1.1Sulfur bound to cyclized polyacrylonitrile
Heating polyacrylonitrile with elemental sulfur forms a conjugated polymer backbone with covalently bound sulfur. The sulfur reacts with lithium during discharge and is reoxidized during charging.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Heating polyacrylonitrile with elemental sulfur forms a conjugated polymer backbone with covalently bound sulfur. The sulfur reacts with lithium during discharge and is reoxidized during charging.
Molten sulfur fills the pores of a conductive carbon scaffold by capillary action. The carbon supplies an electron path and provides internal volume for lithium sulfide deposition during discharge.
Molten selenium infiltrates a porous triazine polymer, which is mixed with conductive carbon to form the positive electrode. Selenium converts to lithium selenide during discharge and is regenerated during charging.
Molten sulfur enters the micropores of the triazine polymer by capillary action. Narrow pore openings restrict the transport of dissolved polysulfides into the bulk electrolyte, and conductive carbon supplies an electron path.
Elemental sulfur occupies a porous carbon network in contact with triazine polymer particles. During discharge, exposed nitrogen sites coordinate lithium ions in dissolved lithium polysulfides and retain the intermediates near the conductive carbon.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Disperse triazine polymer powder bearing covalently grafted sulfur in a porous polyvinylidene fluoride bead matrix. Pack the beads between retaining screens in a water treatment column. Pass water containing dissolved mercury ions through the bed, where the ions coordinate with accessible sulfur sites. Track mercury concentration in the outlet to determine when to replace the bed.
Deposit a thin composite film of sulfur-grafted triazine polymer and a porous binder on the active face of a quartz crystal microbalance. Mount a second crystal with a binder-only film in the same flow cell as a reference. Pass a gas sample over both crystals so mercury vapor binds to accessible sulfur sites and increases the mass of the active film. Use the difference in frequency shifts to measure uptake against a calibration curve recorded at the same temperature and flow rate.
Use poly(4-vinylpyridine) as the polymer backbone in place of the triazine polymer. React a fraction of the pyridine nitrogens with 2-bromoethyl methyl disulfide in a polar aprotic solvent to form pendant pyridinium groups bearing covalently tethered disulfides. Precipitate and wash the polymer to remove unreacted reagent, then dry it under vacuum. The pyridinium groups anchor the disulfide side chains through two-carbon linkers.
Disperse triazine polymer powder bearing covalently grafted sulfur in a waterborne acrylic binder and apply the slurry to a ceramic honeycomb with 2 mm channels. Mask the downstream section during coating so that only the first 20 mm of each channel receives a 25 to 50 micrometer dry coating. Pass the process stream through the channels so it contacts the sulfur-bearing film along the inlet section. Install multiple honeycombs in parallel to increase throughput while keeping the channel dimensions and coating thickness fixed.
Place a cartridge of porous granules containing sulfur-grafted triazine polymer downstream of an iminodiacetate ion-exchange bed. The upstream bed captures dissolved copper and nickel before the stream reaches the sulfur sites in the downstream cartridge. The downstream cartridge captures residual dissolved mercury. Fit sample ports between the beds and after the cartridge to measure the contribution of each stage.
Charge triazine polymer powder and elemental sulfur into a stirred, jacketed reactor under nitrogen. A controller holds the reaction temperature and logs agitator torque while an automated sampler withdraws aliquots for analysis. A sampling station extracts free sulfur and measures the sulfur retained in the washed solids by combustion analysis. The controller starts cooling when the retained sulfur reaches a target calibrated against batches with independently verified grafting.
Cyclotrimerization of an aromatic dinitrile yields a crosslinked triazine framework. Elemental sulfur melts at about 115 °C and infiltrates the accessible pores during heating at 155 °C.
Wet milling disperses elemental sulfur and triazine polymer powder in a volatile solvent. Solvent evaporation yields a composite powder that is blended with carbon black and a binder for electrode coating.
A base converts pendant thiols on the triazine polymer to thiolate groups. These groups open elemental sulfur rings and form polysulfide chains tethered to the polymer through sulfur–sulfur bonds.
A soluble alkali-metal polysulfide displaces chloride at chlorotriazine sites on the polymer and forms carbon–sulfur bonds. Reaction at both ends of a polysulfide chain creates a sulfur bridge between two triazine sites.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Illustrative embodiments of the invention include compositions of matter comprising graphitic carbon nitride combined with Sulfur, a nonporous conductive carbon nanoparticles (e.g. ones having an average diameter between 80 nanometers and 10 micrometer), and a polymeric material so as to form a composite.B · US 2016/0233487 A1 · ¶ 12
The sulfur in relatively small size is the poly-sulfur groups covalently bonded with the PPY matrix.A · US 2014/0186717 A1 · ¶ 43
In certain embodiments of the invention, the graphitic carbon nitride is doped with at least one of: Sulfur, Carbon, Phosphorus, or Boron.B · US 2016/0233487 A1 · ¶ 12
An empty cell means only that no passage was reproduced there.
Thus, an irreversible loss of sulfur is induced, thereby decreasing a capacity of the lithium ion battery.A · US 2014/0186717 A1 · ¶ 5
What is needed, therefore, is to provide a sulfur composite lithium ion battery having a large utilization of the sulfur.A · US 2014/0186717 A1 · ¶ 6
The instant disclosure describes graphitic carbon nitride (g-CN) materials that can be used as solid state redox catalysts for electrochemical reactions such as those involved in the Lithium-sulfur (Li/S) battery electrochemical couple.B · US 2016/0233487 A1 · ¶ 6
These g-CN materials can further act as a sorbent to bind soluble polysulfides, thereby limiting their bulk diffusion into the electrolyte.B · US 2016/0233487 A1 · ¶ 6
patent.fyi, US 2026/0357011 A1, claim 1, first published 2026-11-20T08:53:13-05:00, https://patent.fyi/US20260357011/, SHA-256 3b349bb7cf4b257bbe868d7b0a92492635ff2d51b2e173b6b7512ac75e4b815e