Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Methyl substitution at R1
What ifWhat if R1 were methyl?
Claim language“an alkyl group having 4 or more carbon atoms”
A methyl-bearing precursor supplies the one-carbon substituent at R1. With methyl at the R2 positions, the chain has a low-polarity siloxane segment, and the terminal vinyl group reacts with silicon hydride groups during addition curing.
1.1Phenyl substitution at R1
What ifWhat if R1 were phenyl?
Claim language“an alkyl group having 4 or more carbon atoms”
A phenyl-bearing precursor supplies a six-carbon aromatic ring at R1. The terminal vinyl group provides a reaction site for silicon hydride groups during addition curing, while the hydroxy group remains available for a separate coupling reaction.
1.1Silicon hydride at an R2 site
What ifWhat if one internal R2 position carried hydrogen directly bonded to silicon?
Claim language“an alkyl group or an aryl group”
A methylhydrosiloxane unit contributes an internal silicon–hydrogen bond. During platinum-catalyzed curing, that bond adds across a vinyl group on another chain and forms a silicon–carbon linkage.
1.1Methoxy at an R2 site
What ifWhat if one internal R2 position carried a methoxy group bonded to silicon through oxygen?
Claim language“an alkyl group or an aryl group”
Water hydrolyzes the silicon–methoxy bond to form a silanol and release methanol. The resulting silanol condenses with a silanol on another chain or a hydroxylated surface to form a silicon–oxygen linkage.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Pigment treatment for silicone inks
Disperse hydroxylated silica-coated pigment in dry heptane and add an organopolysiloxane with a vinyl group at one end and a silanol group at the other. Remove the solvent and heat the treated pigment under reduced pressure to promote condensation between the terminal silanol and the surface silanols. Disperse the dried pigment in a silicone ink containing a silicon hydride crosslinker and a platinum catalyst so the exposed vinyl groups participate in curing.
Component substitution
Isobutyl substitution at the vinyl end
Use isobutyl in place of a straight-chain butyl group for R1 and use methyl for each R2. React isobutyllithium with trivinyltrimethylcyclotrisiloxane under dry inert gas to form the initiating silanolate. Add hexamethylcyclotrisiloxane to extend the chain and protonate the terminal silanolate with acetic acid to obtain the silanol end group.
Phenyl substitution within the siloxane backbone
Replace part of the hexamethylcyclotrisiloxane feed with a cyclic trimer containing three methylphenylsiloxane units. Feed the mixed cyclic monomers to the vinyl-bearing initiating silanolate to incorporate dimethylsiloxane and methylphenylsiloxane units along the chain. Protonate the terminal silanolate with acetic acid and use proton nuclear magnetic resonance to measure the incorporated phenyl fraction from the aromatic and silicon-bound methyl signals.
Parameter or scale variation
Two target siloxane chain lengths
Prepare separate batches using 10 and 40 moles of hexamethylcyclotrisiloxane per mole of titrated active initiating silanolate. Each ring adds three siloxane units, giving nominal additions of 30 and 120 units per active chain at full incorporation. Protonate each batch with acetic acid and use proton nuclear magnetic resonance to estimate average chain length from the terminal vinyl and silicon-bound methyl integrals after correcting for the methyl groups in the initiating end unit.
Combination with existing systems
Additive in a two-part silicone system
Blend the vinyl- and silanol-terminated organopolysiloxane into the catalyst-side component of a two-part addition-cure silicone containing vinyl-terminated silicone base polymer. Keep the silicon hydride crosslinker in the second component and count the additive's terminal vinyl when setting the hydride-to-vinyl ratio. Combine the components through a static mixer and cure the mixture in a heated mold so the additive's vinyl end attaches to the silicone network by hydrosilylation.
Automated or data-driven variant
Chromatographic control of the reaction endpoint
Fit the polymerization reactor with a sampling valve that transfers small aliquots into sealed vials containing a fixed amount of dilute acetic acid and an internal standard. Use an automated gas chromatograph calibrated for hexamethylcyclotrisiloxane to measure residual cyclic monomer in each quenched aliquot. When two consecutive results meet the residual monomer setpoint, the controller stops the feed and meters the acid charge into the stirred reactor.
Specific version of a part
Linear butyl with methyl substituents
R1 is linear butyl, with the structure –CH₂CH₂CH₂CH₃, and every R2 is methyl. The repeat count n is 10.
Hexyl with mixed methyl and phenyl
R1 is linear hexyl, and n is 20. One R2 position on each silicon that carries two R2 groups is methyl, and the other is phenyl.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1in formula (1), R1 represents an alkyl group having 4 or more carbon atoms, each R2 independently represents an alkyl group or an aryl group, and n represents 0 or an integer of 1 or more.
a) contain substituents of the type —(CH2)n—NR1R2, bonded to the cellulose or a side chain, e.g. hydroxyalkyl chain, in which n is at least 2 and the radicals R1 and R2 independently of one another are aliphatic or branched or cyclic alkyl or aryl substituents optionally substituted by heteroatoms, or H, or two radicals R1 and R2 can form a ring together with the nitrogen, R1 and R2 independently comprising 1-24 C-Atoms,
A · US 2006/0041117 A1 · ¶ 43
(e) a C1-C8 alkyl substituent group;
B · US 2012/0142918 A1 · abstract
An empty cell means only that no passage was reproduced there.
Statements in these documents
The object of the invention was therefore to provide an environmentally friendly, safe and cost-effective process for the preparation of cellulose derivatives containing amino groups.
A · US 2006/0041117 A1 · ¶ 7
The invention relates to a process for the preparation of cellulose derivatives containing amino groups by the reaction of alkali cellulose with reagents containing amino groups, it being possible to obtain water-soluble or water-dispersible reaction products in one reaction step starting from unsubstituted cellulose or cellulose derivatives.
A · US 2006/0041117 A1 · ¶ 2
PTA complexes may be used in aqueous phase catalysis or biphasic homogeneous catalysis.
B · US 2012/0142918 A1 · ¶ 3
PTA may also be used as a catalyst in non complexed form, i.e. as an organocatalyst.
B · US 2012/0142918 A1 · ¶ 3
Cite aspatent.fyi, US 2026/0357014 A1, claim 1, first published 2026-11-20T08:53:13-05:00, https://patent.fyi/US20260357014/, SHA-256 5e0902db381a303ea8e472df1418e9c1111ea4f0a8a87f38be6c42d86410d524