1.1Sodium methoxide catalysis
A sealed stirred reactor contacts polyethylene terephthalate flakes with methanol and sodium methoxide at 120 degrees Celsius. Methoxide promotes ester exchange, yielding dimethyl terephthalate and ethylene glycol.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A sealed stirred reactor contacts polyethylene terephthalate flakes with methanol and sodium methoxide at 120 degrees Celsius. Methoxide promotes ester exchange, yielding dimethyl terephthalate and ethylene glycol.
A stirred pressure reactor heats polyethylene terephthalate flakes in aqueous sodium hydroxide at 150 degrees Celsius. Hydrolysis produces dissolved sodium terephthalate and ethylene glycol, and acidification precipitates terephthalic acid.
A stirred vessel contacts finely ground polyethylene terephthalate with methanol, a swelling cosolvent such as dichloromethane, and potassium carbonate at 60 degrees Celsius under reflux. Swelling increases access to the ester bonds, and ester exchange produces dimethyl terephthalate and ethylene glycol.
A pressure reactor contacts polyethylene terephthalate with excess methanol at 280 degrees Celsius and 20 megapascals. Methanol cleaves the ester bonds by transesterification, and cooling the reactor effluent allows dimethyl terephthalate to crystallize.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A rotary cutter chops undyed polyethylene terephthalate fabric offcuts from garment production, and a dryer removes residual moisture. A stirred pressure vessel contacts the chopped fabric with methanol and triethylamine at 150 degrees Celsius. Cooling crystallizes dimethyl terephthalate, which a filter separates from the liquid containing ethylene glycol.
A stirred pressure vessel contacts polyethylene terephthalate flakes with dry ethanol and triethylamine at 175 degrees Celsius. Ethanol cleaves the polyester ester bonds to form diethyl terephthalate and ethylene glycol. After cooling, a vacuum evaporator recovers excess ethanol, and a crystallizer separates diethyl terephthalate from the glycol-rich liquid.
A jacketed stirred pressure vessel holds polyethylene terephthalate flakes, methanol and triethylamine at 120 degrees Celsius for 15 minutes while agitation wets and disperses the flakes. The jacket then raises the batch to 165 degrees Celsius and holds it there for 75 minutes to continue ester cleavage. Cooling water returns the batch to 25 degrees Celsius before filtration recovers the dimethyl terephthalate crystals.
A pressure-rated slurry pump feeds finely milled polyethylene terephthalate dispersed in methanol and triethylamine into the first of two stirred pressure vessels connected in series. Both vessels operate at 160 degrees Celsius and 30 bar absolute, with liquid levels and feed rate set for a nominal residence time of 45 minutes per vessel. A heat exchanger cools the second vessel's discharge under pressure before a back-pressure valve releases it into a crystallizer. A filter collects the dimethyl terephthalate crystals and passes the ethylene glycol in the filtrate.
A stirred pressure reactor contacts polyethylene terephthalate flakes with methanol and triethylamine at 150 degrees Celsius. A cooled crystallizer and filter remove dimethyl terephthalate from the reactor discharge. A fractional distillation column recovers a methanol-rich overhead stream from the filtrate, and a recycle tank blends that stream with fresh methanol and triethylamine for the next batch. Ethylene glycol concentrates in the column bottoms for separate recovery.
A stirred pressure reactor contacts polyethylene terephthalate flakes with methanol and triethylamine at 155 degrees Celsius. An automated sampler withdraws liquid through a heated filter and dilutes each sample in a measured volume of acetonitrile for liquid chromatography. A controller calculates the dimethyl terephthalate concentration from a calibration curve and starts jacket cooling when the concentration changes by less than 2 percent across three samples taken five minutes apart.
A sealed stirred reactor contacts polyethylene terephthalate flakes with methanol containing dissolved triethylamine at 175 degrees Celsius. The tertiary amine provides basic catalysis for ester exchange, and the closed vessel retains methanol under pressure.
A sealed stirred vessel contacts polyethylene terephthalate particles with a solution of ethanolamine in ethanol at 160 degrees Celsius. The primary amine attacks ester carbonyls, releasing ethylene glycol and forming bis(2-hydroxyethyl) terephthalamide.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
In one or more embodiments, the treating step (a) and the converting step (b) are performed at a temperature between 105° C. and 300° C. and a pressure of between 14 psia and 5000 psia. In one or embodiments, the treating step (a) and the converting step (b), are performed at a temperature between 150° C. and 300° C. and a pressure between 200 psia and 600 psia.A · US 2023/0014630 A1 · ¶ 22
In methanolysis, the polyester is reacted with methanol to produce a depolymerized polyester mixture comprising polyester oligomers, dimethyl terephthalate (“DMT”), and ethylene glycol (“EG”).B · US 2023/0022664 A1 · ¶ 4
An empty cell means only that no passage was reproduced there.
For example, the energy usage associated with superheating and/or condensing the excess methanol may markedly increase the operational cost of the process.A · US 2023/0014630 A1 · ¶ 6
A continuing unmet need therefore exists for a polyester methanolysis depolymerization process with increased polyester depolymerization and/or DMT yield and reduced methanol requirements.A · US 2023/0014630 A1 · ¶ 7
The presence of one or more of these side species can negatively impact the use and recovery of more useful or commercially valuable components of the reaction product stream.B · US 2023/0022664 A1 · ¶ 7
While some of these products may be separable from the product stream as-is, their separation and subsequent disposal can be expensive, time-consuming and environmentally problematic.B · US 2023/0022664 A1 · ¶ 7