Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Solution preparation of stabilized polyester
What ifWhat if the polyester and stabilizer combine in a solution vessel?
Claim language“in a first melt mixing device”
A stirred vessel dissolves an amorphous copolyester and a multifunctional epoxy compound in a common solvent. A vacuum dryer removes the solvent, and a granulator breaks the solid residue into particles for melt blending with the aromatic polycarbonate.
1.2Two zones in one extruder
What ifWhat if one continuous extruder performs both mixing operations in separate barrel zones?
Claim language“in a second melt mixing device”
Upstream kneading blocks mix molten polyester with a polymeric carbodiimide. A heated side extruder supplies molten aromatic polycarbonate to a downstream port, and downstream kneading blocks in the same main extruder disperse it into the polyester stream.
1.2Polyester stabilization within final blend
What ifWhat if aromatic polycarbonate first combines with untreated polyester and the stabilizer enters the combined melt downstream?
Claim language“combining said stabilized polyester”
Upstream kneading blocks disperse the aromatic polycarbonate and untreated polyester together. A downstream port meters a multifunctional epoxy compound into the blend, and a heated mixing section provides residence time for the epoxy groups to react with polyester end groups.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Housings for commercial laundry pumps
A first twin-screw extruder melt mixes polybutylene terephthalate with a polymeric carbodiimide to stabilize the polyester. A second twin-screw extruder blends the stabilized polyester with aromatic polycarbonate and forms pellets. An injection molding press uses the dried pellets to mold pump housings with integral mounting bosses and a flange that compresses a separate gasket.
Component substitution
Silicone acrylic core shell modifier
A first melt mixer compounds polybutylene terephthalate with a polymeric carbodiimide. A silicone-acrylic core-shell powder serves as the impact modifier in place of a butadiene-based modifier. A side feeder introduces the powder into the second mixer after the stabilized polyester and aromatic polycarbonate form a melt, and downstream kneading elements disperse the particles before pelletization.
Parameter or scale variation
Parallel blending at pilot scale
One first-stage extruder compounds polyester with a polymeric carbodiimide and supplies 6 kg/h of stabilized polyester pellets to a buffer hopper. Two loss-in-weight feeders each meter 3 kg/h of these pellets into a separate second-stage extruder. Each second-stage extruder receives 7 kg/h of aromatic polycarbonate and produces 10 kg/h of blend, for a combined output of 20 kg/h.
Combination with existing systems
Direct extrusion of flat sheet
A first melt mixer compounds polyester with an epoxy-functional stabilizer, and a second melt mixer blends the stabilized polyester with aromatic polycarbonate. A screen changer filters the blend at the second mixer outlet, and a gear pump meters the filtered melt into a flat sheet die. A three-roll cooling stack sets the sheet thickness before edge trimming and cutting.
Automated or data-driven variant
Viscosity feedback for stabilizer dosing
A side-stream capillary rheometer measures the stabilized polyester at the first mixer outlet at a fixed temperature and flow rate. A controller compares apparent viscosity with a target band established for the polyester grade and adjusts the epoxy-functional stabilizer feeder within preset dosing limits. The controller holds each adjustment for at least one measured transit time from the feeder to the rheometer, and the main melt stream enters the second mixer for blending with aromatic polycarbonate.
Specific version of a part
Stabilizer concentrate feeds final blend
A first extruder disperses a polymeric carbodiimide in a low-melting ethylene copolymer carrier and produces concentrate pellets. A second extruder melts the polyester and aromatic polycarbonate with the concentrate, where the carbodiimide reacts with polyester carboxyl end groups.
Carbodiimide in a twin screw
A gravimetric feeder supplies dried polybutylene terephthalate pellets to a co-rotating twin-screw extruder, and a side feeder meters polymeric carbodiimide into the molten polyester. Kneading blocks disperse the additive at a melt temperature of about 240 °C before pelletization.
Epoxy mixing in a batch chamber
A heated batch mixer melts polybutylene terephthalate at about 240 °C before receiving a multifunctional epoxy oligomer. Intermeshing rotors distribute the oligomer through the polyester melt and bring its epoxy groups into contact with polyester end groups.
Downstream feeding of impact modifier
A second co-rotating twin-screw extruder melts dried stabilized polyester pellets with aromatic polycarbonate pellets at about 260 °C. A downstream side feeder adds an acrylic core-shell impact modifier, and kneading blocks disperse its particles before the blend exits the die.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a) combining the polyester with the hydrolytic stabilizer composition in a first melt mixing device so as to form a stabilized polyester, and
Apart from the addition of the hydrolysis stabilizer in form of a masterbatch, the hydrolysis stabilizer may be added directly during the production of the polyester article, e.g. film. Particularly good results are obtained when twin-screw extruders are used and the hydrolysis stabilizer is metered directly into the melt of the respective extruder.
B · US 11,384,222 B2 · ¶ 29
1.2b) combining said stabilized polyester with the aromatic polycarbonate and optionally the impact modifier in a second melt mixing device,
A method of, in two reaction tanks in which a reaction tank for conducting the step 1 and a reaction tank for performing the step 2 are connected, charging an aliphatic polycarbonate diol and a chain extender into a first reaction tank, performing a reaction of the step 1, transferring the resulting reaction product to a second reaction tank, charging aromatic polyester chips into the second reaction tank, and heating and stirring the mixture to perform a blocking reaction to
A · US 2010/0041858 A1 · ¶ 50
An empty cell means only that no passage was reproduced there.
Statements in these documents
From the background, development of a polyester-polycarbonate type thermoplastic polyester elastomer having high blocking property and excellent retainability of the blocking property is strongly solicited.
A · US 2010/0041858 A1 · ¶ 7
For this reason, establishment of a process for economically producing a polyester-polycarbonate type thermoplastic polyester elastomer having preferable property is strongly solicited.
A · US 2010/0041858 A1 · ¶ 8
However, a disadvantage of unstabilized polyester films is their susceptibility to hydrolysis, especially at temperatures above the glass transition temperature of the particular polyester.
B · US 11,384,222 B2 · ¶ 3
It is therefore an object of the present invention to provide a hydrolysis-resistant polyester raw material which avoids the disadvantages of the prior art described.
B · US 11,384,222 B2 · ¶ 8
Cite aspatent.fyi, US 2026/0357018 A1, claim 1, first published 2026-11-20T08:53:13-05:00, https://patent.fyi/US20260357018/, SHA-256 746d841d34982f5f5af6080f62dacc7258a7b764acca40bfd84faa5f7572930e