1.1Melt filtration for gel removal
An extruder melts the polyethylene and feeds it through a screen pack with openings sized to retain gel particles. A differential pressure sensor signals when the loaded screen needs replacement.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
An extruder melts the polyethylene and feeds it through a screen pack with openings sized to retain gel particles. A differential pressure sensor signals when the loaded screen needs replacement.
A capillary rheometer extrudes the melt through a round die at a fixed temperature and flow rate. A laser micrometer measures the strand diameter at a fixed distance from the die, and the diameter divided by the die bore gives the swell ratio.
A rotational rheometer applies sinusoidal shear at 1 rad/s and 190 °C within the linear viscoelastic range. The instrument reports the storage modulus at that frequency for comparison with a limit calibrated at the same setting.
A rotational rheometer applies a small shear strain step to the melt and records the decay in stress while holding the strain constant. A relaxation spectrum fitted to the stress decay yields the storage and loss moduli over the frequency range supported by the time record.
A shallow cone oscillates above a flat lower plate with the polyethylene melt held at 190 °C. The instrument calculates both moduli from the torque amplitude and phase using the cone geometry.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A thermal visbreaking line supplies polyethylene to an extrusion coating line for woven protective covers. A slot die lays the treated melt onto the moving fabric, and a chilled nip roll presses the coating into contact with the fabric and solidifies it. A camera downstream of the chill roll counts raised defects per square metre at a fixed coating weight.
A jacketed batch reactor with a close-clearance anchor agitator replaces the extruder for thermal visbreaking. A nitrogen blanket covers the polyethylene melt, and the agitator sweeps the heated wall throughout the treatment hold. A bottom outlet feeds a gear pump that transfers the treated melt to a cooled strand die for solidification and sampling.
A melt gear pump meters polyethylene at 5 kg/h through a heated treatment section with interchangeable melt hold volumes of 0.12 and 0.36 L. At a melt density of 0.72 kg/L, those volumes give nominal mean residence times of about 1 and 3 minutes, respectively. The line cools the melt after each hold, and separate samples provide MIE, ER, and gel counts at each residence time.
A continuous screen changer sits downstream of the thermal treatment section and upstream of an underwater pelletizer. Pressure transducers across the screen pack track the buildup of retained material and trigger screen indexing at a set differential pressure. A gear pump delivers filtered melt to the pelletizing die, where rotating blades cut the polymer and circulating water cools and carries the pellets.
A sidestream capillary rheometer downstream of the heated section measures the pressure drop at fixed melt temperature and flow rate. A controller maps that signal to an estimated MIE using paired laboratory measurements at 190 °C under a 2.16 kg load. The controller adjusts the melt metering pump within preset limits to change residence time, and periodic oscillatory shear measurements supply ER for checking the MIE/ER ratio.
A sidestream gear pump feeds treated polyethylene through a small slot die onto a chill roll to form a film at a fixed gauge. A transmitted-light line-scan camera records the film, and software counts defects by projected size per unit area. The inspection system timestamps the counts and associates them with treatment temperature and throughput after accounting for transport time to the camera.
A twin-screw extruder feeds polyethylene with ER from 1 to 8 and MIE from 0.1 to 5 g/10 min through a heated reaction zone. Melt temperature and residence time control thermal chain scission, and cooling arrests the treatment. Measurements on the cooled material verify a MIE/ER ratio from 0.2 to 2.44.
A frequency sweep provides neighboring data points with loss moduli below and above 0.5 kPa. Interpolation between the paired loss and storage modulus readings gives the storage modulus at the target loss modulus.
A rotational rheometer holds a polyethylene disk between 25 mm parallel plates at a 1 mm gap and 190 °C. The upper plate oscillates over a range of frequencies at a strain within the linear viscoelastic range, and the instrument calculates both moduli from the amplitude and phase of the torque response.
A melt flow tester holds the polyethylene charge at 190 °C and applies a total piston load of 2.16 kg. After preheating, the operator collects timed extrudate cuts within the measurement travel interval, weighs them, and converts the measured mass per unit time to grams per 10 minutes.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
The standardized basic software is utilized to calculate the rheological properties, i.e. the storage-modulus, G′, the loss-modulus, G″, the phase lag δ (=arctan(G″/G′)) and the complex viscosity, η*, as a function of the applied frequency, namely η*(ω)=[G′(ω)2+G″(ω)2]1/2/ω.A · US 9,873,783 B2 · ¶ 86
After 4 min of annealing the sample at the measurement temperature of 200° C. under a constant strain-amplitude of 5%, the stress response of the material is measured and analyzed in a range of excitation frequencies (ω) from 670 to 0.02 rad/s. The standardized basic software is utilized to calculate the rheological properties, i.e. the storage-modulus, G′, the loss-modulus, G″, the phase lag δ (=arctan(G″/G′)) and the complex viscosity, η*, as a function of the applied frequency, namely η*(ω)=[G′(ω)2+G″(ω)2]1/2/ω.A · US 9,873,783 B2 · ¶ 86
In some embodiments, the ethylene alpha-olefin copolymers provided herein have a melt index of about 0.4 dg/10 min to about 2.0 dg/10 min, about 0.4 dg/10 min to about 1.0 dg/10 min, or about 0.4 dg/10 min to about 0.7 dg/10 min.B · US 10,654,956 B2 · ¶ 25
An empty cell means only that no passage was reproduced there.
In certain applications, these compositions may require enhanced tensile properties, such as when large amounts of fillers/additives are present, to avoid excessive deformation, thinning and failure under tensile stresses.A · US 9,873,783 B2 · ¶ 4
The ethylene polymer compositions of the present disclosure exhibit a favorable balance of tensile strength at break, elongation at break and compression set, while still maintaining good thermoplastic properties.A · US 9,873,783 B2 · ¶ 6
Maximizing this improvement in performance as the density decreases would be useful in a number of applications.B · US 10,654,956 B2 · ¶ 4
Therefore, ethylene alpha-olefin copolymers, including superhexene LLDPE resins, having an improved balance of impact versus density may be suitable for a number of applications.B · US 10,654,956 B2 · ¶ 4
patent.fyi, US 2026/0357024 A1, claim 1, first published 2026-11-20T09:31:44-05:00, https://patent.fyi/US20260357024/, SHA-256 7e7d9ebc18eb4dea731218c418565c5c414194da5f293018af7cb3b4f554b53a