Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Self-condensing amino anhydride
What ifWhat if a single monomer bearing one primary amine and one cyclic anhydride supplies both reactive groups?
Claim language“a diamine compound-containing first component”
The primary amine of 4-(4-aminophenoxy)phthalic anhydride opens the anhydride ring of another molecule, forming an amic acid linkage. Repeated ring opening builds a polyamic acid, which is cast and heated to form imide rings.
1.1Tetracarboxylic acid diester precursor
What ifWhat if an aromatic tetracarboxylic acid diester supplies the groups that react with the diamine?
Claim language“a tetracarboxylic dianhydride-containing second component”
A pyromellitic acid diethyl ester with two free carboxyl groups is mixed with an aromatic diamine to form a castable precursor. Heating the cast layer drives condensation and ring closure, releasing ethanol and water as imide rings form.
1.2Vapor deposition of monomers
What ifWhat if separate monomer vapors carry the reactants to the film surface?
Claim language“a solvent”
Separate heated sources deliver pyromellitic dianhydride and 4,4′-oxydianiline vapors to a cooler substrate under vacuum. The monomers condense and react on the surface to form a precursor layer, which is heated to close the imide rings.
1.3Single solvent casting medium
What ifWhat if one liquid dissolves the monomers and carries the polymer precursor through casting?
Claim language“a mixed solvent comprising two or more solvents”
Dry N,N-dimethylacetamide dissolves 4,4′-oxydianiline and serves as the reaction medium when pyromellitic dianhydride is added. The resulting polyamic acid solution is cast, dried to remove the solvent, and heated to form a polyimide film.
1.4Lactone and sulfone medium
What ifWhat if a cyclic ester supplies the second liquid in a sulfone-based reaction medium?
Claim language“an amide-based solvent”
Gamma-butyrolactone and sulfolane form a polar medium for reacting an aromatic diamine with a fluorinated aromatic dianhydride to produce a polyamic acid. The solution is cast and dried in stages, with reduced pressure helping remove the high-boiling liquids before final imidization.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Electrical insulation for motor slots
An aromatic diamine reacts with an aromatic tetracarboxylic dianhydride in a mixture of N,N-dimethylacetamide and sulfolane to form a polyamic acid casting solution. A doctor blade spreads the solution on polished stainless steel, and staged heating removes the solvents and converts the precursor to polyimide. The resulting film is released, cut into strips, folded into channels, and inserted into motor stator slots before the windings are installed.
Component substitution
Phosphoryl cosolvent in place of sulfolane
Triethyl phosphate replaces sulfolane as the cosolvent in a liquid phase containing 90 percent N,N-dimethylacetamide and 10 percent triethyl phosphate by mass. The diamine dissolves in the dry solvent blend, and the tetracarboxylic dianhydride is added in portions under nitrogen to form polyamic acid. The precursor solution is cast on glass, dried in stages, and held under vacuum before the final high-temperature imidization step.
Parameter or scale variation
Two thicknesses from one formulation
A polyamic acid solution at 15 percent solids by mass is prepared from an aromatic diamine and an aromatic tetracarboxylic dianhydride in an 85:15 mass blend of N,N-dimethylacetamide and sulfolane. A metered coating head deposits wet layers of 100 and 250 micrometers on separate areas of the same glass carrier. Both layers receive the same staged drying and imidization cycle, and a contact gauge measures the cured thickness of each layer after release.
Metered dianhydride addition during batch mixing
A jacketed vessel holds a diamine dissolved in dry N,N-dimethylacetamide and sulfolane at 15 to 20 degrees Celsius under nitrogen. A gravimetric feeder adds the tetracarboxylic dianhydride in ten equal portions at three-minute intervals, with the total charge set at one mole of dianhydride per mole of diamine. The agitator runs throughout the addition and for four hours afterward, and the resulting polyamic acid solution passes through a 10-micrometer filter before casting.
Combination with existing systems
Polyimide casting on a moving belt
A continuous casting line meters a filtered polyamic acid solution prepared from a diamine and a tetracarboxylic dianhydride in N,N-dimethylacetamide and sulfolane through a slot die onto a moving stainless steel belt. An enclosed drying tunnel removes enough solvent for the supported layer to form a self-supporting web. The web peels from the belt, enters a tenter oven that grips its edges during final drying and imidization, and winds onto a take-up roll.
Automated or data-driven variant
Sensor control of coating viscosity
A stirred vessel holds a polyamic acid solution prepared from a diamine and a tetracarboxylic dianhydride in N,N-dimethylacetamide and sulfolane. A recirculating loop passes the solution through an inline viscometer and a temperature sensor upstream of the coating head. When the temperature-corrected viscosity exceeds its setpoint, a controller adds a metered dose of the original solvent blend, allows time for mixing, and repeats the measurement before releasing the solution to the coater.
Specific version of a part
Dry polar reaction medium
Dry N,N-dimethylacetamide dissolves the aromatic diamine before the dianhydride is added. The higher-boiling cosolvent is dried separately before blending to limit hydrolysis of the anhydride groups.
Two liquids with staged drying
A mixture of 80 parts N,N-dimethylacetamide and 20 parts sulfolane by mass carries the polyamic acid during casting. An initial drying stage removes much of the lower-boiling amide, and a hotter stage removes residual solvent.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a polymerizable component comprising a diamine compound-containing first component and a tetracarboxylic dianhydride-containing second component; and
When a prepolymer of the polyimide precursor having a terminal amino group is produced, each monomer may be added to the aqueous solvent, for example, at a blending ratio such that the molar equivalent of the diamine compound is higher than the molar equivalent of the second tetracarboxylic dianhydride.
A · US 9,505,886 B2 · ¶ 145
As for a water-soluble polyimide precursor, Patent Literature 1, for example, proposes a process for producing an aqueous polyamide acid salt solution composition, comprising polymerizing a tetracarboxylic dianhydride and a diamine in an organic solvent, to provide a polyamide acid;
B · US 11,407,857 B2 · ¶ 6
1.2a solvent,
A method for producing an aqueous polyimide precursor solution composition includes forming a polyamic acid by the reaction of a tetracarboxylic acid component and a diamine component in an aqueous solvent together with an imidazole in an amount of 1.6 mole or more per mole of the tetracarboxylic acid component of the polyamic acid.
B · US 11,407,857 B2 · abstract
1.3wherein the solvent comprises a mixed solvent comprising two or more solvents, and
A polyimide precursor composition includes a polyimide precursor including a condensation polymer of a tetracarboxylic dianhydride containing a first tetracarboxylic dianhydride having a benzene ring to which two carboxylic anhydride groups are bonded, and a second tetracarboxylic dianhydride other than the first tetracarboxylic dianhydride, and a diamine compound; and a first aqueous solvent containing water and at least one water-soluble organic solvent selected from the gr
A · US 9,505,886 B2 · abstract
1.4wherein the mixed solvent comprises an amide-based solvent and a sulfone-based solvent.
Examples of the organic solvent include N,N-dimethylformamide, N,N-dimethylacetamide, N, N-diethylacetamide, N-methyl-2-pyrrolidone, N-ethyl-2-pyrrolidone, 1,3-dimethyl-2-imidazolidinone, N-methylcaprolactam, hexamethylphosphoric triamide, 1,2-dimethoxyethane, bis(2-methoxyethyl)ether, 1,2-bis(2-methoxyethoxy)ethane, tetrahydrofuran, bis[2-(2-methoxyethoxy)ethyl]ether, 1,4-dioxane, dimethyl sulfoxide, dimethyl sulfone, diphenyl ether, sulfolane, diphenyl sulfone, tetramethylu
B · US 11,407,857 B2 · ¶ 87
An empty cell means only that no passage was reproduced there.
Statements in these documents
A polyimide resin is a material having characteristics of high durability and excellent heat resistance, and is widely used in electronic material applications.
A · US 9,505,886 B2 · ¶ 5
A polyimide obtained from a specific aqueous polyimide precursor solution composition of the present invention, in particular, has excellent properties such as heat resistance, mechanical strength, electrical properties, and solvent resistance, and further has excellent flexibility.
B · US 11,407,857 B2 · ¶ 2
In the meantime, there is a need for a polyimide further having excellent flexibility, for example, in the binder application, flexible-device application and the like.
B · US 11,407,857 B2 · ¶ 5
Cite aspatent.fyi, US 2026/0357012 A1, claim 1, first published 2026-11-20T08:53:13-05:00, https://patent.fyi/US20260357012/, SHA-256 0f020a2e11f11249d15b1dabfe9aed9de1a874785b70eb48250de2d5ba56fa22