conductors. A guide tip centers the bundle in an annular die, and a haul-off sets the line speed relative to melt delivery to control jacket thickness. A water trough cools the jacket before a diameter gauge checks the finished cable.

Automated or data-driven variant

Sensor control of condensation endpoint

A stirred reactor condenses 1,5-pentamethylenediamine and adipic acid with benzoguanamine and removes water through a condenser. Temperature and agitator torque sensors feed a controller that estimates melt viscosity from a calibration at fixed agitator speed. After the reactor reaches the finishing temperature, the controller holds the selected vacuum until the estimated viscosity stays within the target band for a programmed dwell time. The controller then breaks the vacuum with dry nitrogen and opens the melt discharge valve.

Specific version of a part

Aqueous salt feed polymerization

Mix equimolar 1,5-pentanediamine and adipic acid in water to form pentamethylenediammonium adipate. Heat the salt solution under pressure, then reduce pressure to remove water and drive melt polycondensation.

Solid state molecular weight increase

Granulate a polyamide 56 prepolymer that retains amine and carboxyl termini. Heat the granules below their melting temperature under dry nitrogen to remove water and increase molecular weight by further condensation.

Benzoguanamine in the monomer feed

Charge 1,5-pentanediamine, adipic acid, and benzoguanamine in the same batch. During polycondensation, an exocyclic amino group on benzoguanamine reacts with a carboxyl chain end to form a terminal amide linkage.

Benzoguanamine added during melt finishing

Prepare a polyamide 56 oligomer with a small molar excess of adipic acid to supply carboxyl termini. Meter benzoguanamine into the stirred oligomer melt, then reduce pressure to remove water as terminal amide bonds form.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2014/0303328 A1
Published
Oct 9, 2014
Filed
Jun 12, 2014
Class
C07D 307/89
Document BUS 2022/0282404 A1
Published
Sep 8, 2022
Filed
Jan 15, 2020
Class
D01F 6/60
Document CUS 2006/0058432 A1
Published
Mar 16, 2006
Filed
Jan 12, 2005
Class
C08K 5/49
Claim 1
Document A
Document B
1.1a polyamide 56 polymer
Monomers typically used to obtain such aliphatic oligo- or polyamide as condensation co-polymers comprises aliphatic diamines such as, hexamethylene diamine, pentamethylene diamine, 2,2,4-trimethyl-hexamethylene diamine, 2,4,4-trimethyl-hexamethylene diamine, 1,4-diaminobutane, and aliphatic di-carboxylic acids such as, oxalic acid, maloic acid, adipic acid, sebacic acid.
A · US 2014/0303328 A1 · ¶ 83
The raw materials for producing the polyamide 56 fiber comprise 1,5-pentane diamine and adipic acid, or a polyamide 56 resin obtained by polymerizing 1,5-pentane diamine monomer and adipic acid monomer; wherein the polyamide 56 fiber has a shrinkage in boiling water of 9% or less, wherein the polyamide 56 fiber comprises a polyamide 56 pre-oriented yarn with a low shrinkage in boiling water and a polyamide 56 draw textured yarn with a low shrinkage in boiling water.
B · US 2022/0282404 A1 · abstract
1.2wherein at least one end group of the polyamide 56 polymer is end-capped with benzoguanamine.
Furthermore, not only oligo- or polyamides may be end-capped via melt mixing with a cross-linkable aromatic carboxylic acid anhydride comprising a carbon-carbon triple bond.
A · US 2014/0303328 A1 · ¶ 96

An empty cell means only that no passage was reproduced there.

Statements in these documents
The present invention refers to novel cross-linkable end-cappers for oligomers and polymers comprising primary amino groups, such as oligo- and polyamides and oligo- and polyimides, and for oligomers and polymers comprising hydroxyl groups, such as oligo- and polyesters, which end-cappers comprise carbon-carbon triple bonds.
A · US 2014/0303328 A1 · ¶ 2
However, as well known within the art, aliphatic polyamides, such as various types of nylon, are less thermo stable and would degrade at temperatures typically used to cross-link PEPA.
A · US 2014/0303328 A1 · ¶ 8
A first object of the present invention is to provide a polyamide 56 fiber with a low shrinkage in boiling water, and meantime having good mechanical properties and dyeing uniformity.
B · US 2022/0282404 A1 · ¶ 4
The aforementioned polyamide 56 fiber with a low shrinkage in boiling water is used in knitted and woven fabrics, and is used in such fields as underwears, shirts, suits, down jackets, outdoor jackets, socks, bags and suitcases, curtains, shoe materials, embroidery threads, labels, sofa-covers, uniforms, sportswears, and elastic tapes.
B · US 2022/0282404 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0357008 A1, claim 1, first published 2026-11-20T08:53:13-05:00, https://patent.fyi/US20260357008/, SHA-256 5d937fb7a328703a677d992c245a8ead428e600431c9ea939fd0d5850b71d0f7
First published
Permanent addresshttps://patent.fyi/US20260357008/
Content fingerprint (SHA-256)5d937fb7a328703a677d992c245a8ead428e600431c9ea939fd0d5850b71d0f7
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi